Please wait a minute...
金属学报  2021, Vol. 57 Issue (2): 171-181    DOI: 10.11900/0412.1961.2020.00308
  综述 本期目录 | 过刊浏览 |
烧结NdFeB永磁材料腐蚀与防护的研究现状及挑战
吴玉程1,2(), 高志强3, 徐光青4, 刘家琴5, 轩海成3, 刘友好6, 衣晓飞6, 陈静武6, 韩培德3
1.太原理工大学 教育部新材料界面科学与工程重点实验室 太原 030024
2.合肥工业大学 有色金属与加工技术国家地方联合工程研究中心 合肥 230009
3.太原理工大学 材料科学与工程学院 太原 030024
4.合肥工业大学 材料科学与工程学院 合肥 230009
5.合肥工业大学 工业与装备技术研究院 合肥 230009
6.安徽大地熊新材料股份有限公司 稀土永磁材料国家重点实验室 合肥 231500
Current Status and Challenges in Corrosion and Protection Strategies for Sintered NdFeB Magnets
WU Yucheng1,2(), GAO Zhiqiang3, XU Guangqing4, LIU Jiaqin5, XUAN Haicheng3, LIU Youhao6, YI Xiaofei6, CHEN Jingwu6, HAN Peide3
1.Key Laboratory of Interface Science and Engineering of New Materials, Ministry of Education, Taiyuan University of Technology, Taiyuan 030024, China
2.National-Local Joint Engineering Research Centre of Nonferrous Metals and Processing Technology, Hefei University of Technology, Hefei 230009, China
3.School of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024, China
4.School of Materials Science and Engineering, Hefei University of Technology, Hefei 230009, China
5.Institute of Industry and Equipment Technology, Hefei University of Technology, Hefei 230009, China
6.State Key Laboratory of Rare Earth Permanent Magnet Materials, Anhui Earth-Panda Advance Magnetic Material Co. , Ltd. , Hefei 231500, China
引用本文:

吴玉程, 高志强, 徐光青, 刘家琴, 轩海成, 刘友好, 衣晓飞, 陈静武, 韩培德. 烧结NdFeB永磁材料腐蚀与防护的研究现状及挑战[J]. 金属学报, 2021, 57(2): 171-181.
Yucheng WU, Zhiqiang GAO, Guangqing XU, Jiaqin LIU, Haicheng XUAN, Youhao LIU, Xiaofei YI, Jingwu CHEN, Peide HAN. Current Status and Challenges in Corrosion and Protection Strategies for Sintered NdFeB Magnets[J]. Acta Metall Sin, 2021, 57(2): 171-181.

全文: PDF(1400 KB)   HTML
摘要: 

烧结NdFeB永磁材料的腐蚀敏感性限制了其在复杂工况下的应用,提高磁体的抗腐蚀能力和开发优异的防护涂层是领域发展的重点方向。尽管针对长寿命NdFeB磁体的探索已经做了大量工作,但是从技术工艺到基础理论,系统地研究NdFeB磁体的腐蚀问题仍然比较少,这一方面是由于材料腐蚀与防护的基础研究滞后于磁性能方面的研究工作,另一方面还与市场对材料品质要求的不断提高及多样化需求有较大关系。本文综述了耐蚀烧结NdFeB永磁材料的最新研究成果,包括影响腐蚀的因素、提高磁体耐蚀性能的基础理论及方法、表面防护战略的基本框架及工程应用中的关键技术;最后,展望了未来前景并分析了面临的挑战,期望为今后的发展指明方向。

关键词 : NdFeB,  腐蚀,  涂层,  双合金法,  物理气相沉积    
Abstract:

The susceptibility of sintered NdFeB to corrosion in harsh environments limits their wide variety of applications. Improved resistance to corrosion of NdFeB magnets and advancement of surface coatings are critical directions in permanent magnet material fields. Significant work has been undertaken on the development of long-life NdFeB magnets. However, comprehensive research of NdFeB corrosion, from process technology to fundamental theory, is lacking, mainly owing to the hysteresis in the study of the elementary works of corrosion and protection related to magnetism, and improving the quality and diversified market demands. This analysis covers recent research that has led to advances in anti-corrosion material technology for NdFeB magnets, including corrosion factors, contemporary methodologies from technology to fundamentals, the basic framework for surface protection and key techniques in the industry application. Finally, prospects and existing challenges in the field of corrosion and protection are reviewed, attempting to identify future developments and directions.

