| Y掺杂Ti膜的吸放氢行为 |
李聪, 王猛, 屠汉俊, 施立群( ) |
| 复旦大学 现代物理研究所 上海 200433 |
|
| Behavior of Hydrogen Absorption and Desorption in Y-doped Ti Films |
LI Cong, WANG Meng, TU Hanjun, SHI Liqun( ) |
| Institute of Modern Physics, Fudan University, Shanghai 200433, China |
引用本文:
李聪, 王猛, 屠汉俊, 施立群. Y掺杂Ti膜的吸放氢行为[J]. 金属学报, 2024, 60(6): 826-836.
Cong LI,
Meng WANG,
Hanjun TU,
Liqun SHI.
Behavior of Hydrogen Absorption and Desorption in Y-doped Ti Films[J]. Acta Metall Sin, 2024, 60(6): 826-836.
| 1 |
Schlapbach L, Züttel A. Hydrogen-storage materials for mobile applications [J]. Nature, 2001, 414: 353
|
| 2 |
Beavis L C, Miglionico C J. Structural behavior of metal tritide films [J]. J. Less Common Met., 1972, 27: 201
|
| 3 |
Duan Y M, Wang W D, Ding W, et al. IBA investigation on the effect of Ti-Mo interdiffusion on the D concentration in TiD x /Mo films [J]. Nucl. Instrum. Methods Phys. Res., 2020, 470B: 61
|
| 4 |
Hirooka Y, Miyake M, Sano T. A study of hydrogen absorption and desorption by titanium [J]. J. Nucl. Mater., 1981, 96: 227
|
| 5 |
Tal-Gutelmacher E, Eliezer D. Hydrogen cracking in titanium-based alloys [J]. J. Alloys Compd., 2005, 404-406: 621
|
| 6 |
Zhao Y, Zheng H, Liu S, et al. Investigation of the structure and the property of hydrogen storage Ti-Mo alloys [J]. Acta Metall. Sin., 2003, 39: 89
|
| 6 |
赵 越, 郑 华, 刘 实 等. Ti-Mo合金的结构及吸放氢性能研究 [J]. 金属学报, 2003, 39: 89
|
| 7 |
Shi L Q, Zhou Z Y, Zhao G Q, et al. Hydrogenation characteristics and observation of disintegration conditions of Ti-Mo and Ni-coated Ti-Mo thin films [J]. J. Vac. Sci. Technol., 2001, 19A: 240
|
| 8 |
Shi L Q, Zhou Z Y, Zhao G Q. Hydrogen storage and hydrogen embrittlement of Ti-Mo alloy films [J]. Acta Metall. Sin., 2000, 36: 530
|
| 8 |
施立群, 周筑颖, 赵国庆. Ti-Mo合金薄膜的储氢特性和抗氢脆能力 [J]. 金属学报, 2000, 36: 530
|
| 9 |
Bing W Z, Long X G, Zhu Z L, et al. Structure and thermodynamic aspect of Ti-Hf alloys and their deuterides [J]. Chin. J. Inorg. Chem., 2010, 26: 1008
|
| 9 |
邴文增, 龙兴贵, 朱祖良 等. Ti-Hf合金的结构和吸氘热力学性质 [J]. 无机化学学报, 2010, 26: 1008
|
| 10 |
Liu B L, Liu S, Wang L B. Investigation on helium bubbles shape in Ti and Ti alloy by transmission electron microscopy [J]. At. Energy Sci. Technol., 2008, 42: 799
|
| 10 |
刘本良, 刘 实, 王隆保. Ti及Ti合金中氦泡形貌的透射电镜研究 [J]. 原子能科学技术, 2008, 42: 799
doi: 10.7538/yzk.2008.42.09.0799
|
| 11 |
Zhao E T, Chen Y Y, Kong F T, et al. Effect of yttrium on microstructure and mold filling capacity of a near-α high temperature titanium alloy [J]. China Foundry, 2012, 9: 344
|
| 12 |
Heo K H, Munirathnam N R, Lim J W, et al. Effect of oxygen and yttrium doping on the electrical resistivity and hardness of titanium metal obtained by electron beam melting [J]. Mater. Chem. Phys., 2008, 112: 923
|
| 13 |
Zhang J C, Wu E D, Liu S. Effects of Y on helium behavior in Ti-Y alloy films [J]. J. Nucl. Mater., 2014, 454: 119
