| TRANSFORMATION OF TWO WAY SHAPE MEMORY MATERIAL CONSTRAINED BY STRESS |
| LIN Guangming;HUANG Yuanshi;ZHANG Jinxiu Zhongshan University; Guangzhou LIN Guangming; Associate Professor; Department of Physics; Zhongshan University;Guongzhou 510275 |
|
Cite this article:
LIN Guangming;HUANG Yuanshi;ZHANG Jinxiu Zhongshan University; Guangzhou LIN Guangming; Associate Professor; Department of Physics; Zhongshan University;Guongzhou 510275. TRANSFORMATION OF TWO WAY SHAPE MEMORY MATERIAL CONSTRAINED BY STRESS. Acta Metall Sin, 1989, 25(6): 16-21.
|
|
|
Abstract The snap-acting transition and snap-acting two way shape memory(TWSM) effect have been obtained in a TWSM spring made of Ni51Ti49 alloyusing the constrained effect of stress on the driving force of TWSM element. Whenthe snap-acting transition has been realized, M_s=M_f and A_s=A_f; hysteresis is rec-tangular, the height (TWSM effect) and width (hysteresis) of the rectangle can bereadjusted by means of constrained stress. The results of resistance measurementsshow that the snap acting TWSM effect mentioned above was supplied mainlyfrom the transformation of P-R. The gradients of the driving force with respectto temperature near critical point have been calculated. The thermodynamic modelhas been proposed to account for the snap-acting transformation.
|
|
Received: 18 June 1989
|
1 铃木雄一,关口行雄.见,舟久保熙康编,形状记忆合金,东京:产业图书店,1984:143 2 Otsuka K, Shimizu K. Int Metall Rev, 1986; 31: 93 3 Delaey L, Aernoudt E. Proc of the ICOMAT-86, held at Nara, Japan, The Japan Institute of Metals, 1987: 926 4 林光明,傅刚.第二届形状记忆合金讨论会论文集,北京:中国有色金属学会,1988 5 罗来忠,张进修,林光明.金属学报,1989;25A153 6 罗来忠,张进修,林光明.发明专利,申请号:87102326,1987 7 林光明,张进修,黄元士.实用新型专利公报,1988;4(31) :88(申请号:87214828) 8 Hwang C M, Wayman C M. J Phys (Paris), 1982; C4: 231 9 铃木雄一.工业材料,1983;31(1) :72 10 张进修,李江宏.物理学报.1988;37:363 11 Wayman C M. Proc of Int Meeting on Advanced Materials, held at Tokyo, Japan, 1988, Materials Research Society, (to be published) |