| Ta等离子体渗氮的非平衡热力学 |
| 张德元; 李放; 罗文; 曾卫军; 付青峰; 林勤 |
| 北京科技大学理化系; 北京 100083 |
|
引用本文:
张德元; 李放; 罗文; 曾卫军; 付青峰; 林勤 . Ta等离子体渗氮的非平衡热力学[J]. 金属学报, 2002, 38(2): 149-152 .
[1] Zhang D Y, Li F, Luo W, Cai L, Xu L P, Lin Q. Chin JNowtrmua Metals, 2000; 10: 189 (张德元,李 放,罗 文,蔡 莉,许兰萍,林 勤.中国有色金属学报,2000;10:189) [2]Prigogine.I.Introduction to Thermodynamics of Irre- versible Process,3rd Ed.New York:Interscience Pub, 1967 [3]Spitsyn B V,Derjaguin D B.Sci Am,1975;233:102 [4] Spitsyn B V,Builov L L,Derjaguin D B.J Cryst Growth, 1981;52:219 [5]Babab zahaknibin A A ed,Li F Z trans.Electrochemical Heat Treatment with Glow Discharge.Beijing:Machinery Industry Press;1985:17 (Babad zahaknibin A A 著, 李凤照译.辉光放电化学热处理,北京:机械工业出版社, 1985: 17) [6] Wang J T,Carlsson J O.Surf Coat Technol,1990;43/44:1 [7] Wang J T,Zhang P T,Yang Q H.In:Ravi K V,DismukesJ P eds, Diamond Materials IV NJ: The Electrochem SocInc Pennington, 1995; PV 95-4: 13 [8] Zhang D Y, Li Q, Zeng W J, Li F, Lu D P. Proc 1st InterConf on Mechan Eng, Shanghai: 2000; 18-22: 601 [9] Zhang D Y, Li Q, Zeng W J, Li F, Xu L P Fu Q F. TransNonferrous Met Soc Chin, 2001; 11: 281 [10] Qiao Z Y, Xu Z H, Liu H L, Computerized Physical Chem-istry of Materials and Metallurgy. Beijing: MetallurgyIndustry Press, 1999: 142 侨芝郁,许志宏,刘洪霖.冶金和材料计算物理化学.北京:冶金工业出版社1999:142) [11] Zhang D Y, Zeng W J, Fu Q F, Li F, Lin Q, Luo W. TransMater Heat hatment, 2001; 22(2): 48 (张德元,曾卫军,付青峰,李 放,林 勤,罗 文. 材料热处理学报,2001;22(2):48)) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|