Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (2): 26-30    DOI:
论文 Current Issue | Archive | Adv Search |
STATISTICAL EVALUATION OF CRITICAL INCLUSION FACTOR FOR SECONDARY RECRYSTALLIZATION IN 3% Si STEEL
LI Shuchen;CHEN Mengzhe;KE Jun Southwestern Jiaotong University; Chengdu University of Science and Technology Beijing Department of Materials Engineering;Southwestern Jiaotong University; Chengdu; Sichuan 610031
Cite this article: 

LI Shuchen;CHEN Mengzhe;KE Jun Southwestern Jiaotong University; Chengdu University of Science and Technology Beijing Department of Materials Engineering;Southwestern Jiaotong University; Chengdu; Sichuan 610031. STATISTICAL EVALUATION OF CRITICAL INCLUSION FACTOR FOR SECONDARY RECRYSTALLIZATION IN 3% Si STEEL. Acta Metall Sin, 1990, 26(2): 26-30.

Download:  PDF(1142KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

On the basis of statistical data of MnS in the conventional 3%Sisteel sheets after various annealing processes, the critical inclusion factor has beenevaluated to be 20mm~(-1). The inhibition of MnS to grain growth has been moreexactly described.

Key words:  3%Si steel      secondary recrystallization      inclusion factor     
Received:  18 February 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I2/26

1 May J E, Turnbull D. Trans AIME, 1958; 212: 769
2 Hillert M. Acta Metall, 1965; 13: 227
3 Gladman T. Proc Royal Soc London, 1966; A294: 298
4 Matsuoka T. Trans Iron Steel Inst Jpn, 1967; 7 (1) : 19
5 Swin W M. Metall Trans, 1973; 4: 841
6 陈易之,马黛,葛明,王谔身.金属学报,1978;14:33
7 Flowers J W. IEEE Trans Magn, 1979; MAG-15 (5) : 1601
8 Nielsen J P. Recrystallization, Grain Growth and Textures, Metals Park, Ohio: ASM, 1966: 141
9 Smith C S. Trans AIME, 1948; 175: 15
10 Hellman P, Hillert M. Scand J Metall, 1975; 4: 211

[1] XU Zhanyi, SHA Yuhui, ZHANG Fang, ZHANG Huabing, LI Guobao, CHU Shuangjie, ZUO Liang. Orientation Selection Behavior During Secondary Recrystallization in Grain-Oriented Silicon Steel[J]. 金属学报, 2020, 56(8): 1067-1074.
[2] Siqian BAO, Bingbing LIU, Gang ZHAO, Yang XU, Shanshan KE, Xiao HU, Lei LIU. Three-Dimensional Morphologies of Abnormally Grown Goss Oriented Grains in Hi-B Steel During Secondary Recrystallization Annealing[J]. 金属学报, 2018, 54(6): 877-885.
[3] Yang XU,Siqian BAO,Gang ZHAO,Xiangbin HUANG,Rusheng HUANG,Bingbing LIU,Nana SONG. Three-Dimensional Morphologies of Different Oriented Grains in Hi-B Steel Formed During Early Stage of Secondary Recrystallization Annealing[J]. 金属学报, 2017, 53(5): 539-548.
[4] Gongtao LIU,Ping YANG,Weimin MAO. EFFECT OF FINAL ANNEALING ATMOSPHERE ON SECONDARY RECRYSTALLIZATION BEHAVIOR IN THIN GAUGE MEDIUM TEMPERATURE GRAIN ORIENTED SILICON STEEL[J]. 金属学报, 2016, 52(1): 25-32.
[5] YAN Mengqi QIAN Hao YANG Ping SONG Huijun SHAO Yuanyuan MAO Weimin. BEHAVIORS OF BRASS TEXTURE AND ITS INFLUENCE ON GOSS TEXTURE IN GRAIN ORIENTED ELECTRICAL STEELS[J]. 金属学报, 2012, 48(1): 16-22.
[6] ZHAO Yu; HE Zhongzhi; WENG Yuqing; WU Baorong (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). GRAIN BOUNDARY SEGREGATION OF TRACE Sn IN HIGH INDUCTION ORIENTED SILICON STEEL[J]. 金属学报, 1992, 28(8): 1-6.
No Suggested Reading articles found!