Please wait a minute...
金属学报  2020, Vol. 56 Issue (5): 723-735    DOI: 10.11900/0412.1961.2019.00292
  本期目录 | 过刊浏览 |
Mg-5.6Gd-0.8Zn合金多向锻造过程中的变形机制及动态再结晶
张阳, 邵建波, 陈韬, 刘楚明, 陈志永()
中南大学材料科学与工程学院 长沙 410083
Deformation Mechanism and Dynamic Recrystallization of Mg-5.6Gd-0.8Zn Alloy During Multi-Directional Forging
ZHANG Yang, SHAO Jianbo, CHEN Tao, LIU Chuming, CHEN Zhiyong()
School of Materials Science and Engineering, Central South University, Changsha 410083, China
引用本文:

张阳, 邵建波, 陈韬, 刘楚明, 陈志永. Mg-5.6Gd-0.8Zn合金多向锻造过程中的变形机制及动态再结晶[J]. 金属学报, 2020, 56(5): 723-735.
Yang ZHANG, Jianbo SHAO, Tao CHEN, Chuming LIU, Zhiyong CHEN. Deformation Mechanism and Dynamic Recrystallization of Mg-5.6Gd-0.8Zn Alloy During Multi-Directional Forging[J]. Acta Metall Sin, 2020, 56(5): 723-735.

全文: PDF(5277 KB)   HTML
摘要: 

以含长周期堆垛有序(LPSO)相的Mg-5.6Gd-0.8Zn (质量分数,%)合金为研究对象,分析了合金多向锻造过程中的变形机制、动态再结晶及显微组织演变。结果表明:变形初期,{101ˉ2}拉伸孪生仅在部分晶粒中激发;随锻造方向的改变,不同晶体取向的晶粒能够激发孪生变形,孪生体积分数增加,孪生变体选择符合Schmid定律。孪生受阻碍的晶粒通过滑移及扭折协调变形,扭折带类型主要为转轴分布在<101ˉ0>晶向的基面扭折。多向锻造过程中,晶界处优先发生动态再结晶;随着变形量的增加,晶界处再结晶体积分数增大,晶内孪晶与扭折界面诱发再结晶,孪晶逐渐演变为条带状细晶组织。在孪晶、扭折带切割晶粒,晶界再结晶,孪晶、扭折带诱发再结晶多重机制的共同作用下,原始粗晶组织得到了显著细化。

关键词 : 镁合金,  LPSO相,  多向锻造,  变形机制,  动态再结晶    
Abstract:

Multi-directional forging (MDF) is an effective way to fabricate wrought magnesium alloy with ultrafine grains and random texture. Therefore, microstructure evolution and dynamic recrystallization (DRX) of magnesium alloys during MDF process have been widely investigated. Mg-Zn-RE alloys containing long-period stacking ordered (LPSO) phase have received considerable attention owing to their excellent mechanical properties. In addition, LPSO phase has great effects on the deformation mechanism and DRX behavior. Still, limited comprehensive studies can be found in the literature dealing with the microstructure evolution, deformation mechanism and DRX of magnesium alloys containing LPSO phase in MDF deformation. In this work, MDF was applied to a Mg-5.6Gd-0.8Zn (mass fraction, %) alloy containing LPSO phase. Microstructure characteristics, deformation mechanism and DRX behavior of the material in different passes were examined. Results show that there are several stages of the microstructure evolution. Twinning was activated only in a small part of grains in the early stage of deformation. As the forging direction changes, the number of twinned grains and the volume fraction of DRX grains increased. A mixed structure with coarse deformed grain and DRX grains was sustained till last forging pass, and the average size of DRX grains is about 4 μm with a random orientation. {101ˉ2} tensile twinning is the main deformation mechanism and the selection of twin variants was dominated by the Schmid law. Change in forging direction is beneficial to twinning stimulation in grains of different orientations. Kink and slipping deformation could effectively accommodate the plastic strain where the operation of twinning was hindered. Kink deformation resulted in lattice rotation predominately about the <101ˉ0> axis. DRX grains nucleated at different places during the forging process. Not only the grain boundaries and the twinned region, but also kink boundaries can induce the nucleation of DRX grains. Eventually, the twinned regions were transformed to a strip-like recrystallization structure. Under the combined influence of twinning and kinking, as well as DRX induced by twins, kink bands and grain boundaries, the initial coarse grains were significantly refined.

