| 激光增材修复单晶高温合金的热裂纹形成机制 |
卢楠楠1, 郭以沫1,2, 杨树林3, 梁静静1, 周亦胄1, 孙晓峰1, 李金国1( ) |
1中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 2沈阳工业大学 材料科学与工程学院 沈阳 110870 3中国航发沈阳黎明航空发动机有限责任公司 沈阳 110043 |
|
| Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys |
LU Nannan1, GUO Yimo1,2, YANG Shulin3, LIANG Jingjing1, ZHOU Yizhou1, SUN Xiaofeng1, LI Jinguo1( ) |
1Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870, China 3AECC Shenyang Liming Aero-Engine Co., Ltd., Shenyang 110043, China |
引用本文:
卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国. 激光增材修复单晶高温合金的热裂纹形成机制[J]. 金属学报, 2023, 59(9): 1243-1252.
Nannan LU,
Yimo GUO,
Shulin YANG,
Jingjing LIANG,
Yizhou ZHOU,
Xiaofeng SUN,
Jinguo LI.
Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. Acta Metall Sin, 2023, 59(9): 1243-1252.
| 1 |
Reed R C, Tao T, Warnken N. Alloys-by-design: Application to nickel-based single crystal superalloys [J]. Acta Mater., 2009, 57: 5898
doi: 10.1016/j.actamat.2009.08.018
|
| 2 |
Lopez-Galilea I, Ruttert B, He J Y, et al. Additive manufacturing of CMSX-4 Ni-base superalloy by selective laser melting: Influence of processing parameters and heat treatment [J]. Addit. Manuf., 2019, 30: 100874
|
| 3 |
Pollock T M. Alloy design for aircraft engines [J]. Nat. Mater., 2016, 15: 809
doi: 10.1038/nmat4709
pmid: 27443900
|
| 4 |
Wang L, Wang N, Yao W J, et al. Effect of substrate orientation on the columnar-to-equiaxed transition in laser surface remelted single crystal superalloys [J]. Acta Mater., 2015, 88: 283
doi: 10.1016/j.actamat.2015.01.063
|
| 5 |
Liang Y J, Cheng X, Li J, et al. Microstructural control during laser additive manufacturing of single-crystal nickel-base superalloys: New processing-microstructure maps involving powder feeding [J]. Mater. Des., 2017, 130: 197
doi: 10.1016/j.matdes.2017.05.066
|
| 6 |
Ur Rahman N, Capuano L, Cabeza S, et al. Directed energy deposition and characterization of high-carbon high speed steels [J]. Addit. Manuf., 2019, 30: 100838
|
| 7 |
Zhou Z P, Huang L, Shang Y J, et al. Causes analysis on cracks in nickel-based single crystal superalloy fabricated by laser powder deposition additive manufacturing [J]. Mater. Des., 2018, 160: 1238
doi: 10.1016/j.matdes.2018.10.042
|
| 8 |
Thompson S M, Bian L K, Shamsaei N, et al. An overview of direct laser deposition for additive manufacturing; Part I: Transport phenomena, modeling and diagnostics [J]. Addit. Manuf., 2015, 8: 36
|
| 9 |
Gäumann M, Bezençon C, Canalis P, et al. Single-crystal laser deposition of superalloys: Processing-microstructure maps [J]. Acta Mater., 2001, 49: 1051
doi: 10.1016/S1359-6454(00)00367-0
|
| 10 |
Liang Y J, Wang H M. Origin of stray-grain formation and epitaxy loss at substrate during laser surface remelting of single-crystal nickel-base superalloys [J]. Mater. Des., 2016, 102: 297
doi: 10.1016/j.matdes.2016.04.051
|
| 11 |
Wang L, Wang N. Effect of substrate orientation on the formation of equiaxed stray grains in laser surface remelted single crystal superalloys: Experimental investigation [J]. Acta Mater., 2016, 104: 250
doi: 10.1016/j.actamat.2015.11.018
|
| 12 |
Guo J C, Chen W J, Yang R N, et al. The effect of substrate orientation on stray grain formation in the (111) plane in laser surface remelted single crystal superalloys [J]. J. Alloys Compd., 2019, 800: 240
doi: 10.1016/j.jallcom.2019.06.029
|
| 13 |
Wang L, Wang N, Provatas N. Liquid channel segregation and morphology and their relation with hot cracking susceptibility during columnar growth in binary alloys [J]. Acta Mater., 2017, 126: 302
doi: 10.1016/j.actamat.2016.11.058
|
| 14 |
Wang N, Mokadem S, Rappaz M, et al. Solidification cracking of superalloy single- and bi-crystals [J]. Acta Mater., 2004, 52: 3173
doi: 10.1016/j.actamat.2004.03.047
|
| 15 |
Carter L N, Martin C, Withers P J, et al. The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy [J]. J. Alloys Compd., 2014, 615: 338
doi: 10.1016/j.jallcom.2014.06.172
|
| 16 |
