Acta Metall Sin  1989, Vol. 25 Issue (5): 124-132    DOI:
Current Issue | Archive | Adv Search |
STEREOLOGICAL CHARACTERIZATION OF MICROSTRUCTURAL EVOLUTION AT LATE STAGES OF SINTERING FOR NICKEL POWDER COMPACTS
LIU Guoquan ;R. T. DEHOFF University of Science and Technology Beijing University of Florida; USA LIU Guoquan; Dept. of Materials Science and Engineering ;Universityof Science and Technology Beijing; 100083 Beijing
Cite this article: 

LIU Guoquan ;R. T. DEHOFF University of Science and Technology Beijing University of Florida; USA LIU Guoquan; Dept. of Materials Science and Engineering ;Universityof Science and Technology Beijing; 100083 Beijing. STEREOLOGICAL CHARACTERIZATION OF MICROSTRUCTURAL EVOLUTION AT LATE STAGES OF SINTERING FOR NICKEL POWDER COMPACTS. Acta Metall Sin, 1989, 25(5): 124-132.

Download:  PDF(1293KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The evolution of both the metric and topological properties of themicrostructure for Ni powder compacts at the late stage of sintering (V_v~5>0.90) hasbeen investigated by means of stereological methods. The effects of precompactionpressure and loose sintering have been studied and discussed.
Key words:  sintering      microstructure      stereology     
Received:  18 May 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I5/124

1 DeHoff R T, Rhines F N. Quantitative Microscopy, New York: McGraw-Hill, 1968
2 Underwood E E. Quantitative Stereology, Reading, Mass: Addison-Wesley, 1970
3 Rhines F N, DeHoff R T, Kronsbein J. A Topological Study of the Sintering Process, Final Report, U S Atomic Energy Commission Contract No. AT-(40-1) -2581, Dec., 1969
4 DeHoff R T. In: Proc 4th Int Congress for Stereology, Nat Bur Stand (U S), Spec. Publ. 431. Washinglon: U S Government Printing Office, 1976: 439
5 Rhines F N, Craig K R, DeHoff R T. Metall Trans, 1974; 5: 413
6 Watwe A S, De Hoff R T. In: Microstructural Science, Vol. X, New York: Elsevier, 1982: 317
7 Hu H, Rath B B. Metall Trans, 1970; 1: 3181
8 Smith C S. Guttman L. Trans AIME, 1953; 197: 81
9 Hsueh C H, Evans A G, Coble R L. Acta Metall, 1982; 30: 1269
10 Aigeltinger E H, Exner H E. Metall Trans, 1977; 8A: 421
11 Watwe A S. Ph. D Dissertation, University of Florida, 1983
12 Rhines F N. In: Benesovsky F ed, Plansee Proceedings, 1958, Third Plansee Seminar, Reutte/Tyrol Springer-Verlay, 1958: 38
13 Lenel F V. Powder Metallurgy Principles and Applications Princeton, New Jersey: Metal Powder Industries Federation, 1980: 242
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[11] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[14] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[15] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
No Suggested Reading articles found!