Key words: magnesium alloy    LPSO phase    multi-directional forging    deformation mechanism    dynamic recrystallization
收稿日期: 2019-09-05     
ZTFLH:  TG146.2  
基金资助:国家自然科学基金项目(51874367);国家自然科学基金项目(51574291)
作者简介: 张 阳,女,1995年生,硕士
图1  多向锻造流程及微观组织观测取样位置示意图
图2  铸态、均匀化态及退火态Mg-5.6Gd-0.8Zn合金的SEM像
图3  退火态合金长周期堆垛结构(LPSO)相的STEM像
图4  退火态合金锻后各道次显微组织的OM像
图5  多向锻造过程中孪生及扭折诱发再结晶
图6  合金锻后各道次样品SEM像
图7  多向锻造过程中的动态再结晶行为示意图
图8  合金锻后各道次取向成像图
图9  合金1道次锻造后孪生及未孪生晶粒取向成像图、{0001}极图及孪生与基面滑移Schmid因子分析
图10  合金2道次锻造后同一晶粒内的孪生及扭折现象分析
图11  合金3道次锻造后孪生晶粒取向成像图、极图及孪生变体Schmid因子分析
1 Ding W J. Magnesium Alloy Science and Technology [M]. Beijing: Science Press, 2007: 24
1 丁文江. 镁合金科学与技术 [M]. 北京: 科学出版社, 2007: 24
2 Dahle A K, Lee Y C, Nave M D, et al. Development of the as-cast microstructure in magnesium-aluminum alloys [J]. J. Light Met., 2001, 1: 61
3 Zhang J H, Leng Z, Liu S J, et al. Microstructure and mechanical properties of Mg-Gd-Dy-Zn alloy with long period stacking ordered structure or stacking faults [J]. J. Alloys Compd., 2011, 509: 7717
4 Polmear I J. Magnesium alloys and applications [J]. Mater. Sci. Technol., 1994, 10: 1
5 Zeng R C, Ke W, Xu Y B, et al. Recent development and application of magnesium alloys [J]. Acta Metall. Sin., 2001, 37: 673
5 曾荣昌, 柯 伟, 徐永波等. Mg合金的最新发展及应用前景 [J]. 金属学报, 2001, 37: 673
6 Miura H, Maruoka T, Yang X, et al. Microstructure and mechanical properties of multi-directionally forged Mg-Al-Zn alloy [J]. Scr. Mater., 2012, 66: 49
7 Kawamura Y, Hayashi K, Inoue A, et al. Rapidly solidified powder metallurgy Mg97Zn1Y2 alloys with excellent tensile yield strength above 600 MPa [J]. Mater. Trans., 2001, 42: 1172
8 Li Y X, Zhu G Z, Qiu D, et al. The intrinsic effect of long period stacking ordered phases on mechanical properties in Mg-RE based alloys [J]. J. Alloys Compd., 2016, 660: 252
9 Zhu J, Chen J B, Liu T, et al. High strength Mg94Zn2.4Y3.6 alloy with long period stacking ordered structure prepared by near-rapid solidification technology [J]. Mater. Sci. Eng., 2017, A679: 476
10 Shao J B, Chen Z Y, Chen T, et al. Texture evolution, deformation mechanism and mechanical properties of the hot rolled Mg-Gd-Y-Zn-Zr alloy containing LPSO phase [J]. Mater. Sci. Eng., 2018, A731: 479
11 Xie G M, Ma Z Y, Xue P, et al. Effects of tool rotation rates on superplastic deformation behavior of friction stir processed Mg-Zn-Y-Zr alloy [J]. Acta Metall. Sin., 2018, 54: 1745
11 谢广明, 马宗义, 薛 鹏等. 工具转速对搅拌摩擦加工Mg-Zn-Y-Zr耐热镁合金超塑性行为的影响 [J]. 金属学报, 2018, 54: 1745
12 Li K, Chen Z Y, Chen T, et al. Hot deformation and dynamic recrystallization behaviors of Mg-Gd-Zn alloy with LPSO phases [J]. J. Alloys Compd., 2019, 792: 894
doi: 10.1016/j.jallcom.2019.04.036
13 Matsuda M, Ando S, Nishida M, et al. Dislocation structure in rapidly solidified Mg97Zn1Y2 alloy with long period stacking order phase [J]. Mater. Trans., 2005, 46: 361
