MICROSTRUCTURE AND MORPHOLOGY OF PHASES IN LASER REMELTING CERAMIC COATINGS
WU Qiuhong;TAO Zengyi;CUI Kun(Huazhong University of Science and Technology;Wuhan 430074);HE Lianlong;LI Douxing;YE Hengqiang(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1994-07-28;in revised form 1995-03-01)
Cite this article: 

WU Qiuhong;TAO Zengyi;CUI Kun(Huazhong University of Science and Technology;Wuhan 430074);HE Lianlong;LI Douxing;YE Hengqiang(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1994-07-28;in revised form 1995-03-01). MICROSTRUCTURE AND MORPHOLOGY OF PHASES IN LASER REMELTING CERAMIC COATINGS. Acta Metall Sin, 1995, 31(11): 508-512.

Download:  PDF(379KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Microstructure,morphology and composition of the phases in 2 kW laser remelted Al_2O_3-13wt-%TiO_2 ceramic coatings on ICr18Ni9Ti substrate were examined by using electron diffraction, diffraction contrast image and EDAX. Results showed that TiO_2 and a part of Al_2O_3 formed Al_2TiO_5 and a superlattice phase appeared in the ceramic layer;a little alloy element of substrate permeated into α-Al_2O_3 and replaced only a part of Ti in Al_2TiO_5.The distribution and morphology of α-Al_2O_3 and Al_2TiO_5 were related with the distance from surface.The shape of Al_2TiO_5 was strip near surface and block near substrate,and the farther from surface,and the more Al_2TiO_5 in the coatings.
Key words:  laser remelting      Al_2O_3 ceramic coating      microstructure     
Received:  18 November 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I11/508

1樱井良文,小泉光慧编,陈俊彦,王余君译,新型陶瓷材料及应用,北京:中国建筑工业出版社,1983:202戴安邦,沈孟长.元素周期表.上海:上海科学技术出版社,1979:13MosinB,LynchRW,ActaCrystallogr,1972;B28:10404饶东生.硅酸盐物理化学,北京:冶金工业出版社,1980:20b
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[4] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[11] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[12] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[13] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[14] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!