|
| 14 |
Li C J, Xiong L Y, Wu E D, et al. Effect of yttrium on nucleation and growth of zirconium hydrides [J]. J. Nucl. Mater., 2015, 457: 142
|
| 15 |
Yun S, Oyama S T. Correlations in palladium membranes for hydrogen separation: A review [J]. J. Membrane Sci., 2011, 375: 28
|
| 16 |
Verma N, Krishnamurthy G, Tichelaar F D, et al. Controlling morphology and texture of sputter-deposited Pd films by tuning the surface topography of the (Ti) adhesive layer [J]. Surf. Coat. Technol., 2019, 359: 24
|
| 17 |
Lim H R, Eom N S A, Cho J H, et al. Hydrogen gettering of titanium-palladium/palladium nanocomposite films synthesized by cosputtering and vacuum-annealing [J]. Int. J. Hydrogen Energy, 2018, 43: 19990
|
| 18 |
Zhang Q J, Qi Q H, Cao Z, et al. Effect of C contamination on H2 uptake of Ti film [J]. Vac. Sci. Technol., 1997, 17: 45
|
| 18 |
张强基, 漆其鸿, 曹 昭 等. 碳污染对钛膜吸氢能力影响的研究 [J]. 真空科学与技术, 1997, 17: 45
|
| 19 |
Griessen R, Huiberts J N, Kremers M, et al. Yttrium and lanthanum hydride films with switchable optical properties [J]. J. Alloys Compd., 1997, 253-254: 44
|
| 20 |
Shi L Q, Zhou Z Y, Zhao G Q. Hydrogenation and thermal release of hydrogen in titanium thin films [J]. At. Energy Sci. Technol., 2000, 34: 328
|
| 20 |
施立群, 周筑颖, 赵国庆. 钛薄膜氢化及热释放特性研究 [J]. 原子能科学技术, 2000, 34: 328
|
| 21 |
Zhang W Z, Tang X H, Li J Q, et al. Deuterium retention in carbon-tungsten co-deposition layers prepared by RF magnetron sputtering [J]. Acta Phys. Sin., 2013, 62: 195202
|
| 21 |
张文钊, 唐兴华, 李嘉庆 等. 氘在碳钨共沉积层中的滞留行为研究 [J]. 物理学报, 2013, 62: 195202
|
| 22 |
Zhao G Q, Ren C G. Nuclear Analysis Technique [M]. Beijing: Atomic Energy Press, 1989: 1
|
| 22 |
赵国庆, 任炽刚. 核分析技术 [M]. 北京: 原子能出版社, 1989: 1
|
| 23 |
L′ Ecuyer J, Brassard C, Cardinal C, et al. An accurate and sensitive method for the determination of the depth distribution of light elements in heavy materials [J]. J. Appl. Phys., 1976, 47: 381
|
| 24 |
Mayer M. Improved physics in SIMNRA 7 [J]. Nucl. Instrum. Meth., 2014, 332B: 176
|
| 25 |
Li M Q, Yao X Y. First-principles study of α-titanium and β-titanium crystal structure with hydrogen [J]. Rare Met. Mater. Eng., 2013, 42: 530
|
| 25 |
李淼泉, 姚晓燕. 置氢α-钛和β-钛晶体结构的第一性原理研究 [J]. 稀有金属材料与工程, 2013, 42: 530
|
| 26 |
Liu S, Wang Y G. First-principles of hydrogen diffusion mechanism in titanium crystals [J]. Chin. J. Nonferrous Met., 2015, 25: 3100
|
| 26 |
刘 松, 王寅岗. 氢在钛晶体中扩散行为的第一性原理 [J]. 中国有色金属学报, 2015, 25: 3100
|
| 27 |
Liu X K, Zhang Y, Zheng Z, et al. Structural and thermodynamic properties of TiH2 from first-principles calculations [J]. Sci. Sin. Phys. Mech. Astron., 2011, 41: 207
|
| 27 |
刘显坤, 张 旸, 郑 洲 等. 第一性原理研究TiH2的结构和热力学性质 [J]. 中国科学: 物理学 力学 天文学, 2011, 41: 207
|
| 28 |
Huang X T, Qing P L, Qin C S, et al. Influences of transition elements (V, Ti, Y) on hydrogen storage property of Mg-Al alloy [J]. Chin. J. Nonferrous Met., 2020, 30: 333
