Acta Metall Sin  1988, Vol. 24 Issue (6): 494-498    DOI:
论文 Current Issue | Archive | Adv Search |
METASTABLE CHARACTERISTICS OFβ-W
HUANG Huimin;CHEN Xinmin Central South University of Technology; Changsha
Cite this article: 

HUANG Huimin;CHEN Xinmin Central South University of Technology; Changsha. METASTABLE CHARACTERISTICS OFβ-W. Acta Metall Sin, 1988, 24(6): 494-498.

Download:  PDF(372KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The nature of the oxygen contained in β-W was investigated withDSC, X-ray analysis on quenched samples and Auger spectroscope. It was shownthat the oxygen contained in nonpyrophoric β-W consists of the reversiblychemisorbed oxygen and the interstitial oxygen which could form an interstitialsolid solution with β-W. It seems better to consider β-W to be a metaphase of Wwith theinterstitial oxygen as stabilizer.

Key words:  tungsten      beta-tungsten      metastable phase      interstitial solid solution     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/494

1 Hartmann H, Ebert F, Bretshneider O. Z Anorg Allg Chem, 1931; 198: 116 2 Hagg G, Schonberg N. Acta Crystallogr, 1954; 7: 351 3 黄慧民,陈新民.中南矿冶学院学报,1987;18(4) :459 4 Barin I, Knacke O. Thermochemical Properties of Inorganic Substances, Berlin: Springer-verlag, 1973: 857
[1] LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun. Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion[J]. 金属学报, 2023, 59(8): 986-1000.
[2] SUN Jiaxiao, YANG Ke, WANG Qiuyu, JI Shanlin, BAO Yefeng, PAN Jie. Microstructure and Mechanical Properties of 5356 Aluminum Alloy Fabricated by TIG Arc Additive Manufacturing[J]. 金属学报, 2021, 57(5): 665-674.
[3] Ping LI, Quan LIN, Yufeng ZHOU, Kemin XUE, Yucheng WU. TEM Analysis of Microstructure Evolution Process of Pure Tungsten Under High Pressure Torsion[J]. 金属学报, 2019, 55(4): 521-528.
[4] Tao ZHANG, Wei YAN, Zhuoming XIE, Shu MIAO, Junfeng YANG, Xianping WANG, Qianfeng FANG, Changsong LIU. Recent Progress of Oxide/Carbide Dispersion Strengthened W-Based Materials[J]. 金属学报, 2018, 54(6): 831-843.
[5] Yutian MA,Junbiao LIU,Rongling HUO,Li HAN,Geng NIU. RESEARCH ON THE PREPARATION AND PERFOR-MANCE OF TUNGSTEN-ALUMINUM TRANSMIS-SION TARGET FOR MICRO-COMPUTED TOMOGRAPHY BY MAGNETRONSPUTTERING[J]. 金属学报, 2015, 51(11): 1416-1424.
[6] Yutian MA,Junbiao LIU,Rongling HUO,Li HAN,Geng NIU. RESEARCH ON THE PREPARATION AND PERFOR-MANCE OF TUNGSTEN-ALUMINUM TRANSMIS-SION TARGET FOR MICRO-COMPUTED TOMOGRAPHY BY MAGNETRONSPUTTERING[J]. 金属学报, 2015, 51(11): 1416-1424.
[7] HUANG Lian, GAO Kunyuan, WEN Shengping, HUANG Hui, WANG Wei, NIE Zuoren. VALENCE ELECTRON STRUCTURE ANALYSIS OF EQUILIBRIUM AND METASTABLE PHASES OF Al3M(M=Ti, Zr, Hf)[J]. 金属学报, 2012, 48(4): 492-501.
[8] WANG Gang ZHENG Zhuo CHANG Litao XU Lei CUI Yuyou YANG Rui. CHARACTERIZATION OF TiAl PRE–ALLOYED POWDER AND ITS DENSIFICATION MICROSTRUCTURE[J]. 金属学报, 2011, 47(10): 1263-1269.
[9] JIN Tao SUN Xiaofeng ZHAO Nairen LIU Jinlai ZHANG Jinghua HU Zhuangqi. STUDY OF MICROSTRUCTURES IN γ/γ'--αMo DIRECTIONAL EUTECTOID ALLOY INDUCED BY LASER  RAPID MELTING SOLIDIFICATION[J]. 金属学报, 2009, 45(5): 527-535.
[10] LIN Sanbao SONG Jianling YANG Chunli MA Guangchao. MICROSTRUCTURE ANALYSIS OF INTERFACIAL LAYER WITH TUNGSTEN INERT GAS WELDING–BRAZING JOINT OF ALUMINUM ALLOY/STAINLESS STEEL[J]. 金属学报, 2009, 45(10): 1211-1216.
[11] Mingxia Liu; Yongfeng Hu; FEI MA; Kewei XU. COHERENT GROWTH OF α-W FILM ON Si WAFER AND ITS THICKNESS DEPENDENT MECHANICAL AND ELECTRICAL PROPERTIES[J]. 金属学报, 2008, 44(5): 631-635 .
[12] . STUDY OF BRAZING ALLOY USED IN BRAZING COMPOSITE ALLOY CLADDING REINFORCED WITH HARD PARTICLES[J]. 金属学报, 2007, 43(4): 433-438 .
[13] LI Jianguo; Hu Dongping; MEI Jun; LIU Shi; LI Yiyi. Enhancing Adhesion Between Diamond Film and WC--Co Substrate[J]. 金属学报, 2006, 42(7): 763-769 .
[14] PENG Ke; YI Maozhong; RAN Liping. Analysis of Valence Electronic Structures and Properties of MoSi2 And WSi2[J]. 金属学报, 2006, 42(11): 1125-1129 .
[15] YANG Mingchuan; SONG Zhenzhen; LU Ke. Synthesis of W--20%Cu Nanocomposite Powders[J]. 金属学报, 2004, 40(6): 639-.
No Suggested Reading articles found!