Key words: NdFeB    corrosion    coating    binary alloy technology    physical vapor deposition
收稿日期: 2020-08-17     
ZTFLH:  TB34  
基金资助:国家自然科学基金项目(20571022);国家科技支撑计划项目(012BAE02B01);安徽省重点研究与开发计划项目;安徽省科技重大专项项目(17030901063);安徽省科技攻关计划项目(1301022080)
作者简介: 吴玉程,男,1962年生,教授,博士
图1  NdFeB材料组织示意图
图2  磁体在腐蚀前后的磁场分布[13]
图3  剩磁对NdFeB磁体腐蚀影响的示意图[22](a) unmagnetized sample(b) axile magnetized sample(c) radial magnetized sample
图4  NdFeB材料的微观组织结构形貌[13]
ElementSpeciationRoleTypical element
Rare earthNd-M1-FeSubstitute for NdDy, Tb, Ce, La, Y
Transition/group elementNd-M2 or Nd-M2-FeSubstitute for FeCu, Al, Ga, Zn, Ge, Sn
Transition/group elementM3-B or Fe-M3-BSubstitute for FeCo, Nb, Zr, Ti, V, Mo
表1  合金化法常用元素及其作用
图5  功能梯度涂层材料结构示意图[106]
1 Jiang W, Shen L D, Wang K, et al. Study on Ni-Ni(S)-Ni(P) multilayer coating by friction-assisted jet electroplating on sintered NdFeB [J]. J. Alloys Compd., 2019, 787: 1089
2 Zhang J X, Zhang T J, Cui K. Mechanism and prevention of NdFeB magnet corrosion [J]. Dev. Appl. Mater., 2001, 16(4): 38
2 张静贤, 张同俊, 崔 琨. NdFeB永磁材料腐蚀机理与防护 [J]. 材料开发与应用, 2001, 16(4): 38
3 Liao X F, Zhang J S, Yu H Y, et al. Understanding the phase structure, magnetic properties and anti-corrosion behavior of melt-spun (La, Y)2Fe14B alloys [J]. J. Magn. Magn. Mater., 2019, 489: 165444
4 Kong X W, Liu G Z, Zhao M J, et al. Research status of corrosion property of sintered NdFeB permanent magnet [J]. Chin. Rare Earths, 2013, 34(6): 69
4 孔祥薇, 刘国征, 赵明静等. 烧结NdFeB永磁体的腐蚀性研究现状 [J]. 稀土, 2013, 34(6): 69
5 Li H Y, Hao Z Z, Liu Y H, et al. Research progress on corrosion mechanism and surface protection technology of sintered NdFeB permanent magnets [J]. Min. Metall. Eng., 2016, 36(6): 118
5 李红英, 郝壮志, 刘宇晖等. 烧结NdFeB永磁材料腐蚀机理与表面防护技术研究进展 [J]. 矿冶工程, 2016, 36(6): 118
6 Yan F Y, Zhao C Y, Zhang L. Advances in protective technology on NdFeB permanent magnetic material [J]. Plat. Finish., 2012, 34(8): 22
6 严芬英, 赵春英, 张 琳. 钕铁硼永磁材料表面防护技术的研究进展 [J]. 电镀与精饰, 2012, 34(8): 22
7 Liu W, Hou J. Production status and prospect of NdFeB magnet electroplating [J]. Plat. Finish., 2012, 34(4): 20
7 刘 伟, 侯 进. 钕铁硼电镀技术生产现状与展望 [J]. 电镀与精饰, 2012, 34(4): 20
8 Wang E S. The anti-corrosion technology of NdFeB chemical conversion coating [J]. Plat. Finish., 2013, 35(12): 13
8 王恩生. 钕铁硼化学转化膜防腐蚀技术 [J]. 电镀与精饰, 2013, 35(12): 13
9 Hu F, Xu W, Dai M J, et al. Research progress on physical vapor deposition and related process of NdFeB magnets [J]. Mater. Rev., 2014, 28(3): 20
9 胡 芳, 许 伟, 代明江等. 钕铁硼永磁材料物理气相沉积技术及相关工艺的研究进展 [J]. 材料导报, 2014, 28(3): 20
10 Chen X P, Zhao D L, Li Y, et al. The development of electroplating process and equipment on NdFeB permanent magnet materials [J]. Met. Funct. Mater., 2015, 22(5): 32
10 陈小平, 赵栋梁, 李 勇等. 钕铁硼永磁材料电镀工艺与装备的发展 [J]. 金属功能材料, 2015, 22(5): 32
11 Peng N, Wang X D, Chen X P, et al. Study on surface protection for NdFeB permanent magnet alloy [J]. Hot Work. Technol., 2016, 45(4): 6
11 彭 楠, 王向东, 陈小平等. 钕铁硼永磁体的表面防护技术研究 [J]. 热加工工艺, 2016, 45(4): 6
12 Liu W Q, Yue M, Zhang J X, et al. Intrinsic corrosion characteristic of sintered NdFeB permanent magnets [J]. Powder Metall. Technol., 2006, 24: 195
12 刘卫强, 岳 明, 张久兴等. 烧结NdFeB永磁合金本征腐蚀特性研究进展 [J]. 粉末冶金技术, 2006, 24: 195
