Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (10): 1009-1015    DOI:
Current Issue | Archive | Adv Search |
FINE STRUCTURE AND CRYSTALLOGRAPHY OF ISOTHERMAL LOWER BAINITE IN AN EXPERIMENTAL STEEL 38Si2Mn2Mo
LUO Chengping(C.P.Luo);LIU Jiangwen;XIAO Xiaoling(Department of Mechanical Engineering; South China University of Technology; Guangzhou 510641)Correspondent:LUO Chengping; professor; Tel:(020)85511617; Fax: (020)87111312;E-mail: mecpluo@letterbox.scut.edu.cn
Cite this article: 

LUO Chengping(C.P.Luo);LIU Jiangwen;XIAO Xiaoling(Department of Mechanical Engineering; South China University of Technology; Guangzhou 510641)Correspondent:LUO Chengping; professor; Tel:(020)85511617; Fax: (020)87111312;E-mail: mecpluo@letterbox.scut.edu.cn. FINE STRUCTURE AND CRYSTALLOGRAPHY OF ISOTHERMAL LOWER BAINITE IN AN EXPERIMENTAL STEEL 38Si2Mn2Mo. Acta Metall Sin, 1998, 34(10): 1009-1015.

Download:  PDF(2418KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The fine structure and crystallography of lower bainite produced in an exgerimental steel 38Si2Mn2Mo isothermally treated at 320℃ were studied using TEM. The lowerbainite contained midrib, subunit, retained austeuite and ε-carbide, and high density of dislocation exist in both the bainite and retained austenite. The habit plane (HP) of the bainitemeasured by double edge-on trace analysis was found ciose to {11,7,15}f, while its orieatationrelationship (OR) with the austeuite matrix was the G-T one. The bainite plates were related toeach other by a relative rotation of about 54.7° or 60° about the normal to their common planes{110}b, which resulted in an approtoate {112}b twin relationship between adjjacent plates. TheOR and HP of the lower bainite were found identical with, and close to tho1122se of the lath martensiterespectively, all in reasonable agreement with the predictions from the phenomenological theoryof martensite crystallography (PTMC). All these results show that the bainitic transformationpossesses the characters of matensitic transformation.
Key words:  steel 38Si2Mn2Mo      lower bainite      fine structure      TEM      phenomenological theory of martensite crystallography     
Received:  18 October 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I10/1009

1 Hehemann R F, Kinsmann K R, Aaronson H I. Metall Trans, 1972; 5A:1077
2 Cohen M, Bhadeshia H K D H, Aaronson H I. Metall Trans, 1990; 21A: 767, 2369
3 Wayman C M, Aaronson H I, Hirth J P. Metall Trans, 1994; 25A: 1787, 2655
4 Sriniruan G R, Wayman C M. Acta Metall, 1968; 16: 621
5 Luo C P, Weatherly G C, Liu Z Y. Metall Trans, 1992; 23A: 1403
6 Rao Narasimha B V. Metall Trans, 1979; 10A: 645
7 罗承萍, 许麟康,查健中.金属学报,,1993; 29: A312(Luo C P, Xu L K, Zha J Z. Acta Metall Sin, 1993; 29: A312)
8 罗承萍,肖晓玲,吴东晓自然科学进展,1997;7:612(Luo C P, Xiao X L, Wu D X. Prog Nat Sci, 1997; 7: 612)
9 Bowels M S, Mackenzie J K. Acta Metall,1954; 2: 29
10 Wechsler M S, lieberman D S, Read T A. Trans AIME 1960; 218: 202
11 Hehemann R F. Phase Transformation. Metals Park, Ohio: ASM,1970: 397
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[3] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[4] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[5] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[6] WANG Hanyu, LI Cai, ZHAO Can, ZENG Tao, WANG Zumin, HUANG Yuan. Direct Alloying of Immiscible Tungsten and Copper Based on Nano Active Structure and Its Thermodynamic Mechanism[J]. 金属学报, 2023, 59(5): 679-692.
[7] SHAO Xiaohong, PENG Zhenzhen, JIN Qianqian, MA Xiuliang. Unravelling the {101¯2} Twin Intersection Between LPSO Structure/SFs in Magnesium Alloy[J]. 金属学报, 2023, 59(4): 556-566.
[8] WANG Di, HE Lili, WANG Dong, WANG Li, ZHANG Siqian, DONG Jiasheng, CHEN Lijia, ZHANG Jian. Influence of Pt-Al Coating on Tensile Properties of DD413 Alloy at High Temperatures[J]. 金属学报, 2023, 59(3): 424-434.
[9] CHENG Yuanyao, ZHAO Gang, XU Deming, MAO Xinping, LI Guangqiang. Effect of Austenitizing Temperature on Microstructures and Mechanical Properties of Si-Mn Hot-Rolled Plate After Quenching and Partitioning Treatment[J]. 金属学报, 2023, 59(3): 413-423.
[10] SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang. Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys[J]. 金属学报, 2023, 59(3): 371-386.
[11] MIAO Junwei, WANG Mingliang, ZHANG Aijun, LU Yiping, WANG Tongmin, LI Tingju. Tribological Properties and Wear Mechanism of AlCr1.3TiNi2 Eutectic High-Entropy Alloy at Elevated Temperature[J]. 金属学报, 2023, 59(2): 267-276.
[12] WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei. Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K[J]. 金属学报, 2023, 59(2): 277-288.
[13] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[14] CHEN Jilin, FENG Guanghong, MA Honglei, YANG Dong, LIU Wei. Microstructure, Mechanical Properties, and Strengthening Mechanism of Cr-Mo Microalloy Cold Heading Steel[J]. 金属学报, 2022, 58(9): 1189-1198.
[15] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
No Suggested Reading articles found!