| 卷取温度对500 MPa级热冲压桥壳用钢组织与力学性能的影响 |
惠亚军1,2( ), 刘锟1, 吴科敏3, 李秋寒1, 牛涛4, 武巧玲4 |
1 首钢集团有限公司技术研究院薄板研究所 北京 100043 2 首钢集团有限公司绿色可循环钢铁流程北京市重点实验室 北京 100043 3 北京首钢股份有限公司制造部 唐山 064404 4 首钢集团有限公司迁顺技术中心 唐山 064404 |
|
| Effect of Coiling Temperature on Microstructure and Mechanical Properties of 500 MPa Grade Hot Stamping Axle Housing Steel |
HUI Yajun1,2( ), LIU Kun1, WU Kemin3, LI Qiuhan1, NIU Tao4, WU Qiaoling4 |
1 Sheet Metal Research Institute, Technology Institute of Shougang Group Co., Ltd., Beijing 100043, China 2 Beijing Key Laboratory of Green Recyclable Process for Iron & Steel Production of Shougang Group Co., Ltd., Beijing 100043, China 3 Manufacturing Department of Beijing Shougang Co., Ltd., Tangshan 064404, China 4 Qian Shun Technology Center of Shougang Group Co., Ltd., Tangshan 064404, China |
引用本文:
惠亚军, 刘锟, 吴科敏, 李秋寒, 牛涛, 武巧玲. 卷取温度对500 MPa级热冲压桥壳用钢组织与力学性能的影响[J]. 金属学报, 2020, 56(12): 1605-1616.
Yajun HUI,
Kun LIU,
Kemin WU,
Qiuhan LI,
Tao NIU,
Qiaoling WU.
Effect of Coiling Temperature on Microstructure and Mechanical Properties of 500 MPa Grade Hot Stamping Axle Housing Steel[J]. Acta Metall Sin, 2020, 56(12): 1605-1616.
| [1] |
Liu W X. Automotive Design [M]. Beijing: Tsinghua University Press, 2001: 67
|
| [1] |
(刘惟信. 汽车设计 [M]. 北京: 清华大学出版社, 2001: 67)
|
| [2] |
Klein B, translated by Chen L H. Leichtbau-Konstruktion [M]. Beijing: Mechanical Industry Press, 2010: 198
|
| [2] |
(Klein B著, 陈力禾, 译. 轻量化设计: 计算基础与构件结构 [M]. 北京: 机械工业出版社, 2010: 198)
|
| [3] |
Liu W X. Automotive Axle Design [M]. Beijing: Tsinghua University Press, 2004: 330
|
| [3] |
(刘惟信. 汽车车桥设计 [M]. 北京: 清华大学出版社, 2004: 330)
|
| [4] |
Wang X. The method study based on the structure intensity analysis of the truck's drive axle [D]. Chongqing: Chongqing Jiaotong University, 2008
|
| [4] |
(王 星. 货车驱动桥壳结构强度分析方法研究 [D]. 重庆: 重庆交通大学, 2008)
|
| [5] |
Chen J R. Automobile Structure (Part 2) [M]. 3rd Ed., Beijing: Mechanical Industry Press, 2009: 154
|
| [5] |
(陈家瑞. 汽车构造(下册) [M]. 第3版,北京: 机械工业出版社, 2009: 154)
|
| [6] |
Cheng L J, Zhao G Q, Zhao X H, et al. FEM simulation of forging process for the design of a rear axle bracket [J]. J. Plast. Eng., 2008, 15(1): 14
|
| [6] |