13 Yan G L, McGuiness P J, Farr J P G, et al. Environmental degradation of NdFeB magnets [J]. J. Alloys Compd., 2009, 478: 188
14 Wu Y P, Zhu M G, Shi X N, et al. Corrosion research of (Ce15Nd85)30FebalB1M sintered magnet in hydrothermal environment [J]. J. Chin. Soc. Rare Earth, 2016, 34: 171
14 吴亚萍, 朱明刚, 石晓宁等. (Ce15Nd85)30FebalB1M永磁体湿热条件下的腐蚀性研究 [J]. 中国稀土学报, 2016, 34: 171
15 Wu Y P, Zhu M G, Shi X N, et al. Study on the diversity of corrosion products of (Ce20Nd80)31FebalB1M magnet [J]. Powder Metall. Ind., 2017, 27(5): 36
15 吴亚萍, 朱明刚, 石晓宁等. (Ce20Nd80)31FebalB1M磁体腐蚀产物多样性的研究 [J]. 粉末冶金工业, 2017, 27(5): 36
16 Liu W Q, Yue M, Zhang D T, et al. Corrosion behavior of conventional and spark plasma-sintered Nd-Fe-B permanent magnets in different solutions [J]. Corrosion, 2009, 65: 501
17 Liu W Q, Yue M, Zhang J X, et al. The effect of Nd-rich phase for sintered NdFeB corrosion resistance [J]. Rare Met. Mater. Eng., 2007, 36: 1066
17 刘卫强, 岳 明, 张久兴等. 富钕相对烧结NdFeB磁体耐腐蚀性的影响 [J]. 稀有金属材料与工程, 2007, 36: 1066
18 Cui J, Kramer M, Zhou L, et al. Current progress and future challenges in rare-earth-free permanent magnets [J]. Acta Mater., 2018, 158: 118
19 Li J J, An G H, Guo C J, et al. Accelerated corrosion behavior of sintered NdFeB magnets in HAST climate [J]. J. Chin. Soc. Rare Earths, 2016, 34: 555
19 李家节, 安桂焕, 郭诚君等. 烧结NdFeB磁体高温高压高湿加速腐蚀行为研究 [J]. 中国稀土学报, 2016, 34: 555
20 Nan H Y, Zhu L Q, Liu H C, et al. Protection of NdFeB magnets by corrosion resistance phytic acid conversion film [J]. App. Surf. Sci., 2015, 355: 1215
21 Zhou L J, Pei W L, Guo X L, et al. Corrosion behavior of low cost sintered Nd-Fe-B magnet containing element Ce [J]. J. Mater. Metall., 2015, 14: 217
21 周丽娟, 裴文利, 郭小莲等. 含Ce烧结Nd-Fe-B磁体的腐蚀行为 [J]. 材料与冶金学报, 2015, 14: 217
22 Zheng J W, Du Z Y, Jiang M Y, et al. Corrosion behavior of Nd-Fe-B sintered magnets at remanence state [J]. Rare Met. Mater. Eng., 2008, 37: 1369
22 郑精武, 都周云, 蒋梅燕等. 烧结钕铁硼在剩磁状态下的腐蚀研究 [J]. 稀有金属材料与工程, 2008, 37: 1369
23 Jiang L Q, Zheng J W. Corrosion behavior of sintered NdFeB magnets in various acid solution [J]. Rare Met. Mater. Eng., 2006, 35: 340
23 姜力强, 郑精武. 烧结钕铁硼在各种酸介质中的腐蚀研究 [J]. 稀有金属材料与工程, 2006, 35: 340
24 Xu J L, Huang Z X, Luo J M, et al. Corrosion behavior of sintered NdFeB magnets in different acidic solutions [J]. Rare Met. Mater. Eng., 2015, 44: 786
25 Ding X, Xue L F, Ding K H, et al. Corrosion behavior of the sintered Nd-Fe-B permanent magnets in different acid solutions [J]. J. Cent. South Univ. (Sci. Technol.), 2016, 47: 1105
25 丁 霞, 薛龙飞, 丁开鸿等. 烧结钕铁硼永磁合金在不同酸溶液中的腐蚀行为 [J]. 中南大学学报(自然科学版), 2016, 47: 1105
26 Sueptitz R, Uhlemann M, Gebert A, et al. Corrosion, passivation and breakdown of passivity of neodymium [J]. Corros. Sci., 2010, 52: 886
27 Liu H, Fu S, Fu Q Q, et al. Research status of medical NdFeB implantation surface modification [J]. Prog. Mod. Biomed., 2019, 19: 175
27 刘 豪, 付 珊, 付琴琴等. 医用钕铁硼体内植入表面改性研究现状 [J]. 现代生物医学进展, 2019, 19: 175
28 Tang Z, Wu J Y, Chen X. In vitro study of the corrosiveness resistance property of NdFeB magnet with different coatings [J]. J. Pract. Stomatol., 2013, 29: 195
28 唐 镇, 吴建勇, 陈 溪. 不同镀膜钕铁硼磁体抗腐蚀性的体外实验研究 [J]. 实用口腔医学杂志, 2013, 29: 195
29 Tian B Y, Liu H, Fu S, et al. In vitro study on corrosion resistance of different surface modified [J]. China Med. Dev., 2019, 34(3): 5
