| Pb-Al合金定向凝固组织形成过程 |
李彦强1,2, 赵九洲1,2( ), 江鸿翔1,2, 何杰1,2 |
1.中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 2.中国科学技术大学 材料科学与工程学院 沈阳 110016 |
|
| Microstructure Formation in Directionally Solidified Pb-Al Alloy |
LI Yanqiang1,2, ZHAO Jiuzhou1,2( ), JIANG Hongxiang1,2, HE Jie1,2 |
1.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2.School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China |
引用本文:
李彦强, 赵九洲, 江鸿翔, 何杰. Pb-Al合金定向凝固组织形成过程[J]. 金属学报, 2022, 58(8): 1072-1082.
Yanqiang LI,
Jiuzhou ZHAO,
Hongxiang JIANG,
Jie HE.
Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. Acta Metall Sin, 2022, 58(8): 1072-1082.
| 1 |
Yi T F, Dai C S, Hu X G, et al. Research progress in lead foam grid materials for lead acid batteries [J]. Batte. Bimonth., 2006, 36: 229
|
| 1 |
伊廷锋, 戴长松, 胡信国 等. 铅酸电池泡沫铅板栅材料的研究进展 [J]. 电池, 2006, 36: 229
|
| 2 |
Xu L, Yan M, Wang X Y, et al. The influences of silver and zinc addition on the electrochemical performances of the Pb-Ca-Sn grids for lead acid batteries [J]. Metall. Res. Technol., 2018, 115: 6
|
| 3 |
Wu Z F, Hu C, Mu J Y, et al. Investigation of Pb-Sr and Pb-Ca binary alloys as grids for lead-acid batteries [J]. Int. J. Electrochem. Sci., 2019, 14: 8709
|
| 4 |
Wang X K, Chen S, Chen B M, et al. Study status of energy saving anodes and electrolyte ions for copper electrowinning [J]. Mater. Prot., 2020, 53(8): 117
|
| 4 |
王秀凯, 陈 胜, 陈步明 等. 铜电积用节能阳极及电解液离子影响的研究现状 [J]. 材料保护, 2020, 53(8): 117
|
| 5 |
Zhuang S W, Wu B, Duan N, et al. Research progress in anodes for zinc electrowinning [J]. Acta Mater. Compos. Sin., 2021, 38: 1313
|
| 5 |
庄思伟, 吴 冰, 段 宁 等. 锌电沉积阳极的研究进展 [J]. 复合材料学报, 2021, 38: 1313
|
| 6 |
Xiong Y L, Wang Y F, Roselle G, et al. Lead/lead-alloy as a corrosion-resistant outer layer packaging material for high level nuclear waste disposal [J]. Nucl. Eng. Des., 2021, 380: 111294
doi: 10.1016/j.nucengdes.2021.111294
|
| 7 |
Ahmed T, Jiang H X, Li W, et al. Solidification of Pb-Al alloys under the influence of electric current pulses [J]. Acta Metall. Sin. (Engl. Lett.), 2018, 31: 842
doi: 10.1007/s40195-017-0685-1
|
| 8 |
Li S R. Lead and Lead Alloy [M]. Changsha: Central South University Press, 1996: 262
|
| 8 |
李松瑞. 铅及铅合金 [M]. 长沙: 中南大学出版社, 1996: 262
|
| 9 |
Cole J F, Goodwin F E. The development and potential applications of a Pb-Al alloy [J]. JOM, 1990, 42: 41
doi: 10.1007/BF03221021
|
| 10 |
Cao Y D. Preparation and performance of a novel lead-based alloy anode for zinc electrowinning [D]. Kunming: Kunming University of Science and Technology, 2009
|
| 10 |
曹远栋. 锌电积用新型铅基合金阳极的制备及性能研究 [D]. 昆明: 昆明理工大学, 2009
|
| 11 |
Li W, Sun Q, Jiang H X, et al. Solidification of Al-Bi alloy and influence of microalloying element Sn [J]. Acta Metall. Sin., 2019, 55: 831
|
| 11 |
黎 旺, 孙 倩, 江鸿翔 等. Al-Bi合金凝固过程及微合金化元素Sn的影响 [J]. 金属学报, 2019, 55: 831
|
| 12 |
Zhao J Z, Ahmed T, Jiang H X, et al. Solidification of immiscible alloys: A review [J]. Acta Metall. Sin. (Engl. Lett.), 2017, 30: 1
doi: 10.1007/s40195-016-0523-x
|
| 13 |
Deng C K, Jiang H X, Zhao J Z, et al. Study on the solidification of Ag-Ni monotectic alloy [J]. Acta Metall. Sin., 2020, 56: 212
|
| 13 |
邓聪坤, 江鸿翔, 赵九洲 等. Ag-Ni偏晶合金凝固过程研究 [J]. 金属学报, 2020, 56: 212
doi: 10.11900/0412.1961.2019.00192
|
| 14 |
Gránásy L, Ratke L. Homogeneous nucleation within the liquid miscibility gap of Zn-Pb alloys [J]. Scr. Metall. Mater., 1993, 28: 1329
doi: 10.1016/0956-716X(93)90477-A
|
| 15 |
Ratke L, Diefenbach S. Liquid immiscible alloys [J]. Mater. Sci. Eng., 1995, R15: 263
|
| 16 |
Li H L. Study of the mechanism of the microstructure evolution in directionally solidified monotectic alloys [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2009
|
| 16 |
李海丽. 偏晶合金定向凝固过程中组织演变机理研究 [D]. 沈阳: 中国科学院金属研究所, 2009
|
| 17 |
Zhao J, Ratke L. Repeated nucleation of minority phase droplets induced by drop motion [J]. Scr. Mater., 1998, 39: 181
doi: 10.1016/S1359-6462(98)00141-9
|
| 18 |
Jiang H X, Zhao J Z. Effect mechanism of a direct current on the solidification of immiscible alloys [J]. Chin. Phys. Lett., 2012, 29: 088104
|
| 19 |
Zhao J Z, Ratke L, Jia J, et al. Modeling and simulation of the microstructure evolution during a cooling of immiscible alloys in the miscibility gap [J]. J. Mater. Sci. Technol., 2002, 18: 197
|
| 20 |
Shangguan D, Ahuja S, Stefanescu D M. An analytical model for the interaction between an insoluble particle and an advancing solid/liquid interface [J]. Metall. Trans., 1992, 23A: 669
|
| 21 |
Li H L, Zhao J Z. Convective effect on the microstructure evolution during a liquid-liquid decomposition [J]. Appl. Phys. Lett., 2008, 92: 241902
doi: 10.1063/1.2945634
|
| 22 |
Einstein A. A new determination of molecular dimensions [J]. Ann. Phys., 1906, 324: 289
doi: 10.1002/andp.19063240204
|
| 23 |
Yu S K, Sommer F, Predel B. Isopiestic measurements and assessment of the Al-Pb System [J]. Z. Metallkd., 1996, 87: 574
|
| 24 |
Takamichi I, Roderick I L G, translated by Xian A P, Wang L W. The Physical Properties of Liquid Metals [M]. Beijing: Science Press, 2006: 256
|
| 24 |
Takamichi I, Roderick I L G著, 冼爱平, 王连文译. 液态金属的物理性能 [M]. 北京: 科学出版社, 2006: 256
|
| 25 |
Li H L, Zhao J Z, Zhang Q X, et al. Microstructure formation in a directionally solidified immiscible alloy [J]. Metall. Mater. Trans., 2008, 39A: 3308
|
|