(程联军, 赵国群, 赵新海等. 有限元模拟在后轴支架锻造设计中的应用 [J]. 塑性工程学报, 2008, 15(1): 14)
|
| [7] |
Wu S Q, Shi Z Y. Identification of vehicle axle loads based on FEM-Wavelet-Galerkin method [J]. J. Vib. Eng., 2006, 19: 494
|
| [7] |
(吴邵庆, 史治宇. 由有限元-Wavelet-Galerkin法识别桥面移动载荷 [J]. 振动工程学报, 2006, 19: 494)
|
| [8] |
Li Y X, Lin Z Q, Jiang A Q, et al. Use of high strength steel sheet for lightweight and crashworthy car body [J]. Mater. Des., 2003, 24: 177
doi: 10.1016/S0261-3069(03)00021-9
|
| [9] |
Li X L, Ouyang K J, Zhang Y, et al. Development and research of steel used in axle housing for 3-ton light-duty truck [J]. Automob. Sci. Technol., 2000, (3): 25
|
| [9] |
(李性林, 欧阳可居, 张 宇等. 三吨轻型车桥壳用钢的开发与应用研究 [J]. 汽车科技, 2000, (3): 25)
|
| [10] |
Chu Y Z, Qi P, Di L H. Development of hot-rolled drawn axle-housing steel [J]. J. Univ. Sci. Technol., 1999, 21: 342
|
| [10] |
(初元璋, 祁 鹏, 狄丽华. 热轧冲压桥壳用钢板的研制开发 [J]. 北京科技大学学报, 1999, 21: 342)
|
| [11] |
Liu D S, Song D, Wang G D, et al. Development of microalloyed automotive steel strip [J]. Iron Steel, 2000, 35(2): 41
|
| [11] |
(刘东升, 宋 丹, 王国栋等. 汽车桥壳用热连轧微合金高强钢板的研究 [J]. 钢铁, 2000, 35(2): 41)
|
| [12] |
Wu J H, Ye X Y, Huang X J, et al. Research on hot-rolled and high-strength steel of 490 MPa automobile axle housings [J]. Sci. Technol. Liuzhou Steel, 2009, (suppl.): 57
|
| [12] |
(吴菊环, 叶晓喻, 黄徐晶等. 490 MPa级汽车桥壳用热轧高强钢板研制 [J]. 柳钢科技, 2009, (增刊): 57)
|
| [13] |
Wang S S, Cao K C, Hao X Q, et al. Process research on DQK415 steel plate for automobile axle housings [J]. Wide Heavy Plate, 2010, 16(6): 19
|
| [13] |
(王绍松, 曹开宸, 郝小强等. 汽车桥壳用DQK415钢板的工艺研究 [J]. 宽厚板, 2010, 16(6): 19)
|
| [14] |
Huang H H, Yao J Y, Liu R J, et al. Damage detection of axle housing based on metal magnetic memory testing technology [J]. J. Electron. Meas. Instrum., 2014, 28: 770
|
| [14] |
(黄海鸿, 姚结艳, 刘儒军等. 基于金属磁记忆技术的车桥桥壳损伤检测 [J]. 电子测量与仪器学报, 2014, 28: 770)
|
| [15] |
Topac M M, Günal H, Kuralay N S. Fatigue failure prediction of a rear axle housing prototype by using finite element analysis [J]. Eng. Fail. Anal., 2009, 16: 1474
doi: 10.1016/j.engfailanal.2008.09.016
|
| [16] |
Fujiwara K, Okaguchi S, Ohtani H. Effect of hot deformation on bainite structure in low carbon steels [J]. ISIJ Int., 1995, 35: 1006.
