| INVESTIGATION OF RAPID DIRECTIONAL SOLIDIFICATION OF AL-BASED IMMISCIBLE ALLOYS Ⅱ. EFFECT OF THE THIRD ELEMENT |
| Jie He;;;;; |
| 金属研究所 |
|
Cite this article:
Jie He. INVESTIGATION OF RAPID DIRECTIONAL SOLIDIFICATION OF AL-BASED IMMISCIBLE ALLOYS Ⅱ. EFFECT OF THE THIRD ELEMENT. Acta Metall Sin, 2007, 43(6): 573-577 .
|
|
|
Abstract The directional solidification experiment has been carried out for the Al-Bi based immiscible alloys. The effect of the addition element Si or Cu and the content on the solidification microstructure was investigated. The results show that both Si and Cu accelerate the coarsening of the Bi-rich sphere, and the addition of Si is more obvious than the element Cu to do under the same experimental condition. The change of the free energy, liquid-liquid interfacial energy and liquid viscosity due to the addition has been analyzed. Also, the effect of the change on the solidification process was discussed in detail. This investigation will enrich the understanding of the solidification feature of the ternary immiscible alloys.
|
|
Received: 09 November 2006
|
|
|
[1]Grugel R G.Metall Trans,1991;22B:339 [2]Chan J W.Metall Trans,1979;10A:119 [3]Zhao J Z,Ratke L,Jia J,Li Q C.J Mater Sci Technol, 2002;18:197 [4]Guo J J,Liu Y,Su Y Q,Ding H S,Zhao J Z,Xue X.Scr Mater,2001;45:1197 [5]Rudrakshi G B,Srivastava V C,Pathak J P,Ojha S N. Mater Sci Eng,2004;A383:30 [6]He J.PhD Dissertation,Institute of Metal Research,Chi- nese Academy of Sciences,Shenyang,2006 (何杰,中国科学院金属研究所博士学位论文,沈阳,2006) [7]Grobner J,Schmid-Fetzer R.JOM,2005;9:19 [8]Ratke L,Diefenbach S.Mater Sci Eng,1995;R15:263 [9]Herlach D M.Solidification and Crystallization.Berlin, Germany,Wiley-VCH,2004:110 [10]Hara S,Hanao M,Ogino K.J Jpn Inst Met,1993;57:164 (原茂太,花尾方史,荻野和己.日本金属学会志,1993;57: 164) [11]Kaban I,Hoyer W,Merkwitz M.Z Metallkd,2003;94: 831 [12]He J,Zhao J Z,Ratke L.Acta Mater,2006;54:1749 [13]He J,Zhao J Z.J Mater Sci Technol,2005;26:759 [14]Zener C.J Appl Phys,1949;20:950 [15]McAlister A J.In:Massalski T B ed.,Binary Alloy Phase Diagrams.Vol.1,Materials Park,OH:ASM International, 1990:128 [16]Villars P,Prince A,Okamoto H.Handbook of Ternary Alloy Phase Diagrams.Vol.3,Materials Park,OH:ASM International,1990 [17]Singh R N,Sommer F.Rep Prog Phys,1997;60:57 [18]Olesinski R W,Abbaschian G J.Bull Alloy Phase Dia- grams,1985;6:359 [19]Gebhardt,Becker M.Dorner S.Aluminum,1959;31:315 [20]Seetharman S,Sichen D.Metall Mater Trans,1994;25B: 589O |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|