29 田波彦, 刘 豪, 付 珊等. 不同表面改性钕铁硼磁体抗胃液腐蚀的体外研究 [J]. 中国医疗设备, 2019, 34(3): 5
30 Tian B Y, Liu H, Fu S, et al. In vitro study on the bile corrosion resistance of NdFeB magnets with different coatings [J]. Prog. Mod. Biomed., 2019, 19: 1006
30 田波彦, 刘豪, 付珊等. 不同镀层钕铁硼磁体抗胆汁腐蚀的体外研究 [J]. 现代生物医学进展, 2019, 19: 1006
31 Costa I, Oliveira M C L, de Melo H G, et al. The effect of the magnetic field on the corrosion behavior of Nd-Fe-B permanent magnets [J]. J. Magn. Magn. Mater., 2004, 278: 348
32 Sueptitz R, Tschulik K, Uhlemann M, et al. Effect of magnetization state on the corrosion behaviour of NdFeB permanent magnets [J]. Corros. Sci., 2011, 53: 2843
33 Yan G L, Williams A J, Farr J P G, et al. The effect of density on the corrosion of NdFeB magnets [J]. J. Alloys Compd., 1999, 292: 266
34 Zhou L, Liu T, Zhang X, et al. Facters affecting corrosion weight loss of sintered NdFeB magnets and improvement in corrosion resistance [J]. J. Magn. Mater. Dev., 2018, 49(4): 10
34 周 磊, 刘 涛, 张 昕等. 烧结钕铁硼磁体腐蚀失重的影响因素及耐蚀性改进 [J]. 磁性材料及器件, 2018, 49(4): 10
35 Wang Z X, Pei K, Zhang J J, et al. Correlation between the microstructure and magnetic configuration in coarse-grain inhibited hot-deformed Nd-Fe-B magnets [J]. Acta Mater., 2019, 167: 103
36 Zhang P, Hu M J, Ke H B, et al. Tuning grain boundary fine structure in Nd65Ni35-added Nd-Fe-B based magnets [J]. J. Magn. Magn. Mater., 2018, 465: 246
37 Tan C L, Bao D X, Yan M. Sintered Nd-Fe-B magnets for high temperatures [J]. Mater. Rev., 2005, 19(4): 97
37 谭春林, 包大新, 严 密. 高工作温度烧结钕铁硼磁体的研究现状 [J]. 材料导报, 2005, 19(4): 97
38 El-Moneim A A, Gebert A, Uhlemann M, et al. The influence of Co and Ga additions on the corrosion behavior of nanocrystalline NdFeB magnets [J]. Corros. Sci., 2002, 44: 1857
39 Li J J, Huang X Y, Zeng L L, et al. Tuning magnetic properties, thermal stability and microstructure of NdFeB magnets with diffusing Pr-Zn films [J]. J. Mater. Sci. Technol., 2020, 41: 81
40 Chen H, Yang X, Sun L, et al. Effects of Ag on the magnetic and mechanical properties of sintered NdFeB permanent magnets [J]. J. Magn. Magn. Mater., 2019, 485: 49
41 Liu W Q, Zha S S, Yue M, et al. Research progress of sintered Nd-Fe-B permanent magnets with high coercivity [J]. J. Beijing Univ. Technol., 2017, 43: 1569
41 刘卫强, 查善顺, 岳 明等. 高矫顽力烧结钕铁硼永磁研究进展 [J]. 北京工业大学学报, 2017, 43: 1569
42 Zhang P, Ma T Y, Liang L P, et al. Influence of Ta intergranular addition on microstructure and corrosion resistance of Nd-Dy-Fe-B sintered magnets [J]. J. Alloys Compd., 2014, 593: 137
43 Yu L Q, Huang C C, Yuan Y F. Effect of Nd, Dy content on magnetic properties and corrosion resistance of NdFeB [J]. Powder Metall. Ind., 2008, 18(6): 19
43 于濂清, 黄翠翠, 袁永锋. Nd, Dy含量对高磁能积烧结NdFeB磁性能和耐蚀性影响 [J]. 粉末冶金工业, 2008, 18(6): 19
44 Xie Z F, Zhang S M, Gao H Q. Effects on addition of Dy and Nb on microstructure and properties of sintered NdFeB magnets [J]. Chin. Rare Earths, 2013, 34(3): 36
44 谢泽峰, 张时茂, 高海强. 添加Dy、Nb对烧结NdFeB磁体结构与性能的影响 [J]. 稀土, 2013, 34(3): 36
45 Li J, Zhou L, Liu T, et al. Progress of grain boundary diffusion technique with Dy for sintered Nd-Fe-B magnet [J]. Chin. Rare Earths, 2013, 34(3): 86
45 李 建, 周 磊, 刘 涛等. 烧结钕铁硼晶界扩散Dy工艺进展 [J]. 稀土, 2013, 34(3): 86
