| 陶瓷颗粒增强Mg65Cu20Zn5Y10块体金属玻璃复合材料 |
| 徐映坤 徐 坚 |
| 中国科学院金属研究所沈阳材料国家(联合)实验室; 沈阳 110016 |
|
| CERAMICS PARTICULATE REINFORCED Mg65Cu20Zn5Y10 BULK METALLIC GLASS COMPOSITES |
| XU Yingkun; XU Jian |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
徐映坤; 徐坚 . 陶瓷颗粒增强Mg65Cu20Zn5Y10块体金属玻璃复合材料[J]. 金属学报, 2004, 40(7): 726-730 .
,
.
CERAMICS PARTICULATE REINFORCED Mg65Cu20Zn5Y10 BULK METALLIC GLASS COMPOSITES[J]. Acta Metall Sin, 2004, 40(7): 726-730 .
[1] Johnson W L. Mater Res Soc Bull, 1999; 24(10) : 42 [2] Inoue A. Acta Mater, 2000; 48: 279 [3] Bruck H A, Christman T, Rosakis A J, Johnson W L. ScrMatall Mater, 1994; 30: 429 [4] Bruck H A, Rosakis A J, Johnson W L. J Mater Res, 1996;11: 503 [5] Choi-Yim H. Appl Phys Lett, 1997; 71: 3808 [6] Conner R D, Choi-Yim H, Johnson W L. J Mater Res,1999; 14: 3292 [7] Choi-Yim H, Bush R, Koster U, Johnson W L. ActaMater, 1999; 47: 2455 [8] Kato H, Inoue A. Mater Trans JIM, 1997; 38: 793 [9] Kato H, Hirano T, Matsuo A, Kawamura Y, Inoue A. ScrMater, 2002; 43: 503 [10] Zhang W, Ishihara S, Inoue A. Mater Trans, 2002; 43:1767 [11] Inoue A, Kato A, Zhang T, Kim S G, Masumoto T. MaterTrans JIM, 1991; 32: 609 [12] Kang H G, Park E S, Kim W T, Kim D H, Cho. H K.Mater Trans JIM, 2000; 41: 846 [13] Men H, Hu Z Q, Xu J. Scr Mater, 2002; 46: 699 [14] Amiya K, Inoue A. Mater Trans JIM, 2000; 41: 1460 [15] Choi-Yim H, Bush R, Johnson W L. J Appl Phys, 1998;83: 7993 [16] Ma C, Inoue A. Mater Trans, 2002; 43: 3266 [17] Flores K M, Dauskardt R H. J Mater Res, 1999; 14: 638 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|