EFFECT OF Cu ON MICROSTRUCTURE AND PROPERTIES OF Al-Li ALLOYS
YAO Daping;HU Zhuangqi;LI Yiyi;ZHANG Yun;SHI Changxu Institute of Metal Research; Academia Sinica; Shenyang Institute of Metal Research;Academia Sinica; Shenyang 110015
Cite this article: 

YAO Daping;HU Zhuangqi;LI Yiyi;ZHANG Yun;SHI Changxu Institute of Metal Research; Academia Sinica; Shenyang Institute of Metal Research;Academia Sinica; Shenyang 110015. EFFECT OF Cu ON MICROSTRUCTURE AND PROPERTIES OF Al-Li ALLOYS. Acta Metall Sin, 1990, 26(2): 21-25.

Download:  PDF(2264KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The aging precipitation structure and its properties of the Al-Li-Cu-Zr alloys with 3 different Cu/Li ratios have been studied. Experimental resultsshow that the aging hardening of the alloys consists of two steps: the first is stre-ngthened by δ'-phase (δ'+T_1 phase in alloy No.3), and the second by δ'+T_1 phase(δ'+T_1+θ' phase in alloy No.3). The plate of T_1-phase can absorb the Li atomsfrom δ' particles when the plate bumped into δ"-phase, and therefore, these δ' pha-se particles become smaller and gradually disappear. The strength and hardness areincreased with the increase of Cu/Li ratio which cuased a decrease in plasticity.The crack mode would change from transgranular to intergranular. This is due to theprecipitation of the equilibrium phases contained Cu at grain boundaries.
Key words:  Al-Li alloy      aging hardening      microstructure      tensile properties     
Received:  18 February 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I2/21

1 Silcock J M. J Inst Met, 1959--60; 88: 357
2 Starke E A Jr., Sanders T H Jr., Palmer I G. J Met, 1981; 33 (8) : 24
3 Huang J C, Ardell A J. J Phys (Paris), 1987; 48 (C3) : 373
4 Cassada W A, Shiflet G J, Starke E A Jr. J Phys (Paris). 1987; 48 (C3) : 397
5 Tosten M H, Vasudevan A K, Howell P R. Metall Trans, 1988; 19A: 51
6 Yao D P, Li Y Y, Hu Z Q, Zhang Y, Shi C X. In: Sanders T H Jr., Starke E A Jr. eds., Aluminum-Lithium Alloys V, Materials Component Engineering Publication Ltd., UK, 1989: 153
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[6] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[11] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[12] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[13] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[14] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[15] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
No Suggested Reading articles found!