46 Liu X L, Wang X J, Liang L P, et al. Rapid coercivity increment of Nd-Fe-B sintered magnets by Dy69Ni31 grain boundary restructuring [J]. J. Magn. Magn. Mater., 2014, 370: 76
47 Liu X L, Zhang Y J, Zhang P, et al. Microstructure evolution of Dy69Ni31-added Nd-Fe-B sintered magnets during annealing [J]. J. Magn. Magn. Mater., 2019, 486: 165260
48 Zhou B B, Li X B, Liang X L, et al. Improvement of the magnetic property, thermal stability and corrosion resistance of the sintered Nd-Fe-B magnets with Dy80Al20 addition [J]. J. Magn. Magn. Mater., 2017, 429: 257
49 Liang L P, Ma T Y, Zhang P, et al. Effects of Dy71.5Fe28.5 intergranular addition on the microstructure and the corrosion resistance of Nd-Fe-B sintered magnets [J]. J. Magn. Magn. Mater., 2015, 384: 133
50 Zeng L L, Li J J, Huang X Y, et al. Thermal stability and corrosion resistance of sintered Nd-Fe-B magnets with intergranular addition of Dy80Fe13Ga7 [J]. Chin. J. Rare Met., 2019, 43: 779
50 曾亮亮, 李家节, 黄祥云等. 晶界添加Dy80Fe13Ga7对烧结钕铁硼热稳定性和耐腐蚀性的影响 [J]. 稀有金属, 2019, 43: 779
51 Liang L P, Ma T Y, Zhang P, et al. Coercivity enhancement of NdFeB sintered magnets by low melting point Dy32.5Fe62Cu5.5 alloy modification [J]. J. Magn. Magn. Mater., 2014, 355: 131
52 Fan X D, Ding G F, Chen K, et al. Whole process metallurgical behavior of the high-abundance rare-earth elements LRE (La, Ce and Y) and the magnetic performance of Nd0.75LRE0.25-Fe-B sintered magnets [J]. Acta Mater., 2018, 154: 343
53 Binnemans K, Jones P T, Blanpain B, et al. Recycling of rare earths: A critical review [J]. J Clean. Prod., 2013, 51: 1
54 Lei W K, Zeng Q W, Hu X J, et al. Research status and prospect of high abundant rare earth of permanent magnetic materials [J]. Nonferrous Met. Sci. Eng., 2017, 8(5): 1
54 雷伟凯, 曾庆文, 胡贤君等. 高丰度稀土永磁材料的研究现状与展望 [J]. 有色金属科学与工程, 2017, 8(5): 1
55 Kim A S, Camp F E. High performance NdFeB magnets (invited) [J]. J. Appl. Phys., 1996, 79: 5035
56 Liu W Q, Sun C, Yue M, et al. Improvement of coercivity and corrosion resistance of Nd-Fe-B sintered magnets by doping aluminium nano-particles [J]. J. Rare Earths, 2013, 31: 65
57 Sun C, Liu W Q, Sun H, et al. Improvement of coercivity and corrosion resistance of Nd-Fe-B sintered magnets with Cu nano-particles doping [J]. J. Mater. Sci. Technol., 2012, 28: 927
58 Zhang P, Ma T Y, Liang L P, et al. Improvement of corrosion resistance of Cu and Nb co-added Nd-Fe-B sintered magnets [J]. Mater. Chem. Phys., 2014, 147: 982
59 Wu Y R, Ni J J, Ma T Y, et al. Corrosion resistance of Nd-Fe-B sintered magnets with intergranular addition of Cu60Zn40 powders [J]. Physica, 2010, 405B: 3303
60 Yan M, Ni J J, Ma T Y, et al. Corrosion behavior of Al100-xCux (15≤x≤45) doped Nd-Fe-B magnets [J]. Mater. Chem. Phys., 2011, 126: 195
61 Zeng H X, Wang Q X, Zhang J S, et al. Grain boundary diffusion treatment of sintered NdFeB magnets by low cost La-Al-Cu alloys with various Al/Cu ratios [J]. J. Magn. Magn. Mater., 2019, 490: 165498
62 Ni J J, Zhou S T, Jia Z F, et al. Improvement of corrosion resistance in Nd-Fe-B sintered magnets by intergranular additions of Sn [J]. J. Alloys Compd., 2014, 588: 558
63 Yang Y, Li Z J, Lv S H, et al. Effect of MgO/Mg nanopowders added to grain boundary on magnetic properties and corrosion resistance of sintered Nd-Fe-B [J]. Rare Met. Mater. Eng., 2020, 49: 1366