14 Matsuda M, Ii S, Kawamura Y, et al. Interaction between long period stacking order phase and deformation twin in rapidly solidified Mg97Zn1Y2 alloy [J]. Mater. Sci. Eng., 2004, A386: 447
15 Yamasaki M, Hagihara K, Inoue S I, et al. Crystallographic classification of kink bands in an extruded Mg-Zn-Y alloy using intragranular misorientation axis analysis [J]. Acta Mater., 2013, 61: 2065
16 Shao X H, Yang Z Q, Ma X L. Strengthening and toughening mechanisms in Mg-Zn-Y alloy with a long period stacking ordered structure [J]. Acta Mater., 2010, 58: 4760
17 Zhou X J, Liu C M, Gao Y H, et al. Evolution of LPSO phases and their effect on dynamic recrystallization in a Mg-Gd-Y-Zn-Zr alloy [J]. Metall. Mater. Trans., 2017, 48A: 3060
doi: 10.3390/ma11112092 pmid: 30366432
18 Zhang D X, Tan Z, Huo Q H, et al. Dynamic recrystallization behaviors of Mg-Gd-Y-Zn-Zr alloy with different morphologies and distributions of LPSO phases [J]. Mater. Sci. Eng., 2018, A715: 389
19 Miura H, Yu G, Yang X. Multi-directional forging of AZ61Mg alloy under decreasing temperature conditions and improvement of its mechanical properties[J]. Mater. Sci. Eng., 2011, A528: 6981
20 Wang B Z, Liu C M, Gao Y H, et al. Microstructure evolution and mechanical properties of Mg-Gd-Y-Ag-Zr alloy fabricated by multidirectional forging and ageing treatment [J]. Mater. Sci. Eng., 2017, A702: 22
21 Wu Y Z, Yan H G, Chen J H, et al. Microstructure and mechanical properties of ZK21 magnesium alloy fabricated by multiple forging at different strain rates [J]. Mater. Sci. Eng., 2012, A556: 164
22 Mehrabi A, Mahmudi R, Miura H. Superplasticity in a multi-directionally forged Mg-Li-Zn alloy [J]. Mater. Sci. Eng., 2019, A765: 138274
23 Deng L P, Cui K X, Wang B S, et al. Microstructure and texture evolution of AZ31 Mg alloy processed by multi-pass compressing under room temperature [J]. Acta Metall. Sin., 2019, 55: 976
23 邓丽萍, 崔凯旋, 汪炳叔等. AZ31镁合金室温多道次压缩过程微观组织和织构演变的研究 [J]. 金属学报, 2019, 55: 976
24 Matsuda M, Ii S, Kawamura Y, et al. Variation of long-period stacking order structures in rapidly solidified Mg97Zn1Y2 alloy [J]. Mater. Sci. Eng., 2005, A393: 269
25 Yamasaki M, Sasaki M, Nishijima M, et al. Formation of 14H long period stacking ordered structure and profuse stacking faults in Mg-Zn-Gd alloys during isothermal aging at high temperature [J]. Acta Mater., 2007, 55: 6798
doi: 10.1016/j.actamat.2007.08.033
26 Xiao H C, Jiang S N, Tang B, et al. Hot deformation and dynamic recrystallization behaviors of Mg-Gd-Y-Zr alloy [J]. Mater. Sci. Eng., 2015, A628: 311
27 Guan D K, Rainforth W M, Ma L, et al. Twin recrystallization mechanisms and exceptional contribution to texture evolution during annealing in a magnesium alloy [J]. Acta Mater., 2017, 126: 132
