| Grain Size Distribution And Topological Evolution in 2D Grain Growth Process Based on Phase Field Simulation |
| SUN Ya; LIU Guoquan; WANG Chao |
| School of Materials Science and Enginering; University of Science and Technology Beijing; Beijing 100083 |
|
Cite this article:
SUN Ya; LIU Guoquan; WANG Chao. Grain Size Distribution And Topological Evolution in 2D Grain Growth Process Based on Phase Field Simulation. Acta Metall Sin, 2004, 40(6): 609-.
|
|
|
Abstract The quasi--steady state grain size distribution in the 2D grain growth process obtained by phase field method can be described well either by Weibull function or Louat distribution function, since the plots of two functions are exactly the same or very similar to each other under certain conditions. The grain side number distribution also achieves self--similarity or the quasi--steady state finally, however, it approaches a lognormal distribution instead. The relationship between the average number of grain sides and grain size appears to be nonlinear. These results agree well not only with those of high purity Al foil but also those obtained from our Monte Carlo simulation.
|
|
Received: 20 June 2003
|
|
|
[1] Fayad W, Thompson C V, Frost H J. Scr Mater, 1999;40(10) : 1199 [2] Wang C, Liu G Q, Qin X G. Acta Metall Sin, 2003; 39:635(王超, 刘国权, 秦湘阁. 金属学报, 2003; 39: 635) [3] Wang C, Liu G Q, Qin X G. ISIJ Int, 2003; 43(5) : 774 [4] Fan D N, Chen L Q. Acta Mater, 1997; 45: 611 [5] Fan D N, G Chengwei, Chen L Q. Acta Mater, 1997; 45:1115 [6] Anderson M P, Fortes M A. Philos Mag, 1989; B59: 293 [7] Wang C. PhD Dissertation, University of Science and Technology Beijing. 2003. 5(王超.北京科技大学博士学位论文, 2003) [8] Nordbakke M W, Ryum N, Hunderi O. Acta Mater, 2002;50: 3661 [9] Beck P A. Philos Mag Suppl, 1954; 3: 245 [10] Tikare V, Holm E A, Fan D, Chen L Q. Acta Mater, 1999;47: 363 [11] Mullins W W. Acta Mater, 1998; 46: 6219 [12] Fradkov V E, Frachenko A S, Shvindlerman L S. Scr Met,1985; 19: 1291 |