|
| 28 |
黄显吞, 卿培林, 覃昌生 等. 过渡金属V、Ti及Y的添加对Mg-Al合金储氢性能的影响 [J]. 中国有色金属学报, 2020, 30: 333
|
| 29 |
Zhu Y, Wang F H. First principles study on the dehydrogenation from MgH2 (001) surface by metal (Li, A1, Ti) doping [J]. Dev. Energy Sci., 2015, 3(1): 20
|
| 29 |
朱 玥, 王福合. 金属原子(Li, A1, Ti)掺杂对MgH2 (001)表面脱氢性能影响的第一性原理研究 [J]. 能源科学发展: 中英文版, 2015, 3(1): 20
|
| 30 |
Germán E, Luna C, Marchetti J, et al. A DFT study of dopant (Zr, Nb) and vacancies on the dehydrogenation on MgH2 (001) surface [J]. Int. J. Hydrogen Energy, 2014, 39: 1732
|
| 31 |
Li Y X. First-principles study on properties and hydrogen atoms diffusion of zirconium-hydrogen system [D]. Taiyuan: North University of China, 2021
|
| 31 |
李越鑫. 锆氢体系性质和氢原子扩散的第一性原理研究 [D]. 太原: 中北大学, 2021
|
| 32 |
Kohn W, Sham L J. Self-consistent equations including exchange and correlation effects [J]. Phys. Rev., 1965, 140: A1133
|
| 33 |
Segall M D, Lindan P J D, Probert M J, et al. First-principles simulation: Ideas, illustrations and the CASTEP code [J]. J. Phys. Condens. Matter, 2002, 14: 2717
|
| 34 |
Perdew J P, Burke K, Ernzerhof M. Generalized gradient approximation made simple [J]. Phys. Rev. Lett., 1996, 77: 3865
doi: 10.1103/PhysRevLett.77.3865
pmid: 10062328
|
| 35 |
Han X L, Wang Q, Sun D L, et al. First-principles study of hydrogen diffusion in alpha Ti [J]. Int. J. Hydrogen Energy, 2009, 34: 3983
|
| 36 |
San-Martin A, Manchester F D. The H-Ti (Hydrogen-Titanium) system [J]. Bull. Alloy Phase Diagrams, 1987, 8: 30
|
| 37 |
Yakel H L. Thermocrystallography of higher hydrides of titanium and zirconium [J]. Acta Crystallogr., 1958, 11: 46
|
| 38 |
Uwamino Y, Ishizuka T, Yamatera H. X-ray photoelectron spectroscopy of rare-earth compounds [J]. J. Electron Spectrosc. Relat. Phenom., 1984, 34: 67
|
| 39 |
Paulin I, Mandrino D, Donik Č, et al. AES and XPS characterization of titanium hydride powder [J]. Mater. Technol., 2010, 44: 73
|
| 40 |
Ebihara K I, Kaburaki H. Numerical modeling of thermal desorption spectra of hydrogen: A review of thermal desorption models [J]. ISIJ Int., 2012, 52: 181
|
| 41 |
Zhang B, Zheng H, Liu S, et al. Hydrogen absorption and desorption of titanium [J]. At. Energy Sci. Technol., 2005, 39: 522
|
| 41 |
张 滨, 郑 华, 刘 实 等. 纯Ti吸放氢过程研究 [J]. 原子能科学技术, 2005, 39: 522
|
| 42 |
Martin M, Gommel C, Borkhart C, et al. Absorption and desorption kinetics of hydrogen storage alloys [J]. J. Alloys Compd., 1996, 238: 193
|
| 43 |
Bhosle V, Baburaj E G, Miranova M, et al. Dehydrogenation of TiH2 [J]. Mater. Sci. Eng., 2003, A356: 190
|
| 44 |
Shi L Q, Zhao G Q, Zhou Z Y, et al. The kinetics of hydrogen interaction with thin films [J]. At. Energy Sci. Technol., 2000, 34: 216
|
| 44 |
施立群, 赵国庆, 周筑颖 等. 储氢薄膜的吸氢动力学研究 [J]. 原子能科学技术, 2000, 34: 216
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|