K18/Mo纳米多层材料的力学性能及高温稳定性 |
金雪松 欧盛荃 |
北京航空航天大学材料科学与工程系; 北京 100083 |
|
引用本文:
金雪松; 欧盛荃 . K18/Mo纳米多层材料的力学性能及高温稳定性[J]. 金属学报, 2000, 36(1): 99-103 .
[1] Lehoczky S L. J Appl Phys, 1978; 49: 5479 [2] Helmersson U, Todorova S, Barnett S A, Sundgren J--E,Markert L C, Greene J E. J Appl Phys, 1987; 62: 481 [3] Alpas A T, Embury J D, Hardwick D A, Springer R W. JMater Sci, 1990; 25: 1603 [4] Xu H B, Gong S K, Deng L. Thin Solid Films, 1998; 344. 98 [5] Movchan B A. JOM, 1996; 48: 40 [6] Movchan B A, Demchishin A V. Fiz Metal Metalloued, 1969;28: 834 |
|