EFFECT OF ACICULAR FERRITE MICROSTRUCTURE COMPOSITION ON STRENGTH OF X65 PIPELINE STEEL |
Wei WANG;; |
中国科学院金属研究所 |
|
Cite this article:
Wei WANG. EFFECT OF ACICULAR FERRITE MICROSTRUCTURE COMPOSITION ON STRENGTH OF X65 PIPELINE STEEL. Acta Metall Sin, 2007, 43(6): 578-582 .
|
Abstract The effect of acicular ferrite (AF) microstructure composition of different phases on the strength of X65 pipeline steel was investigated by varying thermo-mechanical control process (TMCP) parameters to the steel. Experimental results showed that lowering the finish rolling temperature or increasing the cooling rate was in favor of formation of the granular ferrite and the bainite ferrite in AF microstructure, thus obviously increasing the strength of the steel. Enhancing the coiling temperature could accelerate the perception strengthening, also in favor of the strength for the steel. However, lowering the finish rolling temperature made the most contribution to the increase of the strength.
|
Received: 26 September 2006
|
|
[1]Smith Y E,Coldren A P,Cryderman R L.Toward Im- proved Ductility and Toughness.Tokyo:Climax Molyb- denum Co.Ltd.,1972:119 [2]Coldren A P,Smith Y E,Cryderman R L.Processing and Properties of Low Carbon Steel.New York:American In- stitute of Mining,Metallurgical and Petroleum Engineers, ??1973:163 [3]Tanaka T.Int Met Rev,1981;26:185 [4]Lee J L,1Hon M H,Cheng G H.J Mater Sci,1987;22: 2767 [5]Thompson S W,Colvin D J,Krauss G.Metall Trans, 1990;21A:1493 [6]Krauss G,Thompson S W.ISIJ Int,1995;35:937 [7]Zhao M C,Shan Y Y,Qu J B,Xiao F R,Zhong Y,Yang K.Acta Metall Sin,2001;37:820 (赵明纯,单以银,曲锦波,肖福仁,钟勇,杨柯.金属学报,2001;37:820) [8]Zhao M C,Xiao F R,Shan Y Y,Li Y H,Yang K.Acta Metall Sin,2002;38:283 (赵明纯,肖福仁,单以银,李玉海,杨柯.金属学报,2002; 38:283) [9]Grong O,Matlock D K.Int Met Rev,1986;31:27 [10]Li H L,Guo S W,Feng Y R,Huo C Y,Chai H F.An Illustrative Collection of Microstructure Micrographs of High Strength Micra-alloyed Steels.Beijing:Petroleum Industry Press,2001:3 (李鹤林,郭生武,冯耀荣,霍春勇,柴慧芬.高强度微合金管线钢显微组织分析与鉴别图谱.北京:石油工业出版社,2001: 3) [11]Massalski T B.Phase Transformations.Metals Park, Ohio:ASM,1970:433 [12]Hillert M.Metall Trans,1984;15A:411 [13]Cawley J,Harris C F,Wilson E A.New Aspects of Mi- crostructures in Modern Low Carbon High Strength Steels. Tokyo:ISIJ,1994:11 [14]Shibata K,Asakura K.New Aspects of Microstructures in Modern Low Carbon High Strength Steels.Tokyo:ISIJ, 1994:31 [15]Terada Y,Chijiiwa R,Tamehiro H,Kikuma T,Funato K.Proc 2nd Int Conf HSLA Steels:Processing,Proper- ties and Applications.Beijing:The Chinese Society for Metals,1990:519 [16]Madariaga I,Romero J L,Gutierrez I.Metall Mater Traus,1998;29A:1003 [17]Babu S S,Bhadeshia H K D H.Mater Traus JIM,1991; 32:679 [18]Yoo J Y,Kim C M.Prac 3rd Int Conf Adv Struct Steels, Gyeongju:Korean Institute of Metals and Materials and POSCO,2006:191 [19]Kong J H,Zhen L,Guo B,Li P H,Wang A H,Xie C S. Mater Des,2004;25:723 [20]Zhao M C,Yang K,Xiao F R,Shah Y Y.Mater Sci Eng, 2003;A355:126 [21]Xiao F R,Liao B,Shah Y Y,Qiao G Y,Zhong Y,Zhang C L,Yang K.Mater Sci Eng,2006;A431:41 [22]Charleux M,Poole W J,Militzer M,Deschamps A.Metall Mater Trans,2001;32A:1635 [23]Kang H C,Lee S H,Shin D H,Lee K J,Kim S J,Lee K S.Mater Sci Forum,2004;449-452:49 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|