PARTICLE STIMULATED NUCLEATION AND THE FORMATION OF RSCRYSTALLIZATION TEXTURE IN Al-Mn ALLOY CONTAINING PARTICLES Ⅱ. Interaction Between Particles and Other Nucleation Sites and the Formation of Recrystallization Texture
YANG Ping; O.ENGLER(Institute of Metal Science and Metal Physics; Aachen University of Technology; Kopernikusstr. 14; D-52056;Aachen; Germany) Now: School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing;100083 Now: Los Alamos National Laboratory; Center for Materials Science; K765; Los Alamos; NM87545; USACorrespondent: YANG Ping; Tel: (010)62333436; Fax: (010)62332336
Cite this article: 

YANG Ping; O.ENGLER(Institute of Metal Science and Metal Physics; Aachen University of Technology; Kopernikusstr. 14; D-52056;Aachen; Germany) Now: School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing;100083 Now: Los Alamos National Laboratory; Center for Materials Science; K765; Los Alamos; NM87545; USACorrespondent: YANG Ping; Tel: (010)62333436; Fax: (010)62332336. PARTICLE STIMULATED NUCLEATION AND THE FORMATION OF RSCRYSTALLIZATION TEXTURE IN Al-Mn ALLOY CONTAINING PARTICLES Ⅱ. Interaction Between Particles and Other Nucleation Sites and the Formation of Recrystallization Texture. Acta Metall Sin, 1998, 34(8): 793-801.

Download:  PDF(3295KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  On the basis of analyzing the subgrain rotations around paricles within deformed matrices and their nucleation, a further investigation of the orientations of grains formed at particles locating at grain boundaries and cube bands was carried out and the formation of recrystallization texture was analyzed. Results reveal that the orientations of the grains at these places retain the orientational features of particle stimulated nucleation within deformed matrices and possess the characteristics of nucleation at grain boundaries or at cube bands. Recrystallization texture is produced by nucleation at different sites.
Key words:  Al-Mn alloy      particle stimulated nucleation      recrystallization texture      EBSD     
Received:  18 August 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I8/793

1 Bleck W, Bunge H J. Acta Metall, 1981; 29: 1401
2 rsund R, Nes E. Scr Metall, 1988; 22: 665
3 Juul Jensen D, Hansen N, Humpherys F J. Acta Metall, 1985; 33: 2155
4 Weiland H, Rouns T N, Liu J. Z Metallkd, 1994; 85: 592
5 Humphreys F J, Ferry M, Johnson C, Pailard P. 16th Ris Inter Sym, Ris National Lab., Denmark1995: 87
6 Johnson C P, Humphreys F J. In: Liang Z et al eds., ICOTOM-11, X'ian, China, 1996: 1263
7 Engler O, Yang P, Kong X. Actd Maten 1996; 44: 3349
8 Nes E, In: Hansen N et al eds., 1st Ris Inter Sym Ris National Lab., Denmark, 1980: 85
9 杨平, Engler 金属学报, 1998; 34: 785(Yang P, Engler O. Acta Metall Sin, 1998; 34: 785)
10 Engler O, Escher C, Gottstein G. Textures Mcrostrvct, 1996; 26: 337
11 Yang P, Engler O. In: Hansen N eds., 16th Ris Inter Symp, Ris National Lab., Denmark, 1995: 595
12 Humphreys F J. In: Hansen N ed., 1st Ris Inter Symp, Ris National Lab., Denmark, 1980: 35
13 Humphreys P J. In: Chandra T ed., Recrystallization'90. The Minerals, Metals & Society 1990: 113
[1] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[2] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[3] ZHOU Hongwei, GAO Jianbing, SHEN Jiaming, ZHAO Wei, BAI Fengmei, HE Yizhu. Twin Boundary Evolution Under Low-Cycle Fatigue of C-HRA-5 Austenitic Heat-Resistant Steel at High Temperature[J]. 金属学报, 2022, 58(8): 1013-1023.
[4] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[5] WU Xiang,ZUO Xiurong,ZHAO Weiwei,WANG Zhongyang. Mechanism of TiN Fracture During the Tensile Process of NM500 Wear-Resistant Steel[J]. 金属学报, 2020, 56(2): 129-136.
[6] Yan YANG, Guangyu YANG, Shifeng LUO, Lei XIAO, Wanqi JIE. Microstructures and Growth Orientation of Directionally Solidification Mg-14.61Gd Alloy[J]. 金属学报, 2019, 55(2): 202-212.
[7] Siqian BAO, Bingbing LIU, Gang ZHAO, Yang XU, Shanshan KE, Xiao HU, Lei LIU. Three-Dimensional Morphologies of Abnormally Grown Goss Oriented Grains in Hi-B Steel During Secondary Recrystallization Annealing[J]. 金属学报, 2018, 54(6): 877-885.
[8] Tingguang LIU, Shuang XIA, Qin BAI, Bangxin ZHOU. Morphological Characteristics and Size Distributions of Three-Dimensional Grains and Grain Boundaries in 316L Stainless Steel[J]. 金属学报, 2018, 54(6): 868-876.
[9] Yanyu LIU, Pingli MAO, Zheng LIU, Feng WANG, Zhi WANG. Theoretical Calculation of Schmid Factor and Its Application Under High Strain Rate Deformation in Magnesium Alloys[J]. 金属学报, 2018, 54(6): 950-958.
[10] Yang XU,Siqian BAO,Gang ZHAO,Xiangbin HUANG,Rusheng HUANG,Bingbing LIU,Nana SONG. Three-Dimensional Morphologies of Different Oriented Grains in Hi-B Steel Formed During Early Stage of Secondary Recrystallization Annealing[J]. 金属学报, 2017, 53(5): 539-548.
[11] Xiancui LIU, Ye PAN, Zhijiao TANG, Weiqiao HE, Tao LU. Microstructure Control and High Temperature Properties of Al-Mn-Based Alloys[J]. 金属学报, 2017, 53(11): 1487-1494.
[12] Quan FU,Yuhui SHA,Zhenghua HE,Fan LEI,Fang ZHANG,Liang ZUO. Recrystallization Texture and Magnetostriction in Binary Fe81Ga19 Sheets[J]. 金属学报, 2017, 53(1): 90-96.
[13] Lina WANG,Ping YANG,Weimin MAO. ANALYSIS OF MARTENSITIC TRANSFORMATIONDURING TENSION OF HIGH MANGANESETRIP STEEL AT HIGH STRAIN RATES[J]. 金属学报, 2016, 52(9): 1045-1052.
[14] Yue HE,Song XIANG,Wei SHI,Jianmin LIU,Yu LIANG,Chaoyi CHEN. EFFECT OF MICROSTRUCTURAL EVOLUTION ON THE PITTING CORROSION OF COLD DRAWING PEARLITIC STEELS[J]. 金属学报, 2016, 52(12): 1536-1544.
[15] Gongtao LIU,Ping YANG,Weimin MAO. EFFECT OF FINAL ANNEALING ATMOSPHERE ON SECONDARY RECRYSTALLIZATION BEHAVIOR IN THIN GAUGE MEDIUM TEMPERATURE GRAIN ORIENTED SILICON STEEL[J]. 金属学报, 2016, 52(1): 25-32.
No Suggested Reading articles found!