													     		                            						                            																	    Abstract  A model responsible for the magnetic--induced rotation of single anisotropic grain in free medium has been proposed firstly based on the classical dynamics of rigid body, in which the grain is treated as a prolate spheroid. A theoretical expression was derived for the alignment time of grain as a function of viscidity of liquid matrix, aspect ratio of grain, difference of anisotropic magnetic susceptibility of grain and applied magnetic intensity. It was applied to predict the alignment time of paramagnetic superconductor material Bi--2212 and ferromagnetic material Bi--3%Mn in melt processing. An experiment was conducted for the latter melted fully at 300℃ then rapidly quenched under different applied magnetic field, and the MnBi texture is obtained. It is found that the alignment time is less than one second, in good agreement with the theoretical prediction.
																										     | 
														 
												  		
														
															| 
															    																	Received:  30 June 2003
																	    
															    															    															  
															 | 
															
														 
														 														
															| 
																
															 | 
														 
																																									    																											 
												 
												
												
												
												 
												
												  
             
                         
            
									            
									               
																												  
															  [1] Farrel D E, Chandrasekhar B S, DeGuire M R, Fang M M, Kogan V G, Clem J R, Finnemore D K. Phys Rev B,1987; 36(7) : 4025 [2] Cloots R, Vandewalle N, Ausloos M. Appl Phys Lett, 1994;65: 3386 [3] Ma Y, Wang Z. Physica C 1997; 282-287: 2619 [4] Ferreira P J, Liu H B, Vander Sande J B. J Mater Res,1999; 14(7) : 2751 [5] Morikawa H, Sassa K, Asai S. Mater Trans JIM,1998;39(8) : 814 [6] Yasuda H, Ohnaka I, Shimamura K. In: Asai S ed, The 3rd Int Symp on EPM.Nagoya, Japan, ISIJ, 2000: 647 [7] Wang H, Ren Z M, Deng K, Xu K D. Acta Metall Sin,2002: 38: 41(王晖, 任忠鸣, 邓康, 徐匡迪.金属学报, 2002; 38: 41)  [8] Wang H, Ren Z M, Deng K, Xu K D. Trans Chin Nonferrous Met Soc, 2002; 12(3) : 556(任晖,任忠鸣,邓康等,徐匡迪.中国有色金属学报,2002; 12(3) :556)  [9] Wan D F, Ma X L. Physics of Magnetism. Beijing: Electric Industry Press, 1999: 436(宛德福, 马兴隆.磁性物理学. 北京: 电子工业出版社, 1999:436)  [10] Probstein R F. Physicochemical Hydrodynamics: An Introduction, Butterworths, Boston, 1989: 85 [11] Barrett S E, Durand D J, Pennington C H. Phys Rev B,1990; 41: 6283 [12] Vaknin D, Sinha S K, Stassis C, Miller L L, Johnson D C.Phys Rev B, 1990; 41: 1926 [13] Shetty M N, Rawat D K, Rai K N. J Mater Sci, 1987; 22:1908 [14] O' Handly R C. Modern Magnetic Materials: Principles and Application. New York: John Wiley and Sons, 2000:45 [15] Moffatt W G. The Handbook of Binary Phase Diagrams.New York: Genium, 1984Y | 
														   
																											 
									             
									           
             
			            			 
			
             
								                
															
																
																	
																																																																									
																				| No Suggested Reading articles found! | 
																			 
																																			 
																 | 
															 
														 
								             
             
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |