HIGH TEMPERATURE DEFORMATION AND ANNEALING TEXTURES OF TiAl BASE INTERMETALLICS |
ZHANG Fang; WANG Yandong; ZHU Yubin; MIAO Jiashi; XU Jiazhen; LIANG Zhide ( Department of Materials Science & Engineering; Northeastern University; Shenyang 110006 Northwest Institute of Nonferrous Metal Research; Xi'an 710016;)Correspondent: WANG Yandong; associate professor; Tel: (024)25912589; Fax: (024)25890448 |
|
Cite this article:
ZHANG Fang; WANG Yandong; ZHU Yubin; MIAO Jiashi; XU Jiazhen; LIANG Zhide ( Department of Materials Science & Engineering; Northeastern University; Shenyang 110006 Northwest Institute of Nonferrous Metal Research; Xi'an 710016;)Correspondent: WANG Yandong; associate professor; Tel: (024)25912589; Fax: (024)25890448. HIGH TEMPERATURE DEFORMATION AND ANNEALING TEXTURES OF TiAl BASE INTERMETALLICS. Acta Metall Sin, 1998, 34(8): 802-806.
|
Abstract Microstructure and texture evolution of Ti-49.6Al-0.16Ni-0.14B alloy forged at 900℃ and then annealed at various temperatures were studied. Their texture components were accurately determined by the modified maximum entropy method (MMEM). Possible mechanisms of texture formation during deformation and annealing were proposed. A microstructure heredity characterization of deformed and annealed γ-TiAl alloy was reported.
|
Received: 18 August 1998
|
1 Lipsitt H A. Mater Res Soc Symp Proc, 1985; 39: 351 2 Kim Y W. JOM 1994; 7: 30 3 Bunge H J. Z Metallk, 1965; 56: 872 4 Hartig C, Fang X F, Mecking H, Dahms M. Acta Metal Mate,, 1992; 40: 1883 5 Wang Y D, Xu J Z, Liang Z D. Textures Mcrostrurrt, 1995; 2627: 103 6 Zhang Y G, Chaturvedi M C. Mater Sci Eng, 1994; A174: 45 7 Lilcke K. In: Brsakman C M ed., Proc 7th Int Conf on Textures of Materials. Amsterdam: Elsevier, 1984: 195 8 Wang Y D, Vadon A, Heizmann J J. Mater Sci Eng, 1997; A222: 71 9 Zhu G, Mao W, Yu Y, Sun Z. In: Liang Z D, Zuo L, Chu Y Y eds., Proc 11th Int Conf on Textures of Materials.Beijing: International Academic Publishers, 1996: 1088 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|