Please wait a minute...
金属学报  2004, Vol. 40 Issue (7): 763-767     
  论文 本期目录 | 过刊浏览 |
304L不锈钢在高温水中的应力腐蚀裂纹扩展
陆永浩 褚武扬 高克玮 乔利杰
北京科技大学 材料物理系; 北京 100083
STRESS CORROSION CRACKING OF 304L STAINLESS STEEL IN WATER AT 288℃
LU Yonghao; CHU Wuyang; GAO Kewei; QIAO Lijie
Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083
引用本文:

陆永浩; 褚武扬; 高克玮; 乔利杰 . 304L不锈钢在高温水中的应力腐蚀裂纹扩展[J]. 金属学报, 2004, 40(7): 763-767 .
, , , . STRESS CORROSION CRACKING OF 304L STAINLESS STEEL IN WATER AT 288℃[J]. Acta Metall Sin, 2004, 40(7): 763-767 .

全文: PDF(293 KB)  
摘要: 敏化的304L不锈钢紧凑拉伸试样在288℃的含氧循环水中发生应力腐蚀(SCC)后, 沿试样横截面将裂纹尖端区制成透射电镜(TEM)试样, 用高分辨分析型TEM观察裂尖, 测量微区成分. 结果表明,在不连续的SCC裂纹周围及裂尖前方存在几百纳米宽的氧化物区, 成分为Cr2O3, Fe3O4或其混合物. 在氧化物中存在大量的纳米级浅裂纹, 在裂尖应力集中作用下, 氧化物中首先形成不连续的微裂纹, 它们长大并和主裂纹连接就导致SCC裂纹的不连续形核及扩展.
关键词 : 304L不锈钢,  高温水,  应力腐蚀    
Abstract:Stress corrosion cracking (SCC) of a sensitized 304L stainless steel was carried out under slow tension of a pre--cracked sample in water containing oxygen at 288℃. Thin foil samples were prepared along its cross--section containing the pre--cracks, and the tip region of SCC was studied by analytical TEM. The observations show that there are oxides with a size of several hundreds nanometers ahead of a crack tip of SCC and around the discontinuous microcracks. Fine--probe analysis was used to determine local compositions of the oxides, indicating the oxides are Cr2O3, Fe3O4 and their mixture. Many microcracks are distributed unevenly in the oxides. Microcracks initiated discontinuously in the oxides ahead of a main crack because of a large stress concentration. The growth and connection of the discontinuous microcracks in the oxides resulted in the propagation of SCC.
Key words: 304L stainless steel    stress corrosion cracking    water at 288℃
收稿日期: 2003-09-23     
ZTFLH:  TG172.8  
[1] Jones R H. Stress-Corrosion Cracking, Metal Park OH:ASM,1992: 91
[2] Smialowska S S, Cragnolino G. Corrosion, 1980; 36: 653
[3] Stachle R W, Hochmann J, McCright R. Stress Corrosion Cracking and Hydrogen Embrittlement of Iron-Based Alloys, Houston: NACE, 1977: 1023
[4] Jenssen A, Ljungberg L G, Walmsley J, Fisher S. Corrosion, 1998; 54: 48
[5] Ford F P. Corrosion, 52; 1996: 375
[6] Li G F, Kaneshima Y, Shoji T. Corros Sci, 2000; 56: 460
[7] Scott P M, Calvar M L. Corrosion-Deformation Interaction CDI'96, London: Inst Metal, 1997: 384
[8] Thomas L E, Bruemmer S M. Corrosion, 2000; 56: 572
[9] Iacocca R G, Woodford D A. Metall Trans, 1988; 19A:2305
[10] Whittle D P, Shida Y, Wood G C, Stott F H, Bastow BD. Philos Mag A, 1982; 46: 931
[11] Rosier J, Muller S. Scr Mater, 1999; 40: 257
[12] Thompson A W, Bernstein I M. Effect of Hydrogen on Behavior of Materials, Metal Park OH: AIMI, 1976: 530
[13] Zhang B Y, Diao F Q, Tang X Y. Acta Met Sin, 1990; 26: A454(张柏玉,刁凤琼,唐祥云.金属学报, 1990;26:A454)
[14] Chu W Y. Hydrogen Damage and Hydrogen-Induced Cracking. Beijing: Metallurgy Industry Press, 1988: 91(褚武杨.氢损伤和滞后断裂.北京:冶金工业出版社,1988:91)
[15] Nowick A S, Button J J. Diffusion in Solids, Recent Developments, New York: Academic Press, 1976: 82
[1] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[2] 韩恩厚, 王俭秋. 表面状态对核电关键材料腐蚀和应力腐蚀的影响[J]. 金属学报, 2023, 59(4): 513-522.
