| TiAl合金板材轧制研究现状 |
陈玉勇1,2( ), 叶园1, 孙剑飞1 |
1.哈尔滨工业大学 材料科学与工程学院 哈尔滨 150001 2.攀枝花学院 国际钒钛研究院 攀枝花 617000 |
|
| Present Status for Rolling TiAl Alloy Sheet |
CHEN Yuyong1,2( ), YE Yuan1, SUN Jianfei1 |
1.School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China 2.International Institute of Vanadium and Titanium, Panzhihua University, Panzhihua 617000, China |
引用本文:
陈玉勇, 叶园, 孙剑飞. TiAl合金板材轧制研究现状[J]. 金属学报, 2022, 58(8): 965-978.
Yuyong CHEN,
Yuan YE,
Jianfei SUN.
Present Status for Rolling TiAl Alloy Sheet[J]. Acta Metall Sin, 2022, 58(8): 965-978.
| 1 |
Appel F, Clemens H, Fischer F D. Modeling concepts for intermetallic titanium aluminides [J]. Prog. Mater. Sci., 2016, 81: 55
doi: 10.1016/j.pmatsci.2016.01.001
|
| 2 |
Zhang W J, Reddy B V, Deevi S C. Physical properties of TiAl-base alloys [J]. Scr. Mater., 2001, 45: 645
doi: 10.1016/S1359-6462(01)01075-2
|
| 3 |
Das G, Kestler H, Clemens H, et al. Sheet gamma TiAl: Status and opportunities [J]. JOM, 2004, 56(11): 42
|
| 4 |
Chen Y Y, Kong F T, Cui N. Preparation and microstructural analysis of TiAl alloy sheet [J]. Mater. China, 2015, 34: 379
|
| 4 |
陈玉勇, 孔凡涛, 崔 宁. TiAl合金板材的制备与组织分析 [J]. 中国材料进展, 2015, 34: 379
|
| 5 |
Lin J P, Chen G L. Development of TiAl intermetallic based compound [J]. Mater. China, 2009, 28(1): 31
|
| 5 |
林均品, 陈国良. TiAl基金属间化合物的发展 [J]. 中国材料进展, 2009, 28(1): 31
|
| 6 |
Zhang D M, Chen G Q, Han J C, et al. Research on gamma TiAl-based alloy sheet fabricated by EB-PVD [J]. J. Aeronaut. Mater., 2006, 26(4): 35
|
| 6 |
章德铭, 陈贵清, 韩杰才 等. EB-PVD制备γ-TiAl基合金薄板的研究 [J]. 航空材料学报, 2006, 26(4): 35
|
| 7 |
Liu J P, Su Y Q, Luo L S, et al. Fabrication of wavy γ-TiAl based sheet with foil metallurgy [J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 72
doi: 10.1016/S1003-6326(11)61142-4
|
| 8 |
Rivard J D K, Blue C A, Ott R D, et al. Advanced manufacturing technologies utilising high density infrared radiant heating [J]. Surf. Eng., 2004, 20: 220
doi: 10.1179/026708404225015022
|
| 9 |
Chen Y Y, Yue H Y, Wang X P, et al. Selective electron beam melting of TiAl alloy: Microstructure evolution, phase transformation and microhardness [J]. Mater. Charact., 2018, 142: 584
doi: 10.1016/j.matchar.2018.06.027
|
| 10 |
Yue H Y, Chen Y Y, Wang X P, et al. Effect of beam current on microstructure, phase, grain characteristic and mechanical properties of Ti-47Al-2Cr-2Nb alloy fabricated by selective electron beam melting [J]. J. Alloys Compd., 2018, 750: 617
doi: 10.1016/j.jallcom.2018.03.343
|
| 11 |
Chen Y Y, Yue H Y, Wang X P. Microstructure, texture and tensile property as a function of scanning speed of Ti-47Al-2Cr-2Nb alloy fabricated by selective electron beam melting [J]. Mater. Sci. Eng., 2018, A713: 195
|
| 12 |
Yue H Y, Chen Y Y, Wang X P, et al. Microstructure, texture and tensile properties of Ti-47Al-2Cr-2Nb alloy produced by selective electron beam melting [J]. J. Alloys Compd., 2018, 766: 450
doi: 10.1016/j.jallcom.2018.07.025
|
| 13 |
Tomita M, Noguchi Y. Miti program on high temperature intermetallics [J]. Trans. Nonferrous Met. Soc. China, 1999, 9(): 346
|
| 14 |
Semiatin S L, Seetharaman V. Deformation and microstructure development during hot-pack rolling of a near-gamma titanium aluminide alloy [J]. Metall. Mater. Trans., 1995, 26A: 371
