| 316L不锈钢强流脉冲电子束表面改性研究 Part I 表面选择净化及机理 |
| 张可敏;杨大智;邹建新;董闯 |
| 大连理工大学材料学院 |
|
| SURFACE MODIFICATION OF 316L STAINLESS STEEL BY HIGH CURRENT PULSED ELECTRON BEAM Part I Selective surface purification and its mechanism |
| ;;; |
| 大连理工大学材料学院 |
引用本文:
张可敏; 杨大智; 邹建新; 董闯 . 316L不锈钢强流脉冲电子束表面改性研究 Part I 表面选择净化及机理[J]. 金属学报, 2007, 42(1): 64-70 .
,
,
,
.
SURFACE MODIFICATION OF 316L STAINLESS STEEL BY HIGH CURRENT PULSED ELECTRON BEAM Part I Selective surface purification and its mechanism[J]. Acta Metall Sin, 2007, 42(1): 64-70 .
[1] Pogrebnjak A D,Ladysev V S,Pogrebnjak N A,Michaliov A D,Shablya V T,Valyaev A N,Valyaev A A,Loboda V B.Vacuum,2000;58:45 [2] Pogrebnjak A D,Mikhaliov A D,Pogrebnjak N A Jr., Tsvintarnaya Y V,Lavrentiev V I, Iljashenko M,Valyaev A N,Bratushka S,Zecca A,Sandrik R.Phys Lett,1998; 241A:357 [3] Ivanov Y,Matz W,Rotshtein V,Gunzel R,Shevchenko N.Surf Coat Technol,2002;150:188 [4] Proskurovsky D I,Rotshtein V P,Ozur G E,Markov A B,Nazarov D S.J Vac Sci Technol,1998;16A:2480 [5] Proskurovsky D I,Rotshtein V P,Ozur G E,Ivanov Y F, Markov A B.Surf Coat Technol,2000;125:49 [6] Pogrebnjak A D,Bratushka S,Boyko V I,Shamanin I V, Tsvintaruaya Y V.Nucl Instrum Methods Phys Res,1998; 145B:373 [7] Pogrebnjak A D,Shumakova N I.Surf Coat Technol, 1999; 122:183 [8] Hao S Z,Gao B,Wu A M,Zou J X,Qin Y,Dong C,An J, Guan Q F.Nucl Instrum Methods Phys Res,2005;240B: 646 [9] Zou J X,Grosdidier T,Zhang K M,Dong C.Acta Mater, 2006;54:5409 [10] Hao S Z,Gao B,Wu A M,Zou J X,Qin Y,Dong C,Guan Q F.Mater Sci Forum,2005;475-479:3959 [11] Gao B,Hao S Z,Zou J X,Grosdidier T,Jiang L M,Dong C,Zhou J Y.J Vac Sci Technol, 2005;23A:1538 [12] Qin Y,Dong C,Wang X G,Hao S Z,Wu A M,Zou J X, Liu Y.J Vac Sci Technol, 2003;21A:1934 [13] Korotaev A D,Ovchinnikov S V,Pochivalov Y I,Tyu- mentsev A N,Shchipakin D A,Tretjak M V,Isakov I F, Remnev G E.Surf Coat Technol,1998;105:84 [14] Shulov V A,Nochovnaya N A.Nucl Instrum Methods Phys Res,1999;148B:154 [15] Zhu X P,Lei M K,Dong Z H,Miao S M,Ma T C.Surf Coat Technol,2003;173:105 [16] Wood B,Perry A,Bitteker L J,Waganaar W j.Surf Coat Technol,1998;108/109:171 [17] Qin Y,Wang X G,Dong C,Hao S Z,Liu Y,Zou J X,Wu A M,Guan Q F.Acta Phys Sin,2003;52:3043 (秦颖,王晓钢,董闯,郝胜智,刘悦,邹建新,吴爱民,关庆丰.物理学报,2003;52:3043) [18] Dong C,Wu A M,Hao S Z,Zou J X,Liu Z M,Zhong P, Zhang A M,Xu T,Chen J M,Xu J,Liu Q,Zhou Z R.Surf Coat Technol,2003;163-164:620 [19] Ryan M P,Williams D E,Chater R J,Hutton B M, McPhail D S.Nature,2002;415:770 [20] Newman R C.Natune,2002;415:743 [21] Qin Y,Zou J X,Dong C,Wang X G,Wu A M,Liu Y,Hao S Z,Guan Q F.Nucl Instrum Methods Phys Res,2004; 225B:544 [22] Zou J X,Qin Y,Dong C,Wu A M,Hao S Z,Wang X G.J Vac Sci Technol, 2004;22A:545 [23] Aziz M J.J Appl Phys,1982;53:1158 [24] Zou J X,Wu A M,Dong C,Hao S Z,Liu Z M,Ma H T, Surf Coat Technol, 2004;183:261 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|