[3] 常立涛. 压水堆主回路高温水中奥氏体不锈钢加工表面的腐蚀与应力腐蚀裂纹萌生:研究进展及展望[J]. 金属学报, 2023, 59(2): 191-204.
[4] 马志民, 邓运来, 刘佳, 刘胜胆, 刘洪雷. 淬火速率对7136铝合金应力腐蚀开裂敏感性的影响[J]. 金属学报, 2022, 58(9): 1118-1128.
[5] 刘振宝,梁剑雄,苏杰,王晓辉,孙永庆,王长军,杨志勇. 高强度不锈钢的研究及发展现状[J]. 金属学报, 2020, 56(4): 549-557.
[6] 马宏驰, 杜翠薇, 刘智勇, 李永, 李晓刚. E690高强低合金钢焊接热影响区典型组织在含SO2海洋环境中的应力腐蚀行为对比研究[J]. 金属学报, 2019, 55(4): 469-479.
[7] 邓平,孙晨,彭群家,韩恩厚,柯伟,焦治杰. 核用304不锈钢辐照促进应力腐蚀开裂研究[J]. 金属学报, 2019, 55(3): 349-361.
[8] 张聪惠, 荣花, 宋国栋, 胡坤. 喷丸表面粗糙度对纯Ti焊接接头在HCl溶液中应力腐蚀开裂行为的影响[J]. 金属学报, 2019, 55(10): 1282-1290.
[9] 余军, 张德平, 潘若生, 董泽华. 井下含硫环空液中P110油管钢应力腐蚀开裂的电化学噪声特征[J]. 金属学报, 2018, 54(10): 1399-1407.
[10] 苑洪钟,刘智勇,李晓刚,杜翠薇. 外加电位对X90钢及其焊缝在近中性土壤模拟溶液中应力腐蚀行为的影响[J]. 金属学报, 2017, 53(7): 797-807.
[11] 郭舒,韩恩厚,王海涛,张志明,王俭秋. 核电站316L不锈钢弯头应力腐蚀行为的寿命预测[J]. 金属学报, 2017, 53(4): 455-464.
[12] 明洪亮,张志明,王俭秋,韩恩厚,苏明星. 国产核电安全端异种金属焊接件的微观结构及局部性能研究[J]. 金属学报, 2017, 53(1): 57-69.
[13] 闫茂成,杨霜,许进,孙成,吴堂清,于长坤,柯伟. 酸性土壤中破损防腐层下X80管线钢的应力腐蚀行为*[J]. 金属学报, 2016, 52(9): 1133-1141.
[14] 刘智勇,李宗书,湛小琳,皇甫文珠,杜翠薇,李晓刚. X80钢在鹰潭土壤模拟溶液中应力腐蚀裂纹扩展行为机理*[J]. 金属学报, 2016, 52(8): 965-972.
[15] 张子龙, 夏爽, 曹伟, 李慧, 周邦新, 白琴. 晶界特征对316不锈钢沿晶应力腐蚀开裂裂纹萌生的影响*[J]. 金属学报, 2016, 52(3): 313-319.