|
| 15 |
Clemens H, Kestler H. Processing and applications of intermetallic γ‐TiAl‐based alloys [J]. Adv. Eng. Mater., 2000, 2: 551
doi: 10.1002/1527-2648(200009)2:9<551::AID-ADEM551>3.0.CO;2-U
|
| 16 |
Zhang G C. TiAl intermetallic sheet isothermal rolling equipment and technology [J]. Titanium Alloy. Inf., 1996, (1): 7
|
| 16 |
张功才. TiAl金属间化合物薄板的等温轧制设备及其工艺 [J]. 钛合金信息, 1996, (1): 7
|
| 17 |
Cui X P. Microstructure and mechanical properties of micro-laminated TiB2-TiAl composite sheets prepared by roll bonding and reaction annealing [D]. Harbin: Harbin Institute of Technology, 2012
|
| 17 |
崔喜平. 轧制及反应退火制备微叠层TiB2-TiAl复合材料板组织与性能 [D]. 哈尔滨: 哈尔滨工业大学, 2012
|
| 18 |
Clemens H, Glatz W, Eberhardt N, et al. Processing, properties and applications of gamma titanium aluminide sheet and foil materials [J]. MRS Online Proc. Lib., 1996, 460: 29
|
| 19 |
Zhou H T, Kong F T, Wang X P, et al. High strength in high Nb containing TiAl alloy sheet with fine duplex microstructure produced by hot pack rolling [J]. J. Alloys Compd., 2017, 695: 3495
doi: 10.1016/j.jallcom.2016.12.005
|
| 20 |
Zhou H T, Kong F T, Wu K, et al. Hot pack rolling nearly lamellar Ti-44Al-8Nb-(W, B, Y) alloy with different rolling reductions: Lamellar colonies evolution and tensile properties [J]. Mater. Des., 2017, 121: 202
doi: 10.1016/j.matdes.2017.02.053
|
| 21 |
Liu H W. Hot working, structure and properties of (γ + α2 + B2) multiphase TiAl alloy [D]. Qinhuangdao: Yanshan University, 2017
|
| 21 |
刘宏武. (γ + α2 + B2)三相TiAl合金热加工特性及组织性能研究 [D]. 秦皇岛: 燕山大学, 2017
|
| 22 |
Zhang Y, Wang X P, Kong F T, et al. A high-performance β-stabilized Ti-43Al-9V-0.2Y alloy sheet with a nano-scaled antiphase domain [J]. Mater. Lett., 2018, 214: 182
doi: 10.1016/j.matlet.2017.12.002
|
| 23 |
Zhang Y, Wang X P, Kong F T, et al. A high-performance β-solidifying TiAl alloy sheet: Multi-type lamellar microstructure and phase transformation [J]. Mater. Charact., 2018, 138: 136
doi: 10.1016/j.matchar.2018.02.005
|
| 24 |
Gao S B, Liang Y F, Ye T, et al. In-situ control of microstructure and mechanical properties during hot rolling of high-Nb TiAl alloy [J]. Materialia, 2018, 1: 229
doi: 10.1016/j.mtla.2018.05.007
|
| 25 |
Liu F X, He Y H, Liu Y, et al. Present status and future prospects for PM TiAl-based alloy sheet [J]. Rare Met. Mater. Eng., 2005, 34: 169
|
| 25 |
刘峰晓, 贺跃辉, 刘 咏 等. 粉末冶金制备TiAl基合金板材的研究现状及趋势 [J]. 稀有金属材料与工程, 2005, 34: 169
|
| 26 |
Yang F, Kong F T, Chen Y Y, et al. Manufacture and present status of TiAl alloy sheet [J]. J. Mater. Eng., 2010, (5): 96
|
| 26 |
杨 非, 孔凡涛, 陈玉勇 等. TiAl合金板材的制备及研究现状 [J]. 材料工程, 2010, (5): 96
|
| 27 |
Xu L, Bai C G, Wang G, et al. Manufacturing of γ-TiAl sheet by hot packed rolling of powder metallurgy preform [J]. Titanium Ind. Prog., 2011, 28(5): 17
|
| 27 |
徐 磊, 柏春光, 王 刚 等. 包覆热轧制备粉末冶金TiAl合金板材及热加工行为研究 [J]. 钛工业进展, 2011, 28(5): 17
|
| 28 |
Liu Y, Liang X P, Liu B, et al. Investigations on processing powder metallurgical high-Nb TiAl alloy sheets [J]. Intermetallics, 2014, 55: 80
doi: 10.1016/j.intermet.2014.07.013
|
| 29 |
Li H Z, Qi Y L, Liang X P, et al. Microstructure and high temperature mechanical properties of powder metallurgical Ti-45Al-7Nb-0.3W alloy sheets [J]. Mater. Des., 2016, 106: 90
doi: 10.1016/j.matdes.2016.05.113
