| 强磁场下电磁振荡对 Al--4.5%Cu合金凝固组织的影响 |
| 余建波 任忠鸣 任维丽 邓 康 王 俊 |
| (上海大学材料科学与工程学院; 上海 200072) |
|
| Effect of electromagnetic vibration on the structure in solidified Al-4.5%Cu alloy under a strong magnetic field |
| YU Jian-Bo |
| 上海大学 |
引用本文:
余建波; 任忠鸣; 任维丽; 邓康; 王俊 . 强磁场下电磁振荡对 Al--4.5%Cu合金凝固组织的影响[J]. 金属学报, 2008, 44(2): 172-176 .
,
,
,
,
.
Effect of electromagnetic vibration on the structure in solidified Al-4.5%Cu alloy under a strong magnetic field[J]. Acta Metall Sin, 2008, 44(2): 172-176 .
[1]Chen W P,Maeda H,Kakimoto K,Zhang P X,Watanabe K,Motokawa M,Kumakura H,Itoh K.J Cryst Growth, 1999;204:69 [2]Sassa K,Morikawa H,Asai S.J Jpn Inst Met,1997;61: 1283 (佐佐健介,森川拓,浅井滋生.日本金属学会志,1997;61:1283) [3]Sata H,Kimura T,Ogawa S,Yamato M,Ito E.Polymer, 1996;37:1879 [4]Kimura T,Kawai T,Sakamoto Y.Polymer,2000;41:809 [5]Suzuki T S,Sakka Y,Kitazawa K.Adv Eng Mater,2001; 3:44 [6]Suzuki T S,Sakka Y.Chem Lett,2002;31:1204 [7]Sugiyama T,Tahashi M,Sassa K,Asai S.ISIJ Int,2003; 43(6):855 [8]Vires C.Mater Sci Eng,1993;A173:169 [9]Radjai A,Miwa K,Nishio T.Metall Mater Trans,1998; 29A:1477 [10]Radjai A,Miwa K,Nishio T.Metall Mater Trans,2002; 33A:3025 [11]Takagi T,Iwai K,Asai S.ISIJ Int,2003;43(6):842 [12]Iwai K,Sugiura K.Mater Sci Forum,2005;475:2695 [13]Usui M,Iwai K,Asai S.ISIJ Int,2006;46:859 [14]Matsushima H,Nohira T,Mogi L.Surf Coat Technol, 2004;179:245 [15]Li X,Ren Z M,Sun Y H,Wang J,Yu J B,Ren W L.Acta Metall Sin,2006;42:147 (李喜,任忠鸣,孙延辉,王俊,余建波,任维丽.金属学报,2006;42:147) [16]Yu J B,Ren Z M,Deng K,Ren W L,Li X,Wang J.Chin Nonferrous Met,2007;17:92 (余建波,任忠鸣,邓康,任维丽,李喜,王俊.中国有色金属学报,2007;17:92) [17]Zhu Y M.J Instrum Mater,1982;13(6):25 (朱耀明.仪表材料,1982;13(6):25) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|