doi: 10.2355/isijinternational.35.1006
|
| [17] |
Yong Q L. Secondary Phases in Steels [M]. Beijing: Metallurgical Industry Press, 2006: 175
|
| [17] |
(雍岐龙. 钢铁材料中的第二相 [M]. 北京: 冶金工业出版社, 2006: 175)
|
| [18] |
Duan H, Shan Y Y, Yang K, et al. Experimental on process, microstructure and mechanical properties of X80 high strength pipeline steel for low temperature [J]. Iron Steel, 2020, 55(2): 103
|
| [18] |
(段 贺, 单以银, 杨 柯等. X80低温用高强度管线钢的工艺与组织性能试验 [J]. 钢铁, 2020, 55(2): 103)
|
| [19] |
Hui Y J, Wu K M, Xu K H, et al. Development of 500 MPa grade high ductility square tube steel and its work hardening behavior [J]. Iron Steel, 2020, 55(2): 131
|
| [19] |
(惠亚军, 吴科敏, 许克好等. 500 MPa级高延性方管用钢的开发及加工硬化行为 [J]. 钢铁, 2020, 55(2): 131)
|
| [20] |
Hui Y J, Pan H, Zhou N, et al. Study on strengthening mechanism of 650 MPa grade V-N microalloyed automobile beam steel [J]. Acta Metall. Sin., 2015, 51: 1481
doi: 10.11900/0412.1961.2015.00082
|
| [20] |
(惠亚军, 潘 辉, 周 娜等. 650 MPa级V-N微合金化汽车大梁钢强化机制研究 [J]. 金属学报, 2015, 51: 1481)
doi: 10.11900/0412.1961.2015.00082
|
| [21] |
Yong Q L, Ma M T, Wu B R. Microalloyed Steel—Physical and Mechanical Metallurgy [M]. Beijing: China Machine Press, 1989: 57
|
| [21] |
(雍岐龙, 马鸣图, 吴宝榕. 微合金钢——物理和力学冶金 [M]. 北京: 机械工业出版社, 1989: 57)
|
| [22] |
Zhang P C, Wu H B, Tang D, et al. Dissolving behaviors of carbonitrides in Nb-V-Ti and V-Ti microalloying steels [J]. Acta Metall. Sin., 2007, 43: 753
|
| [22] |
(张鹏程, 武会宾, 唐 荻等. Nb-V-Ti和V-Ti微合金钢中碳氮化物的回溶行为 [J]. 金属学报, 2007, 43: 753)
|
| [23] |
Wang P W, Zhao X H, Du C Z, et al. Analysis of high temperature mechanical properties of vanadium microalloyed steel [J]. Steel Rolling, 2020, 37(1): 45
|
| [23] |
(王培文, 赵新华, 杜传治等. 钒微合金钢的高温力学性能分析 [J]. 轧钢, 2020, 37(1): 45)
|
| [24] |
Chen Z Y, Chen Z G, Qin X Y. Influence of cooling speed on microstructure of Nb-V microalloyed high strength steel [J]. Iron Steel Vanadium Titanium, 2010, 31(3): 59
|
| [24] |
(陈振业, 陈子刚, 秦秀英. 冷却速度对Nb-V微合金化高强度钢显微组织的影响 [J]. 钢铁钒钛, 2010, 31(3): 59)
|
| [25] |
Gao F, Qian T C, Wang R Z. Phase transformation characteristics of vanadium microalloying low carbon bainitic steel in continuous cooling process [J]. J. Iron Steel Res., 2011, 23(12): 40
|
| [25] |
(高 飞, 钱天才, 王瑞珍. 钒微合金化低碳贝氏体钢的连续冷却相变特性 [J]. 钢铁研究学报, 2011, 23(12): 40)
|
| [26] |
Brownrigg A, Prior G K. Hardenability reduction in VN microalloyed eutectoid steels [J]. Scr. Mater., 2002, 46: 357
doi: 10.1016/S1359-6462(01)01251-9
|
| [27] |
Liu H H, Fu P X, Liu H W, et al. Effect of vanadium micro-alloying on the microstructure evolution and mechanical properties of 718H pre-hardened mold steel [J]. J. Mater. Sci. Technol., 2019, 35: 2526
doi: 10.1016/j.jmst.2019.04.033
|
| [28] |
Gwon H, Kim J K, Shin S, et al. The effect of vanadium micro-alloying on the microstructure and the tensile behavior of TWIP steel [J]. Mater. Sci. Eng., 2017, A696: 416
|
| [29] |
Li Y, Milbourn D, Baker T. Effect of vanadium microalloying on the HAZ microstructure and properties of low carbon steels [J]. J. Iron Steel Res. Int., 2011, 18(suppl.): 393
|
| [30] |
Ishikawa F, Takahashi T, Ochi T. Intragranular ferrite nucleation in medium-carbon vanadium steels [J]. Metall. Mater. Trans., 1994, 25A: 929
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|