|
| 30 |
Zhang D D. Preparation of powder TiAl alloy sheet and study on microstructure and properties [D]. Harbin: Harbin Institute of Technology, 2020
|
| 30 |
张冬冬. 粉末TiAl合金板材的制备及其组织性能研究 [D]. 哈尔滨: 哈尔滨工业大学, 2020
|
| 31 |
Matsuo M. Developments in processing technology of gamma titanium aluminides for potential application to airframe structures [J]. ISIJ Int., 1991, 31: 1212
doi: 10.2355/isijinternational.31.1212
|
| 32 |
Hanamura T, Hashimoto K. Improvement of microstructure and mechanical properties in TiB2-doped TiAl alloy by direct sheet casting [J]. Mater. Trans. JIM, 1998, 39: 724
|
| 33 |
Shen Z Z. The Investigation of manufacturing, microstructure, properties of high Nb-TiAl alloy sheet [D]. Beijing: University of Science and Technology Beijing, 2016
|
| 33 |
沈正章. 高Nb-TiAl合金板材制备及组织性能研究 [D]. 北京: 北京科技大学, 2016
|
| 34 |
Zeng S W. Research on hot deformation and oxidation behavior of TiAl containing Nb, Mo [D]. Beijing: University of Science and Technology Beijing, 2016
|
| 34 |
曾尚武. 含铌、钼TiAl合金热变形及氧化行为研究 [D]. 北京: 北京科技大学, 2016
|
| 35 |
Chen L. Study on microstructure optimization and creep properties of TiAl alloy containing β stable element [D]. Beijing: University of Science and Technology Beijing, 2021
|
| 35 |
陈 林. 含β稳定元素TiAl合金组织优化及其蠕变性能研究 [D]. 北京: 北京科技大学, 2021
|
| 36 |
Li T R, Liu G H, Xu M, et al. High temperature deformation and control of homogeneous microstructure during hot pack rolling of Ti-44Al-5Nb-(Mo, V, B) alloys: The impact on mechanical properties [J]. Mater. Sci. Eng., 2019, A751: 1
|
| 37 |
Luo J G, Acoff V L. Processing gamma-based TiAl sheet materials by cyclic cold roll bonding and annealing of elemental titanium and aluminum foils [J]. Mater. Sci. Eng., 2006, A433: 334
|
| 38 |
Zhang R G, Acoff V L. Processing sheet materials by accumulative roll bonding and reaction annealing from Ti/Al/Nb elemental foils [J]. Mater. Sci. Eng., 2007, A463: 67
|
| 39 |
Chaudhari G P, Acoff V L. Titanium aluminide sheets made using roll bonding and reaction annealing [J]. Intermetallics, 2010, 18: 472
doi: 10.1016/j.intermet.2009.09.008
|
| 40 |
Kong F T, Chen Y Y. Preparation of γ-TiAl/TC4 composite sheet and its microstructure and properties [J]. Rare Met. Mater. Eng., 2009, 38: 1484
|
| 40 |
孔凡涛, 陈玉勇. γ-TiAl/TC4复合板材的制备及组织性能研究 [J]. 稀有金属材料与工程, 2009, 38: 1484
|
| 41 |
Bian Z W. Study of process of rolling and heat treatment on multilaminated Ti-B4C/Al sheets [D] Harbin: Harbin Institute of Technology, 2010
|
| 41 |
边卓伟. 多层Ti-(B4C/Al)板轧制和热处理工艺研究 [D]. 哈尔滨: 哈尔滨工业大学, 2010
|
| 42 |
Wang Y. Microstructure and mechanical properties of titanium aluminide composite sheet prepared by roll bonding and reactive annealing [D]. Harbin: Harbin Institute of Technology, 2011
|
| 42 |
王 银. 叠轧及热处理制备钛铝基复合材料板的微观组织与性能 [D]. 哈尔滨: 哈尔滨工业大学, 2011
|
| 43 |
Sun W, Yang F, Kong F T, et al. Interface characteristics of Ti6Al4V-TiAl metal-intermetallic laminate (MIL) composites prepared by a novel hot-pack rolling [J]. Mater Charact., 2018, 144: 173
doi: 10.1016/j.matchar.2018.07.010
|
| 44 |
Ren L B, Wang J, Wang H W, et al. A method for preparing titanium alloy sheet by roll bonding using steel plate can [P]. Chin Pat, 201110104578.8, 2011
|
| 44 |
任连宝, 王 俭, 王红武 等. 一种钢板包覆叠轧制备钛合金薄板的方法 [P]. 中国专利, 201110104578.8, 2011)
|
|