| 脉冲高能量密度等离子体表面改性AlN膜的形成和结构 |
| 吴杏芳 韦鲲 单小鸥 杨思泽 |
| 北京科技大学材料物理系;北京100083 |
|
引用本文:
吴杏芳; 韦鲲; 单小鸥; 杨思泽 . 脉冲高能量密度等离子体表面改性AlN膜的形成和结构[J]. 金属学报, 2002, 38(6): 652-656 .
[1] Yan P X, Yang S Z, Li B, Chen X S. Phy Stat Sol(A),1994; 145: k29 [2] Wei K, Wu X F, Yang S Z, Li B. Mater Sci Eng, 1998;A254:129 [3] Fu Y, Wu X F, Wang Y, Li B, Yang S Z. Appl Surf Sci,2000; 157: 167 [4] Yan P X, Yang S Z, Chen X S. Acta Metall Sin (Englishlett), 1994; 11: 24 [5] Wei k, Wu X F, Fu Y. J Mater Sci, 1999; 34: 4633 [6] Yan P X, Yang S Z. Chin Phys Lett, 1994; 11: 558 [7] Briggs D, Seah M P. Practical Surface Analysis-Auger andX-ray Photoelectronscopy. Wiley: Chichester, 1990:1 [8]Wills D A, Xu X F, Poon G C, Tam A C. Opt Eng, 1998;37:1033 [9]Pauling G, Thorpe S J, Aust K T. Scr Metall Mater, 1990;24: 1347 [10]Chritensen N E, Goreczya L. Phys Rev B, 1993; 47: 4307 [11]Wang J, Wang W L, Ding P D, Yang Y X, Fang L, EsteveJ, Polo M C, Sanchez G. Diamond Relat Mater, 1999; 8:1342 |
|