Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (6): 487-493    DOI:
Current Issue | Archive | Adv Search |
UNUSUAL SOLIDIFICATION MICROSTRUCTURE OF Fe_(70)Cr_(18)Mo_2Si_1B_9 SINGLE-ROLL QUENCHED RIBBON
LIN Yijian;YOU Yunlong;ZHANG Xiaomin;JING Chunyong;YU Quanqin Shanghai Iron and Steel Research Institute
Cite this article: 

LIN Yijian;YOU Yunlong;ZHANG Xiaomin;JING Chunyong;YU Quanqin Shanghai Iron and Steel Research Institute. UNUSUAL SOLIDIFICATION MICROSTRUCTURE OF Fe_(70)Cr_(18)Mo_2Si_1B_9 SINGLE-ROLL QUENCHED RIBBON. Acta Metall Sin, 1988, 24(6): 487-493.

Download:  PDF(1413KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The solidification microstructure of Fe_(70)Cr_(18)Mo_2Si_1B_9 single-roll quench-ed ribbons with different rotating speed of roller and under different atmosphereconditions was investigated. Apart from usual crystallization by homogeneous andheterogeneous nucleation, it was found that α-iron columnar grains with strongpreferred orientation formed beneath free surface and that spheres of α-iron singlecrystal with a size of several μm up to 20 μm, which have rarely been reported,appeared inside the ribbons. There was experimental evidence suggesting that clust-ers of metal atoms formed from fluctuation in early undercooled liquid might playa role as pre-existed nuclei and, in fact, control. the formation of amorphous forthis alloy.
Key words:  Fe_(70)Cr_(18)Mo_2Si_1B_9      single-roll quenched ribbon      microstructure     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/487

1 Ray R. Mater Sci Eng, 1982; 52: 85
2 Koster U, Herold U. In: Masumoto T et al. eds., Proc 4th Int Conf on the Rapidly Quenched Metals, Sendai, 1981, Japan: The Japan Institute Metals, 1982: 717
3 林一坚,尤云龙,张小岷,井春永,严守平,章靖国.金属学报,1987;23:A326
4 Kunimasa Takeshita, Paul Hideo Shingu. Trans Jpn Inst Met, 1983; 24: 529
5 Kunimasa Takeshita, Paul Hideo Shingu. Trans Jpn Inst Met, 1986; 27: 141
6 Hideo Shingu P, Kobayashi K, Sukuki R, Takashita K. In: Masumoto T et al eds., Proc 4th Int Conf on the Rapidly Quenched Metals, Sendai, 1981, Japan: The Japan Institute Metals, 1982: 57
7 Neumann W, Leonhardt M, Loser W, Sellger R, Jurisch M. J Mater Sci, 1985; 20; 3141
8 胡坚,许嘉龙,张士勋,章靖国.上海钢铁研究所硕士论文,1987
9 胡汉起.金属凝固,冶金工业出版社,1985
10 Bergmann H W, Fritsch H U. Met Sci, 1982; 16: 197
11 Kemeny T, Vincze I, Fogarassy B. Phys Rev B, 1979; 20: 476
12 Vincze I, Boudreaux D S, Tegze M. Phys Rev B, 1979; 19: 4896
13 长田和雄,井野博满.日本金属学会志,1985;49:402
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[6] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[11] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[12] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[13] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[14] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[15] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
No Suggested Reading articles found!