| 半固态钢铁材料轧制产品的力学特性 |
| 宋仁伯; 康永林; 孙建林; 赵爱民; 毛卫民 |
| 北京科技大学材料科学与工程学院; 北京 100083 |
|
引用本文:
宋仁伯; 康永林; 孙建林; 赵爱民; 毛卫民 . 半固态钢铁材料轧制产品的力学特性[J]. 金属学报, 2002, 38(2): 153-156 .
[1] Mayerhofer J. In: Chiarmetta G L, Rosso M eds, Proceed-ings 6th International Conference on Semi-solid Process-ing of Alloy and Composites, Materials Science and Chem-ical Engineering Depertment, Italy, Turin: 2000: 195 [2] Miwa K, Kawamura S. In: Chiarmetta G L, Rosso Meds, Proceedings 6th Internatlonal Condrence on Semi-solid Processing of Alloy and Compo8ites, Materials Science and Chemical Engineering Depertment, ItaIy, Turin:2000: 279 [3] Xie S S, Huang S H. Technique and Application of Semi-solid Metal Processing. Beijing: Metallurgical IndustryPress. 1999: 2 (谢水生.黄声宏.半固态会属加工技术及其应用. 北京:冶金工业出版社.1999:2) [4] Chen X Y, Mao W M, Zhong X Y. Mater Mech Eng, 1998;22(4). 25 (陈晓阳. 毛卫民. 钟雪友. 机械工程材料.1998;22(4):25) [5] Lapkowki W, Sinczak J, Rusz S. J Mater Technol, 1997;63: 260 [6] Kang C G, Chei J S. J AIateT Technol, 1998; 73: 251 [7] Owasaki H, Mori T, Mabuchi M. Higashil K. Acta Mater,1998, 46: 6351 [8] Chei J S, Hyung J P. J Mater Techno, 1998; 82. 107 [9] Jiang P, He X M, Zhang X F. Hot Rolling Work, 1999;(1): 42 (蒋 鹏.贺小毛.张秀峰 .热加工工艺.1999;(1):42) [10] Yt H Q, Chen J D. Metal Plastic Forming Theory. Bei-jing: Machinery Industry Press, 1999: 15 (俞汉清.陈金德.金属塑性成形原理. 北京:机械工业出版社1999:15) [11] Chen P Q. Mcrostructure Saperplasticity. Harbin:Harbin Institute of Technology Press. 1988: 112 (陈浦泉 .组织超塑性. 哈尔滨:哈尔滨工业大学出版社.1988:112)U |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|