CYCLIC DEFORMATION BEHAVIOUR OF Ni_3(Al,Zr) SINGLE CRYSTAL AT ROOM TEMPERATURE |
GU Yuefeng;LIU Yi;LIN Dongliang(T.L.Lin)(Shanghai Jiaotong University;Shanghai 200030);GUO Jianting(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-01-13;in revised form 1995-07-03) |
|
Cite this article:
GU Yuefeng;LIU Yi;LIN Dongliang(T.L.Lin)(Shanghai Jiaotong University;Shanghai 200030);GUO Jianting(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-01-13;in revised form 1995-07-03). CYCLIC DEFORMATION BEHAVIOUR OF Ni_3(Al,Zr) SINGLE CRYSTAL AT ROOM TEMPERATURE. Acta Metall Sin, 1995, 31(11): 513-518.
|
Abstract Fully reversed strain-controlled tension-compression tests were performed at room temperature to study cyclic-deformation properties of Ni_3(Al,Zr) single crystal.Both cyclic strain hardening and a tension-compression flow stress asymmetry were recorded,the stress asymmetry becomes more prominent as the strain amplitude becomes larger;the cyclic hardening can divide into initiation and saturation stages.TEM observation showed that there are a profusion superlattic intrinsic stacking faults(SISFs) in fatigued Ni_3(Al,Zr) single crystal samples.The cyclic strain hardening is explained by the dislocation structure.
|
Received: 18 November 1995
|
1GuardKW,WestbrookJH,TransAIME,1959;215:8072Noguchi,OyaY,SuzukiT.MetallTrans,1981;12A:16473EzzSS,PopeDP.ScrMetall,1985;19:7414BondaNR,PopeDP,LairdC,ActaMetall,1987;35:23715BondaNR,PopeDP,LairdC.ActaMetall,1987;35:23856HsiungLM,StoloffNS.ActaMetallMater,1990;38:11917谷月峰.上海交通大学博士学位论文,上海,19948TakeuchiS,KuramotoE,YamamotoT,TaokaT.JpnJApplPhys,1973;12:4869BakerI,SchulsonEM.PhysStatusSolid,1985;a89:16310YanW,JonesIP,SmallmanRE.PhysStatusSolid,1991;a125:46911ChibaA,HanadaS.PhilosMag,1994;A69:75112MughrabiH,WuthrichC.PhilosMag,1976;A33:96313PakHR,HsiungLM,KatoM.In:KochCC,LiuCT,StoloffNSeds.,HighTemperatureOrderIntermetallicAlloy,Vol.39,Pittsburgh,PA:MRS,1985:23914LallC,ChinS,PopeDP.MetallTrans,1979;10A:132315PlcquerasJ,GrosskreutzJC,FrankW.PhysStatusSolid,1972;a11:56716BauschingerJ.Civilingenieur,1981;27:28917YamaguchiM,PaidarV,PopeDP,VitekV.PhilosMag,1982;45:86718PaidarV,YamaguchiM,PopeDP,VitekV.PhilosMag,1982;45:883 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|