| Cu含量对K4061合金显微组织和拉伸性能的影响 |
曹姝婷1,2, 赵剑3, 巩桐兆1, 张少华1( ), 张健1 |
1.中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 2.中国科学技术大学 材料科学与工程学院 沈阳 110016 3.西安航天动力研究所 西安 710100 |
|
| Effects of Cu Content on the Microstructure and Tensile Property of K4061 Alloy |
CAO Shuting1,2, ZHAO Jian3, GONG Tongzhao1, ZHANG Shaohua1( ), ZHANG Jian1 |
1.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2.School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China 3.Xi'an Aerospace Propulsion Institute, Xi'an 710100, China |
引用本文:
曹姝婷, 赵剑, 巩桐兆, 张少华, 张健. Cu含量对K4061合金显微组织和拉伸性能的影响[J]. 金属学报, 2024, 60(9): 1179-1188.
Shuting CAO,
Jian ZHAO,
Tongzhao GONG,
Shaohua ZHANG,
Jian ZHANG.
Effects of Cu Content on the Microstructure and Tensile Property of K4061 Alloy[J]. Acta Metall Sin, 2024, 60(9): 1179-1188.
| 1 |
Kudrin A A, Zuev D S, Ponomareva L L, et al. Influence of microalloying on the plasticity of KhN58MBYuD-VI nickel alloy [J]. Steel Transl., 2008, 38: 252
|
| 2 |
Nedashkovskii K I, Zheleznyak O N, Gromyko B M, et al. Effect of low temperatures on mechanical and physical properties of high-strength nickel alloy ÉK61-ID and stainless maraging steel Ek49-VD [J]. Met. Sci. Heat Treat., 2003, 45: 233
|
| 3 |
Polyanskii A M, Polyanskii V M. Structural changes in alloy ÉK-61 due to cyclic deformation at elevated temperature [J]. Met. Sci. Heat Treat., 2010, 52: 279
|
| 4 |
Sorokina N A, Gal'tsova V I. High-temperature ductility of nickel alloys type KhN55MBYu with a high iron content [J]. Met. Sci. Heat Treat., 1994, 36: 476
|
| 5 |
Huang J, Xu G H, Qin H Y, et al. Correlation between fracture morphology and microstructural evolution during long-term aging of EK61 superalloy [J]. Scanning, 2020, 2020: 1087024
|
| 6 |
Mignanelli P M, Jones N G, Pickering E J, et al. Gamma-gamma prime-gamma double prime dual-superlattice superalloys [J]. Scr. Mater., 2017, 136: 136
|
| 7 |
Alam T, Chaturvedi M, Ringer S P, et al. Precipitation and clustering in the early stages of ageing in Inconel 718 [J]. Mater. Sci. Eng., 2010, A527: 7770
|
| 8 |
Slama C, Abdellaoui M. Structural characterization of the aged Inconel 718 [J]. J. Alloys Compd., 2000, 306: 277
|
| 9 |
Semenov V N, Akimov N V, Glushko V P. Formation of cracks in ÉP202 and ÉK61 alloys in welding of structures of liquid rocket engines [J]. Weld. Int., 2013, 27: 159
|
| 10 |
Monroe R W, Bates C E, Pears C D. Metal combustion in high-pressure flowing oxygen [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres [C]. West Conshohocken: ASTM, 1983: 126
|
| 11 |
Holt R T, Wallace W. Impurities and trace elements in nickel-base superalloys [J]. Int. Met. Rev., 1976, 21: 1
|
| 12 |
Davis S E. An elementary overview of the selection of materials for service in oxygen-enriched environments [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: 13th Volume [C]. West Conshohocken: ASTM, 2012: 1
|
| 13 |
Li Y M, Hu W, Chen Y. Effect of copper on solidification process and segregation in K4169 superalloy [J]. Spec. Cast. Nonferrous Alloys, 2013, 33: 895
|
| 13 |
李亚敏, 胡 伟, 陈 毅. Cu对K4169合金凝固过程及凝固偏析的影响 [J]. 特种铸造及有色合金, 2013, 33: 895
|
| 14 |
Li Y M, Zhang Y Y, Zhao W, et al. First-principles study on the effect of Cu on Nb segregation in Inconel 718 alloy [J]. Acta Metall. Sin., 2022, 58: 241
doi: 10.11900/0412.1961.2020.00495
|
| 14 |
李亚敏, 张瑶瑶, 赵 旺 等. Cu对Inconel 718合金Nb偏析影响机理的第一性原理研究 [J]. 金属学报, 2022, 58: 241
doi: 10.11900/0412.1961.2020.00495
|
| 15 |
Gwalani B, Choudhuri D, Soni V, et al. Cu assisted stabilization and nucleation of L12 precipitates in Al0.3CuFeCrNi2 fcc-based high entropy alloy [J]. Acta Mater., 2017, 129: 170
|
| 16 |
Detrois M, Pei Z R, Rozman K A, et al. Partitioning of tramp elements Cu and Si in a Ni-based superalloy and their effect on creep properties [J]. Materialia, 2020, 13: 100843
|
| 17 |
He Y W. Study on the effect and mechanism of V, Cu in a new Ni-Cr-Fe-Nb superalloy [D]. Shenyang: Northeastern University, 2016
|
| 17 |
贺玉伟. V、Cu在新型Ni-Cr-Fe-Nb高温合金中的作用机理研究 [D]. 沈阳: 东北大学, 2016
|
| 18 |
Pan J S, Tong J M, Tian M B. Fundamentals of Materials Science [M]. Beijing: Tsinghua University Press, 2011: 96
|
| 18 |
潘金生, 仝健民, 田民波. 材料科学基础 [M]. 北京: 清华大学出版社, 2011: 96
|
| 19 |
Oblak J M, Paulonis D F, Duvall D S. Coherency strengthening in Ni base alloys hardened by DO22 γ'' precipitates [J]. Metall. Trans., 1974, 5: 143
|
| 20 |
Han D W, Yu L X, Liu F, et al. Effect of heat treatment on the microstructure and mechanical properties of the modified 718 alloy [J]. Acta Metall. Sin. (Engl. Lett.), 2018, 31: 1224
|
| 21 |
Goodfellow A J. Strengthening mechanisms in polycrystalline nickel-based superalloys [J]. Mater. Sci. Technol., 2018, 34: 1793
|
| 22 |
Roth H A, Davis C L, Thomson R C. Modeling solid solution strengthening in nickel alloys [J]. Metall. Mater. Trans., 1997, 28A: 1329
|
|