Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (6): 22-29    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF Zr, Cr AND B ADDITIVES ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ni_3 Al ALLOYS
GUO Jianting;LI Hui;SUN Chao;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang GUO Jianting; associate professor; Institute of Metal Research; Academia Sinica;Shenyang 110015
Cite this article: 

GUO Jianting;LI Hui;SUN Chao;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang GUO Jianting; associate professor; Institute of Metal Research; Academia Sinica;Shenyang 110015. EFFECT OF Zr, Cr AND B ADDITIVES ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ni_3 Al ALLOYS. Acta Metall Sin, 1989, 25(6): 22-29.

Download:  PDF(2509KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure and the mechanical properties from room temper-ature up to 1050℃ of Ni_3Al base alloys containing 0--0.6 at.-%Zr, 0--7.7 at.-%Crand 0--2.22 at.-%B have been investigated. It was found that the temperature depen-dence of their yield strength variation reveals to be anomalous, i. e., the strengthincreases with the elevating of temperature, and thence decreases till it surpassedthe peak value. Both Zr and Zr + Cr may improve the yield strength of thealloys in the entire range or testing temperatures, as well as the tensile strengthand elongation under high temperature. B is favourable to raise the tensile andyield strength of the alloys, and also the plasticity. But the strength will reduce asB added over 1.37 at.-%. The Ni_(20)Al_3B_6 and Ni_3Al eutectic mixture like islandsand globes precipitated inside grain and along grain boundaries, which are harmfulto the strength and ductility, may be formed when the B content exceeds the limitof solubility.
Key words:  Ni_3Al      microstructure      mechanical properties      yield strength     
Received:  18 June 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I6/22

1 青木清,和泉修.日本金属学会志,1979;43: 1190
2 Liu C T, Sikka V K. J Met, 1986; 38(5) : 19
3 Hsu S E, Hsu N N, Tong C H, Ma C Y. Lee S Y. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds., Proc MRS Symp. High-Temperature Ordered Intermetallic Alloys Ⅱ, Vol. 81, Mars, Pennsylvania: MRS, 1987: 507
4 Liu C T, White C L, Horton J A. Acta Metall. 1985; 33: 213
5 Ochiai S, Oya Y, Suzuki T. Acta Metall, 1984; 32: 289
6 Ochiai S, Mishima Y, Yodogawa M, Suzuki T. Trans Jpn Inst Met, 1986: 27: 32
7 Chang K M, Huang S C, Taub A I. GE-CRD Report No. 86CRD202, 1986
8 Ogura T, Hanada S, Masumoto T, Izumi O. Metall Trans, 4, 1985; 16A: 441
9 李辉,刘祥,郭建亭,胡壮麒.金属学报,1989;25:A25
10 Schulson E M, Baker I, Frost H J. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds., Proc MRS Symp. High-Temperature Ordered Intermetallic Alloys Ⅱ, Vol. 81, Mars. Pennsylvania: MRS, 1987: 195
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[11] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[12] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[13] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[14] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[15] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
No Suggested Reading articles found!