28 Liu W, Zhang J S, Wei L Y, et al. Extensive dynamic recrystallized grains at kink boundary of 14H LPSO phase in extruded Mg92Gd3Zn1Li4 alloy [J]. Mater. Sci. Eng., 2017, A681: 97
29 Wu J, Ikeda K I, Shi Q, et al. Kink boundaries and their role in dynamic recrystallisation of a Mg-Zn-Y alloy [J]. Mater. Charact., 2019, 148: 233
30 Yu Y N. Metallurgical Principle [M]. 2nd Ed., Beijing: Metallurgical Industry Press, 2013: 931
30 余永宁. 金属学原理 [M]. 第2版. 北京: 冶金工业出版社, 2013: 931
31 Chapuis A, Xin Y C, Zhou X J, et al. {101¯2} twin variants selection mechanisms during twinning, re-twinning and detwinning [J]. Mater. Sci. Eng., 2014 ,A612: 431
32 Stanford N, Barnett M R. Effect of particles on the formation of deformation twins in a magnesium-based alloy [J]. Mater. Sci. Eng., 2009, A516: 226
33 Hong S G, Park S H, Lee C S. Role of {101¯2} twinning characteristics in the deformation behavior of a polycrystalline magnesium alloy [J]. Acta Mater., 2010, 58: 5873
34 Guo C F, Xin R L, Zheng X, et al. Influence of observation plane on twin variant identification in magnesium via trace and misorientation analysis [J]. Mater. Sci. Eng., 2014, A618: 558
35 Barnett M R. A Taylor model based description of the proof stress of magnesium AZ31 during hot working [J]. Metall. Mater. Trans., 2003, 34A: 1799
36 Chun Y B, Davies C H J. Investigation of prism <a> slip in warm-rolled AZ31 alloy [J]. Metall. Mater. Trans., 2011, 42A: 4113
37 Wang L, Sabisch J, Lilleodden E T. Kink formation and concomitant twin nucleation in Mg-Y [J]. Scr. Mater., 2016, 111: 68
[1] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] 张海峰, 闫海乐, 方烽, 贾楠. FeMnCoCrNi高熵合金双晶微柱变形机制的分子动力学模拟[J]. 金属学报, 2023, 59(8): 1051-1064.
[3] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[4] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[5] 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌. 初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响[J]. 金属学报, 2023, 59(7): 855-870.
[6] 邵晓宏, 彭珍珍, 靳千千, 马秀良. 镁合金LPSO/SFs结构间{101¯2}孪晶交汇机制的原子尺度研究[J]. 金属学报, 2023, 59(4): 556-566.
[7] 沈朝, 王志鹏, 胡波, 李德江, 曾小勤, 丁文江. 镁合金抗高温氧化机理研究进展[J]. 金属学报, 2023, 59(3): 371-386.
[8] 唐伟能, 莫宁, 侯娟. 增材制造镁合金技术现状与研究进展[J]. 金属学报, 2023, 59(2): 205-225.
[9] 朱云鹏, 覃嘉宇, 王金辉, 马鸿斌, 金培鹏, 李培杰. 机械球磨结合粉末冶金制备AZ61超细晶镁合金的组织与性能[J]. 金属学报, 2023, 59(2): 257-266.
[10] 娄峰, 刘轲, 刘金学, 董含武, 李淑波, 杜文博. 轧制态Mg-xZn-0.5Er合金板材组织及室温成形性能[J]. 金属学报, 2023, 59(11): 1439-1447.
[11] 彭立明, 邓庆琛, 吴玉娟, 付彭怀, 刘子翼, 武千业, 陈凯, 丁文江. 镁合金选区激光熔化增材制造技术研究现状与展望[J]. 金属学报, 2023, 59(1): 31-54.
[12] 吴彩虹, 冯迪, 臧千昊, 范诗春, 张豪, 李胤樹. 喷射成形AlSiCuMg合金的热变形组织演变及再结晶行为[J]. 金属学报, 2022, 58(7): 932-942.
[13] 陈扬, 毛萍莉, 刘正, 王志, 曹耕晟. 高速冲击载荷下预压缩AZ31镁合金的退孪生行为与动态力学性能[J]. 金属学报, 2022, 58(5): 660-672.
[14] 曾小勤, 王杰, 应韬, 丁文江. 镁及其合金导热研究进展[J]. 金属学报, 2022, 58(4): 400-411.
[15] 任少飞, 张健杨, 张新房, 孙明月, 徐斌, 崔传勇. 新型Ni-Co基高温合金塑性变形连接中界面组织演化及愈合机制[J]. 金属学报, 2022, 58(2): 129-140.