| 不同温度轧制多晶铝的微观组织与晶界分布 |
| 张新明 邓运来 刘 瑛 唐建国 周卓平 |
| 中南大学材料科学与工程学院; 长沙 410083 |
|
| MICROSTRUCTURES AND BOUNDARY DISTRIBUTIONS IN Al POLYCRYSTALS ROLLED AT DIFFERENT TEMPERATURES |
| ZHANG Xinming; DENG Yunlai; LIU Ying; TANG Jianguo; ZHOU Zhuoping |
| College of Materials Science and Engineering; Central South University; Changsha 410083 |
引用本文:
张新明; 邓运来; 刘瑛; 唐建国; 周卓平 . 不同温度轧制多晶铝的微观组织与晶界分布[J]. 金属学报, 2005, 41(9): 947-952 .
,
,
,
,
.
MICROSTRUCTURES AND BOUNDARY DISTRIBUTIONS IN Al POLYCRYSTALS ROLLED AT DIFFERENT TEMPERATURES[J]. Acta Metall Sin, 2005, 41(9): 947-952 .
[1] Doherty R D,Hughes D A,Humphreys F J, Jonas J J, Jensen D J, Kassner M E, King W E, McNelley T R, McQueen H J, Rollett A D. Mater Sci Eng, 1997; A238: 219 [2] Gottstein G. Mater Sci Froum, 2002; 408: 1 [3] Bunge H-J. Mathematische Methoden der Texturanalyse. Berlin: Akademie-Verlag, 1969: 4 [4] Sevillano J G, van Houtte P, Aernoudt E. Prog Mater Sci, 1980; 25: 69 [5] Hirsch J, Lucke K.Acta Metall, 1988; 36: 2883 [6] Chen Z Y, Zhang X M, Du Y X, Yao Z Y, Liu C M. Mater Sci Forum, 2002; 408: 475 [7] Deng Y L, Zhang X M, Liu Y, Tang J G, Zhou Z P. Chin J Nonferrous Met, 2002; 12: 634 (邓运来,张新明,刘 瑛,唐建国,周卓平.中国有色金属学 报, 2002;12:634) [8] Delannay L, Mishin O V, Jensen D J, van Houtte P. Acta Mater, 2001; 49: 2441 [9] Wu G L, Liu W, Godfrey A, Liu Q. Acta Metall Sin, 2004; 40: 699 (吴桂林,刘伟,Godfrey A,刘庆.金属学报,2004;40: 699) [10] Wang Y N, Wu B L, Wang G, Jiang Q W, Zhao X, Zuo L. Acta Metall Sin, 2002; 38: 1085 (王轶农,武保林,王刚,蒋奇武,赵骧,左良.金属学 报,2002;38:1085) [11] OIM?Analysis For Windows User Manual. TexSEM Lab. Inc., Mahwah, USA, 1998 [12] Bishop J F W, Hill R. Philos Mag, 1951; 42: 414 [13] Bishop J F W, Hill R. Philos Mag, 1951; 42: 1298 [14] Chen Z Y, Zhang X M, Liu C M, Li S Y, Zhou Z P, Yang Y. Acta Metall Sin, 2000; 36: 1121 (陈志永,张新明,刘楚明,李赛毅,周卓平,杨 扬.金属学 报,2000;36:1121) [15] Huang Y, Humphreys F J. Acta Mater, 2000; 48: 2017 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|