SOLID-STATE JOINING OF TiAl BASED ALLOYS
HE Yuehui;HUANG Baiyun;WANG Bin;LIU Yong;WANG Jiannong(State Key Laboratory for Powder Metallurgy;Central South University of Technology; Changsha 410083) GUO Jingjie (Materials Science College; Harbin University of Technology; Harbin 150001)
Cite this article: 

HE Yuehui;HUANG Baiyun;WANG Bin;LIU Yong;WANG Jiannong(State Key Laboratory for Powder Metallurgy;Central South University of Technology; Changsha 410083) GUO Jingjie (Materials Science College; Harbin University of Technology; Harbin 150001). SOLID-STATE JOINING OF TiAl BASED ALLOYS. Acta Metall Sin, 1998, 34(11): 1167-1172.

Download:  PDF(1862KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Solid-state joining between TiAl based alloy samples with various microstructures was investigated. When joining between coarse-grained TiAl based alloys, a fine recrystallized microstructure, which was different from those of the substrates, formed in the joining interface. When joining between a coarse-grained TiAl based alloy and an alloy of fine duplex microstructure, the coarse-grained part was penetrated by the fine-grained part due to its high superplasticity, and good joining interface was obtained. When solid joining between fine-grained parts, because both parts had high superplasticity, perfect joining interface with the microstructure of substrate was obtained through grains sliding in thermal plastic deformation, and the joining component had high mechanical properties (σba=533 MPa and δ≈2%). So all the fracture occurred away from the joining interface.
Key words:  TiAl based alloy      welding      mechanical property      microstructure     
Received:  18 November 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I11/1167

1Lipsitt H A. Metall Trans, 1975;6A:1991
2信木稔,桥本健纪,还本得藏,浅并羲一.日本金属学会志,1986;50(9):840(Nobuki M,Hashimoto K,Tsujimoto T,Azai Y.J Jpn Inst Met, 1986; 50(9): 840)
3笠原和男,桥本健纪,土肥春夫,还本得藏.日本金属学会志.1989;53(1):58(Kashar K,hashimoto K,Doi H,Tsujimoto T. J Jpn Inst Met,1989;53(1):58)
4Koepee C. Metall Trans; 1993; 24A: 1795
S He Y H,Huang B Y.Acta Metall Sin,1997;234:369
6贺跃辉,黄伯云.材料研究学报,1996;(6):606(He Y H, Huang B Y. Chin J Mater Res,1996;(6):606)
7 Baeslack W A. Weld J, 1989; 68(12):4835
8David S A. Weld J, 1990; 69(4):133S
9 Cieslak M J. Metall Trans,1990; 21A:1273
10 Nakao Y.ISIJ Int,1991; 31(10):1260
11 Baselack W A.Mater Charact,1994;33:357
12 Uenishi K.Z Metallk,1995;86(1):64
13 Cam G JOM, 1996; 11: 66(
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[6] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[9] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[10] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[11] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[12] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[13] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[14] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[15] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
No Suggested Reading articles found!