Abstract A model to describe dislocation patterns based on cellular automaton and molecular dynamics is presented, which takes into account the short—range interaction and long--range interaction between edge dislocations with opposite Burger's vectors on the same glide plane or the different glide planes. This model uses molecular dynamics to deal with long--range interaction, and cellular automaton to describe the short--range interaction. Using the model, the dislocation structures of single crystal Cu are simulated under no external stress and applied cyclic stress.
|
|
Received: 17 June 2003
|
|
|
[1] Kuhlmann-Wilsdorf D, van der Merve J H. Mater Sci Eng, 1982; 55; 79 [2] Bassim M N, Jesser W A, Kuhlmann-Wilsdorf D, Wilsdorf H G F. Mater Sci Eng, 1986; 81; 122 [3] Holt D L. J Appl Phys, 1970; 41; 3179 [4] Hahner P. Acta Mater, 1996; 44; 2345 [5] Walgraef D, Aifantis E C. J Appl Phys, 1985; 15; 688 [6] Groma I, Balogh P. Acta Mater, 1999; 47; 3647 [7] Zhang L, Wang Y M, Zhang C B. Acta Metall Sin, 2001;37; 882(张林,王元明,张彩碚.金属学报, 2001; 37; 882) [8] Zhang L, Zhang C B, Liu X H, Wang G D, Wang Y M. J Mater Sci Technol, 2002; 18; 163 [9] Zhang L, Zhang C B, Wang Y M, Liu X H, Wang G D. J Mater Res, 2002; 17; 2251 [10] Zhang L, Wang Y M, Zhang C B, Wang S Q, Ye H Q.Modelling Simul Mater Sci Technol, 2003; 11; 791 [11] Zhang L, Zhang C B, Wang Y M, Wang S Q, Ye H Q.Acta Mater, 2003; 51; 5519 [12] Lepinoux J. Solid State Phenom, 1988; 3; 335 [13] Kubin L P, Canova G, Condat M, Devincre B, Pontikis V, Brechet Y. Solid State Phenom, 1992; 23-24; 455 [14] Fournet R, Salazar J M. Phys Rev B, 1996; 53; 6283 [15] Salazar J M, Fournet R, Banai N. Acta Mater, 1995; 43;1127d |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|