Abstract The evolution of microstructure and phase transformation in TC16 titanium alloy after solution and then quenching from 700 ℃ to 900℃ were investigated by XRD, SEM and TEM, and the corresponding tensile properties were also measured. The results reveal that TC16 titanium alloy consists of primary α phase, metastable β phase and small amount of ω phase when quenching at 700 and 750 ℃. With quenching temperature increasing, the phase transformation of β → α'' happens. The alloy is completely composed of α'' martensite when quenching from single β phase field. Tensile test shows the yield strength of metastable microstructure samples is lowered due to stress induced α'' martensitic transformation.
|
Received: 07 April 2011
|
|
[1] Zhang Q L, Wang Q R, Li X W. Mater Eng, 2007; 284: 11(张庆玲, 王庆如, 李兴无. 材料工程, 2007; 284: 11)[2] Ma Q Q, Zheng W W, Li X W. Mater Eng, 2009; 308: 19(马琴琴, 郑为为, 李兴无. 材料工程, 2009; 308: 19)[3] Li X W, Lu M X, Sha A X, Zhang L. Mater Sci Eng, 2008; A490: 193[4] Wu C Z, Li X W. Rare Met Mater Eng, 2008; 37(suppl.3): 580(吴崇周, 李兴无. 稀有金属材料与工程, 2008; 37(增3): 580)[5] Sha A X, Li X W, Li H E, Wang Q R. Chin J Nonferrous Met, 2010; 20: 943(沙爱学, 李兴无, 李红恩, 王清瑞. 中国有色金属学报, 2010; 20: 943)[6] Li X W, Sha A X, Chu J P, Zhang L, Lu M X. Mater Eng, 2007; 292: 3(李兴无, 沙爱学, 储俊鹏, 张雷, 路民旭. 材料工程, 2007; 292: 3)[7] Li X W, Su S M, Lu M X, Sha A X, Chu J P. J Aeronaut Mater, 2008; 28(3): 82(李兴无, 苏生明, 路民旭, 沙爱学, 储俊鹏. 航 空材料学报, 2008; 28(3): 82)[8] Sass S L. J Less–Common Met, 1972; 28: 157[9] Jones N G, Dashwood R J, Jackson M, Dye D. Acta Mater, 2009; 57: 3830[10] Boyer R, Welsch G, Collings E W. Materials Properties Handbook: Titanium Alloy. OH, Materials Park: ASM International, 1994: 41[11] Luetjering G, Williams J C. Titanium. Heidelberg: Springer, 2003: 30[12] Borisova E A et al, translated by Chen S Q. Metallography of Titanium Alloys. Beijing: National Defence Inductry Press, 1986: 327(鲍利索娃 E A 等著, 陈石卿 译. 钛合金金相学. 北京: 国防工业出版社, 1986: 327)[13] Duerig T W, Albrecht J, Richter D, Fishcher P. Acta Mater, 1982; 30: 2161[14] Duerig T W, Terlinde G T, Williams J C. Metall Trans, 1980; 11A: 1987[15] Grosdidier T, Philippe M J. Mater Sci Eng, 2000; A291: 218 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|