Ruttert B, Ramsperger M, Roncery L M, et al. Impact of hot isostatic pressing on microstructures of CMSX-4 Ni-base superalloy fabricated by selective electron beam melting [J]. Mater. Des., 2016, 110: 720
doi: 10.1016/j.matdes.2016.08.041
|
| 17 |
Ojo O A, Richards N L, Chaturvedi M C. Contribution of constitutional liquation of gamma prime precipitate to weld HAZ cracking of cast Inconel 738 superalloy [J]. Scr. Mater., 2004, 50: 641
doi: 10.1016/j.scriptamat.2003.11.025
|
| 18 |
Chauvet E, Kontis P, Jägle E A, et al. Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron Beam Melting [J]. Acta Mater., 2018, 142: 82
doi: 10.1016/j.actamat.2017.09.047
|
| 19 |
Ramakrishnan A, Dinda G P. Direct laser metal deposition of Inconel 738 [J]. Mater. Sci. Eng., 2019, A740-741: 1
|
| 20 |
Boswell J H, Clark D, Li W, et al. Cracking during thermal post-processing of laser powder bed fabricated CM247LC Ni-superalloy [J]. Mater. Des., 2019, 174: 107793
doi: 10.1016/j.matdes.2019.107793
|
| 21 |
Yang J J, Li F Z, Wang Z M, et al. Cracking behavior and control of Rene 104 superalloy produced by direct laser fabrication [J]. J. Mater. Process. Technol., 2015, 225: 229
doi: 10.1016/j.jmatprotec.2015.06.002
|
| 22 |
Dantzig J A, Rappaz M. Solidification [M]. 2nd Edition -Revised & Expanded. Switzerland: EPFL Press, 2016: 618
|
| 23 |
Rong P, Wang N, Wang L, et al. The influence of grain boundary angle on the hot cracking of single crystal superalloy DD6 [J]. J. Alloys Compd., 2016, 676: 181
doi: 10.1016/j.jallcom.2016.03.164
|
| 24 |
Ci S W. Study on microstructure and mechanical properties of nickel-based single crystal superalloy by laser additive manufacturing [D]. Shenyang: University of Science and Technology of China(Institute of Metal Research, CAS), 2021
|
| 24 |
慈世伟. 激光增材制造镍基单晶高温合金显微组织和力学性能研究 [D]. 沈阳: 中国科学技术大学(中国科学院金属研究所), 2021
|
| 25 |
Lu N N, Lei Z L, Hu K, et al. Hot cracking behavior and mechanism of a third-generation Ni-based single-crystal superalloy during directed energy deposition [J]. Addit. Manuf., 2020, 34: 101228
|
| 26 |
Rappaz M, Drezet J M, Gremaud M. A new hot-tearing criterion [J]. Metall. Mater. Trans., 1999, 30A: 449
|
| 27 |
Rappaz M, Jacot A, Boettinger W J. Last-stage solidification of alloys: Theoretical model of dendrite-arm and grain coalescence [J]. Metall. Mater. Trans., 2003, 34A: 467
|
| 28 |
Anderson P M, Hirth J P, Lothe J. Theory of Dislocations [M]. 3rd Ed., Cambridge: Cambridge University Press, 2017: 536
|
| 29 |
Academic Committee of the Superalloys. China Superalloys Handbook [M]. Beijing: Standards Press of China, 2012: 589
|
| 29 |
中国金属学会高温材料分会. 中国高温合金手册 [M]. 北京: 中国标准出版社, 2012: 589
|
| 30 |
Read W T, Shockley W. Dislocation models of crystal grain boundaries [J]. Phys. Rev., 1950, 78: 275
doi: 10.1103/PhysRev.78.275
|
| 31 |
Asta M, Hoyt J J, Karma A. Calculation of alloy solid-liquid interfacial free energies from atomic-scale simulations [J]. Phys. Rev., 2002, 66B: 100101
|
| 32 |
Kurz W, Fisher D J. Fundamentals of Solidification [M]. 4th Ed., Switzerland: Trans Tech Publications Ltd, 1998: 51
|
| 33 |
Debroy T, Wei H L, Zuback J S, et al. Additive manufacturing of metallic components—Process, structure and properties [J]. Prog. Mater. Sci., 2018, 92: 112
doi: 10.1016/j.pmatsci.2017.10.001
|
| 34 |
Frenk A, Marsden C F, Wagniere J D, et al. Influence of an intermediate layer on the residual stress field in a laser clad [J]. Surf. Coat. Technol., 1991, 45: 435
doi: 10.1016/0257-8972(91)90253-S
|
| 35 |
Mukherjee T, Zhang W, Debroy T. An improved prediction of residual stresses and distortion in additive manufacturing [J]. Comput. Mater. Sci., 2017, 126: 360
doi: 10.1016/j.commatsci.2016.10.003
|
| 36 |
Kattamis T Z, Voorhees P W. Coarsening of solid-liquid mixtures: A review [A]. Proceedings of the Merton C. Flemings Symposium on Solidification and Materials Processing [C]. Cambridge, MA: TMS, 2000: 119
|
| 37 |
Huang Q Y, Li H K. Superalloys [M]. Beijing: Metallurgical Industry Press, 2000: 67
|
| 37 |
黄乾尧, 李汉康. 高温合金 [M]. 北京: 冶金工业出版社, 2000: 67
|
|