63 杨 洋, 李志杰, 吕森浩等. 晶界添加MgO/Mg纳米粉对烧结钕铁硼磁性和抗腐蚀性的影响 [J]. 稀有金属材料与工程, 2020, 49: 1366
64 Li Z J, Wang X E, Li J Y, et al. Effects of Mg nanopowders intergranular addition on the magnetic properties and corrosion resistance of sintered Nd-Fe-B [J]. J. Magn. Magn. Mater., 2017, 442: 62
65 Fernengel W, Rodewald W, Blank R, et al. The influence of Co on the corrosion resistance of sintered Nd-Fe-B magnets [J]. J. Magn. Magn. Mater., 1999, 196-197: 288
66 Zhang P, Ma T Y, Liang L P, et al. Improved corrosion resistance of low rare-earth Nd-Fe-B sintered magnets by Nd6Co13Cu grain boundary restructuring [J]. J. Magn. Magn. Mater., 2015, 379: 186
67 Isotahdon E, Huttunen-Saarivirta E, Kuokkala V T, et al. Corrosion behaviour of sintered Nd-Fe-B magnets [J]. Mater. Chem. Phys., 2012, 135: 762
68 Zhang P, Liang L P, Jin J Y, et al. Magnetic properties and corrosion resistance of Nd-Fe-B magnets with Nd64Co36 intergranular addition [J]. J. Alloys Compd., 2014, 616: 345
69 Hu Z H, Liu G J, Wang H J. Effect of niobium on thermal stability and impact toughness of Nd-Fe-B magnets with ultra-high intrinsic coercivity [J]. J. Rare Earths, 2011, 29: 243
70 Yu L Q, Wen Y H, Yan M. Effects of Dy and Nb on the magnetic properties and corrosion resistance of sintered NdFeB [J]. J. Magn. Magn. Mater., 2004, 283: 353
71 Yu L Q, Zhong X L, Zhang Y P, et al. Production and corrosion resistance of NdFeBZr magnets with an improved response to thermal variations during sintering [J]. J. Magn. Magn. Mater., 2011, 323: 1152
72 Liang L P, Ma T Y, Wu C, et al. Coercivity enhancement of Dy-free Nd-Fe-B sintered magnets by intergranular adding Ho63.4Fe36.6 alloy [J]. J. Magn. Magn. Mater., 2016, 397: 139
73 Xu J L, Xiao Q F, Mei D D, et al. Microstructure, corrosion resistance and formation mechanism of alumina micro-arc oxidation coatings on sintered NdFeB permanent magnets [J]. Surf. Coat. Technol., 2017, 309: 621
74 Xu J L, Xiao Q F, Mei D D, et al. Fabrication and properties of micro-arc oxidation coatings on sintered NdFeB permanent magnets [J]. Rare Met. Mater. Eng., 2018, 47: 1059
75 Xu J L, Xiao Q F, Mei D D, et al. Preparation and characterization of amorphous SiO2 coatings deposited by mirco-arc oxidation on sintered NdFeB permanent magnets [J]. J. Magn. Magn. Mater., 2017, 426: 361
76 Milošev I, Frankel G S. Review-conversion coatings based on zirconium and/or titanium [J]. J. Electrochem. Soc., 2018, 165: C127
77 Huang T, Wang X D, Shi X N, et al. Progress in protection technologies of NdFeB permanent magnets [J]. J. Chin. Soc. Rare Earths, 2018, 36: 394
77 黄 涛, 王向东, 石晓宁等. 钕铁硼稀土永磁材料腐蚀防护技术的研究进展 [J]. 中国稀土学报, 2018, 36: 394
78 Zhang P J, Cao Y J, Sun W, et al. Synthesis and corrosion resistance of CeO2/silane composite coatings on surface of sintered NdFeB magnet [J]. Trans. Mater. Heat Treat., 2020, 41(1): 123
78 张鹏杰, 曹玉杰, 孙 威等. 烧结钕铁硼磁体表面CeO2/硅烷复合涂层的制备及其耐蚀性能 [J]. 材料热处理学报, 2020, 41(1): 123
79 Zaferani S H, Peikari M, Zaarei D, et al. Using silane films to produce an alternative for chromate conversion coatings [J]. Corrosion, 2013, 69: 372
80 Gao Z Q, Zhang D W, Li X G, et al. Current status, opportunities and challenges in chemical conversion coatings for zinc [J]. Colloids Surf., 2018, 546A: 221
