| 超细搪瓷涂层对Ti60合金氧化及力学性能的影响 |
| 熊玉明 朱圣龙 王福会 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室; 沈阳 110016 |
|
| EFFECT OF ULTRAFINE ENAMEL COATING ON THE OXIDATION AND MECHANICAL PROPERTY OF Ti60 ALLOY |
| XIONG Yuming; ZHU Shenglong; WANG Fuhui |
| State Key Laboratory for Corrosion and Protection; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
熊玉明; 朱圣龙; 王福会 . 超细搪瓷涂层对Ti60合金氧化及力学性能的影响[J]. 金属学报, 2004, 40(7): 768-772 .
,
,
.
EFFECT OF ULTRAFINE ENAMEL COATING ON THE OXIDATION AND MECHANICAL PROPERTY OF Ti60 ALLOY[J]. Acta Metall Sin, 2004, 40(7): 768-772 .
[1] Unnam J, Shenoy R N, Clark R K. Oxid Met, 1986; 26: 231 [2] Clark R K, Unnam J. TMS-AIME Paper No.A84. S7TMS-AIMS Annual Meeting, Los Angeles, 1984 [3] Xiong Y M, Wang F H, Wu W T, Niu Y. Mater Sci Forum, 2001; 369-372: 743 [4] Wang F H, Tang Z L, Guan C H, Xiong Y M, Wu W T. Chinese Patent, No.98114349. 0, 1998. 8(王福会,唐兆麟,关春红,熊玉明,吴维(?).中国发明专利(No.98114349. 0) ,1998. 8) [5] Xiong Y M, Wang F H. Acta Metall Sin, 1999; 35(Suppl.1) : S215(熊玉明,王福会.金属学报, 1999;35(Suppl.1) :S215) 38(Suppl):S626 [6] Tang Z L, Wang F H. Mater Sci Eng, 2000; A276: 70 [7] Xiong Y M, Zhu S L, Wang F H. Acta Metall Sin, 2002; 38(Suppl): S626(熊玉明,朱圣龙,王福会.金属学报,2002;38(Suppl):S626) [8] Shao G X, Gou W B, Wen R C. Enamel, Beijing: Light Industry Press, 1983: 81, 101(邵规贤,芶文彬,闻瑞昌.搪瓷学.北京:轻工业出版社,1983:81,101) [9] Xiong Y M. Master Thesis, Institute of Metal Corrosion and Protection, The Chinese Academy of Sciences, 2000(熊玉明.中国科学院金属腐蚀与防护研究所硕士学位论文,2000) [10] Taniguchi S, Shibada T, Yamada T, Liu X, Zou S. ISIJInt, 1993; 33: 869 [11] Xu D, Zhu H, Tand L Y, Yang Y J, Zheng Z H, Liu X H,Taniguchi S, Shibada T. Acta Metall Sin, 1995; 31: 164(徐东,朱宏,汤丽娟,杨云洁,郑志宏,柳襄怀,谷口滋次,柴田俊夫.金属学报, 1995;31:164) [12] Taniguchi S, Shibada T, Takeuchi K. Mater Trans JIM,1991; 32(3) : 299 [13] Tang Z L, Wang F H, Wu W T. Chin J Mater Res, 1997;11: 507(唐兆麟,王福会,吴维(?).材料研究学报, 1997;11:507) [14] Zhang Y M, Zhou L J, Wang W L, Li T F, Chen C W. Rare Met Mater Eng, 1993; 22(1) : 27(张亚明,周龙江,王卫林,李铁藩,陈崇伟.稀有金属材料与工程,1993;22(1) :27) [15] Streiff R, Poize S. In: Rapp R A ed., High TemperatureCorrosion, Nace-6, Houston, 1983: 591 [16] Mckee D W, Luthra L. Surf Coat Technol, 1993; 56: 109 [17] Tang Z L, Wang F H, Wang Q J, Wu W T, Li D. ActaMetall Sin, 1998; 34: 325(唐兆麟,王福会,王清江,吴维(?),李东.金属学报,1998;34:325) [18] McCarron L, Schaeffer J C, Meier G H, Berztiss D, Perkins R A, Cullinan J. In: Froes F H, Caplan I eds., Titanium '92, Warrendale, PA: TMS, 1993; 1971 [19] Tang Z L, Wang F H, Wu W T. Oxid Met, 1997; 48: 511 [20] Tang Z L, Wang F H, Wu W T. Proc Japan-China Workshop on Titanium Alloys and Titanium Intermetallics, KawabeY, Hagiwara M eds., Japan Inter Sci Technol Exchange Centre, March 3-5, 1997: 237 [21] Tang Z L, Wang F H, Wu W T. Corros Sci Prot Technol, 1998; 18: 35(唐兆麟,王福会,吴维炭.腐蚀与防护科学技术, 1998;18:351 [22] Leyens C, van Liere J W, Peters M, Kaysser W A. SurfCoat Technol, 1998; 108-109: 30 [23] Brady M P, Smialek J L, Smith J, Humphrey D L. ActaMater, 1997; 45: 2357 [24] Brady M P, Smialek J L, Humphrey D L, Smith J, ActaMater, 1997; 45: 2371 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|