81 Gao Z Q, Zhang D W, Liu Z Y, et al. Formation mechanisms of environmentally acceptable chemical conversion coatings for zinc: A review [J]. J. Coat. Technol. Res., 2019, 16: 1
82 Zhang X, Sloof W G, Hovestad A, et al. Characterization of chromate conversion coatings on zinc using XPS and SKPFM [J]. Surf. Coat. Technol., 2005, 197: 168
83 Ouyang Y B, Qiu R, Xiao Y M, et al. Magnetic fluid based on mussel inspired chemistry as corrosion-resistant coating of NdFeB magnetic material [J]. Chem. Eng. J., 2019, 368: 331
84 He W T, Zhu L Q, Chen H N, et al. Electrophoretic deposition of graphene oxide as a corrosion inhibitor for sintered NdFeB [J]. Appl. Surf. Sci., 2013, 279: 416
85 Zhang P J, Xu G Q, Liu J Q, et al. Effect of pretreating technologies on the adhesive strength and anticorrosion property of Zn coated NdFeB specimens [J]. Appl. Surf. Sci., 2016, 363: 499
86 Li Y, Zhu L Q, Li W P, et al. Electrodeposition and properties of copper layer on NdFeB device [J]. J. Mater. Eng., 2017, 45(6): 55
86 李 悦, 朱立群, 李卫平等. 钕铁硼器件表面电沉积铜层及性能 [J]. 材料工程, 2017, 45(6): 55
87 Chen J, Xu B J, Ling G P. Amorphous Al-Mn coating on NdFeB magnets: Electrodeposition from AlCl3-EMIC-MnCl2 ionic liquid and its corrosion behavior [J]. Mater. Chem. Phys., 2012, 134: 1067
88 Ding J J, Xu B J, Ling G P. Al-Mn coating electrodeposited from ionic liquid on NdFeB magnet with high hardness and corrosion resistance [J]. Appl. Surf. Sci., 2014, 305: 309
89 Luo C, Qiu X M, Ruan Y, et al. Effect of Bi addition on the corrosion resistance and mechanical properties of sintered NdFeB permanent magnet/steel soldered joints [J]. Mater. Sci. Eng., 2020, A792: 139832
90 Zhang P J, Wu Y C, Cao Y J, et al. Effects of pretreatment technologies on structure and properties of Al coatings on sintered NdFeB substrates via vacuum evaporation [J]. China Surf. Eng., 2016, 29(4): 49
90 张鹏杰, 吴玉程, 曹玉杰等. 前处理工艺对NdFeB表面真空蒸镀Al薄膜结构及性能的影响 [J]. 中国表面工程, 2016, 29(4): 49
91 Liu J Q, Cao Y J, Zhang P J, et al. Preparation and properties of Al coating on sintered NdFeB magnet surface via vacuum evaporations [J]. Trans. Mater. Heat Treat., 2017, 38(3): 159
91 刘家琴, 曹玉杰, 张鹏杰等. 钕铁硼表面真空蒸镀Al膜的制备及其性能 [J]. 材料热处理学报, 2017, 38(3): 159
92 Chen J, Yang H Y, Xu G Q, et al. Phosphating passivation of vacuum evaporated Al/NdFeB magnets boosting high anti-corrosion performances [J]. Surf. Coat. Technol., 2020, 339: 126115
93 Tao L, Li H Q, Huang Y Q, et al. Structure and corrosion resistance of SiC thin film coated on NdFeB by magnetron sputtering [J]. J. Hefei Univ. Technol. (Nat. Sci.), 2015, 38: 1040
93 陶 磊, 李合琴, 黄依琴等. NdFeB磁控溅射SiC薄膜的结构及耐腐蚀性能 [J]. 合肥工业大学学报(自然科学版), 2015, 38: 1040
94 Hu F, Dai M J, Lin S S, et al. Influences of cycles argon ion bombardment on structure and properties of Al films deposited by magnetron sputtering [J]. China Surf. Eng., 2015, 28(1): 49
94 胡 芳, 代明江, 林松盛等. 循环氩离子轰击对磁控溅射铝膜结构和性能的影响 [J]. 中国表面工程, 2015, 28(1): 49
95 Mao S D, Yang H X, Song Z L, et al. Corrosion behaviour of sintered NdFeB deposited with an aluminium coating [J]. Corros. Sci., 2011, 53: 1887
96 Zhang P J, Liu J Q, Xu G Q, et al. Anticorrosive property of Al coatings on sintered NdFeB substrates via plasma assisted physical vapor deposition method [J]. Surf. Coat. Technol., 2015, 282: 86
97 Mao S D, Yang H X, Li J L, et al. Corrosion properties of aluminium coatings deposited on sintered NdFeB by ion-beam-assisted deposition [J]. Appl. Surf. Sci., 2011, 257: 5581
98 Su Y A, Wan P S, Guo H M. Corrosion mechanism and surface protective technology of sintered Nd-Fe-Boron permanent magnetic material [J]. Mater. Rev., 2004, 18(S3): 257
98 苏永安, 万潘顺, 郭惠铭. 烧结钕铁硼永磁材料腐蚀机理与表面防护技术 [J]. 材料导报, 2004, 18(S3): 257
99 Chaudhary V, Mantri S A, Ramanujan R V, et al. Additive manufacturing of magnetic materials [J]. Prog. Mater. Sci., 2020, 114: 100688
100 Périgo E A, Jacimovic J, Ferré F G, et al. Additive manufacturing of magnetic materials [J]. Addit. Manuf., 2019, 30: 100870
101 He J Z, Lin T, Shao H P, et al. 3D printing of NdFeB rare earth permanent magnet [J]. Chin. J. Rare Met., 2018, 42: 657
101 何建壮, 林 涛, 邵慧萍等. 稀土永磁钕铁硼材料的3D打印研究现状 [J]. 稀有金属, 2018, 42: 657
102 Borkar T, Conteri R, Chen X, et al. Laser additive processing of functionally-graded Fe-Si-B-Cu-Nb soft magnetic materials [J]. Mater. Manuf. Process., 2017, 32: 1581
103 Chaudhary V, Kumar Yadav N M S K, Mantri S A, et al. Additive manufacturing of functionally graded Co-Fe and Ni-Fe magnetic materials [J]. J. Alloys Compd., 2020, 823: 153817
104 Mazeeva A K, Staritsyn M V, Bobyr V V, et al. Magnetic properties of Fe-Ni permalloy produced by selective laser melting [J]. J. Alloys Compd., 2020, 814: 152315
105 Liu Z Q, Meyers M A, Zhang Z F, et al. Functional gradients and heterogeneities in biological materials: Design principles, functions, and bioinspired applications [J]. Prog. Mater. Sci., 2017, 88: 467
106 Zhang C, Chen F, Huang Z F, et al. Additive manufacturing of functionally graded materials: A review [J]. Mater. Sci. Eng., 2019, A764: 138209
[1] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] 王宗谱, 王卫国, Rohrer Gregory S, 陈松, 洪丽华, 林燕, 冯小铮, 任帅, 周邦新. 不同温度轧制Al-Zn-Mg-Cu合金再结晶后的{111}/{111}近奇异晶界[J]. 金属学报, 2023, 59(7): 947-960.
[3] 赵平平, 宋影伟, 董凯辉, 韩恩厚. 不同离子对TC4钛合金电化学腐蚀行为的协同作用机制[J]. 金属学报, 2023, 59(7): 939-946.
[4] 陈润农, 李昭东, 曹燕光, 张启富, 李晓刚. 9%Cr合金钢在含Cl-环境中的初期腐蚀行为及局部腐蚀起源[J]. 金属学报, 2023, 59(7): 926-938.
[5] 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生. Cr添加对孪生诱发塑性钢腐蚀行为的影响[J]. 金属学报, 2023, 59(7): 905-914.
[6] 张奇亮, 王玉超, 李光达, 李先军, 黄一, 徐云泽. EH36钢在不同粒径沙砾冲击下的冲刷腐蚀耦合损伤行为[J]. 金属学报, 2023, 59(7): 893-904.
[7] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[8] 李小涵, 曹公望, 郭明晓, 彭云超, 马凯军, 王振尧. 低碳钢Q235、管线钢L415和压力容器钢16MnNi在湛江高湿高辐照海洋工业大气环境下的初期腐蚀行为[J]. 金属学报, 2023, 59(7): 884-892.
[9] 冯力, 王贵平, 马凯, 杨伟杰, 安国升, 李文生. 冷喷涂辅助感应重熔合成AlCo x CrFeNiCu高熵合金涂层的显微组织和性能[J]. 金属学报, 2023, 59(5): 703-712.
[10] 黄鼎, 乔岩欣, 杨兰兰, 王金龙, 陈明辉, 朱圣龙, 王福会. 基体表面喷丸处理对纳米晶涂层循环氧化行为的影响[J]. 金属学报, 2023, 59(5): 668-678.
[11] 吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展[J]. 金属学报, 2023, 59(4): 502-512.
[12] 韩恩厚, 王俭秋. 表面状态对核电关键材料腐蚀和应力腐蚀的影响[J]. 金属学报, 2023, 59(4): 513-522.
[13] 王京阳, 孙鲁超, 罗颐秀, 田志林, 任孝旻, 张洁. 以抗CMAS腐蚀为目标的稀土硅酸盐环境障涂层高熵化设计与性能提升[J]. 金属学报, 2023, 59(4): 523-536.
[14] 王迪, 贺莉丽, 王栋, 王莉, 张思倩, 董加胜, 陈立佳, 张健. Pt-Al涂层对DD413合金高温拉伸性能的影响[J]. 金属学报, 2023, 59(3): 424-434.
[15] 夏大海, 计元元, 毛英畅, 邓成满, 祝钰, 胡文彬. 2024铝合金在模拟动态海水/大气界面环境中的局部腐蚀机制[J]. 金属学报, 2023, 59(2): 297-308.