| 部分再结晶退火对无取向硅钢的磁性能与力学性能的影响 |
于雷,罗海文( ) |
| 北京科技大学冶金与生态工程学院 北京 100083 |
|
| Effect of Partial Recrystallization Annealing on Magnetic Properties and Mechanical Properties of Non-Oriented Silicon Steel |
YU Lei,LUO Haiwen( ) |
| School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
于雷,罗海文. 部分再结晶退火对无取向硅钢的磁性能与力学性能的影响[J]. 金属学报, 2020, 56(3): 291-300.
Lei YU,
Haiwen LUO.
Effect of Partial Recrystallization Annealing on Magnetic Properties and Mechanical Properties of Non-Oriented Silicon Steel[J]. Acta Metall Sin, 2020, 56(3): 291-300.
| [1] | Sha Y H, Sun C, Zhang F, et al. Strong cube recrystallization texture in silicon steel by twin-roll casting process [J]. Acta Mater., 2014, 76: 106 | | [2] | Zhang N, Yang P, Mao W M. Through process texture evolution of new thin-gauge non-oriented electrical steels with high permeability [J]. J. Magn. Magn. Mater., 2016, 397: 125 | | [3] | Gong J, Luo H W. Progress on the research of high-strength non-oriented silicon steel sheets in traction motors of hybrid/electrical vehicles [J]. J. Mater. Eng., 2015, 43(6): 102 | | [3] | 龚 坚, 罗海文. 新能源汽车驱动电机用高强度无取向硅钢片的研究与进展 [J]. 材料工程, 2015, 43(6): 102 | | [4] | Pan Z D, Xiang L, Zhang C, et al. Development of high-strength non-oriented electrical steel by TSCR [J]. Iron Steel Van. Tit., 2013, 34(4): 78 | | [4] | 潘振东, 项 利, 张 晨等. TSCR 试制高强度无取向电工钢 [J]. 钢铁钒钛, 2013, 34(4): 78 | | [5] | Wang Y Q, Zhang X M, He Z, et al. Effect of copper precipitates on mechanical and magnetic properties of Cu-bearing non-oriented electrical steel processed by twin-roll strip casting [J]. Mater. Sci. Eng., 2017, A703: 340 | | [6] | Lu Y K, Zu G Q, Luo L, et al. Investigation of microstructure and properties of strip-cast 4.5 wt% Si non-oriented electrical steel by different rolling processes [J]. J. Magn. Magn. Mater., 2019, 497: 165975 | | [7] | Tanaka I, Yashiki H, Iwamoto S, et al. Development of high strength electrical steel SXRC of resource-saving design [J]. J. Iron Steel Res. Int., 2011, 6: 15 | | [8] | Liu B, Song X L, Zhu R Q, et al. Effect of niobium on goss texture evolution of low temperature orientation silicon steel [J]. Trans. Mater. Heat Treat., 2017, 38(11): 71 | | [8] | 刘 彪, 宋新莉, 朱瑞琪等. Nb对低温取向硅钢高斯织构演变的影响 [J]. 材料热处理学报, 2017, 38(11): 71 | | [9] | Huang J, Luo H W. Influence of annealing process on microstructures, mechanical and magnetic properties of Nb-containing high-strength non-oriented silicon steel [J]. Acta Metall. Sin., 2018, 54: 377 | | [9] | 黄 俊, 罗海文. 退火工艺对含Nb高强无取向硅钢组织及性能的影响 [J]. 金属学报, 2018, 54: 377 | | [10] | Honda A, Senda K, Sadahiro K. Electrical steel for motors of electric and hybrid vehicles [J]. Kawasaki Steel Tech. Rep., 2002, 34: 85 | | [11] | Goldschmidt H J. The constitution of the iron-niobium-silicon system [J]. J. Iron Steel Inst., 1960, 194: 169 | | [12] | Raghavan V, Ghosh G. The Fe-Nb-Si (iron-niobium-silicon) system [J]. Trans. Indian Inst. Met., 1984, 37: 421 | | [13] | Raghavan V. Phase Diagrams of Ternary Iron Alloys [M]. Metals Park, Ohio: ASM International, 1987: 226 | | [14] | Singh B N, Gupta K P. Laves and μ phases in the Nb-Fe-Si and Nb-Co-Si systems [J]. Metall. Trans., 1972, 3: 1427 | | [15] | Wang D, Yang S Y, Yang M J, et al. Experimental investigation of phase equilibria in the Fe-Nb-Si ternary system [J]. J. Alloys Compd., 2014, 605: 183 | | [16] | Muraki M, Toge T, Sakata K, et al. Formation mechanism of {111} recrystallization texture in ferritic steels [J]. Tetsu Hagané, 1999, 85: 751 | | [16] | 村木 峰男, 峠 哲雄, 坂田 敬, 待って. フェライト鋼の{111}再結晶集合組織生成機構の-考察. 鉄と鋼, 1999, 85: 751 | | [17] | Park J T, Szpunar J A. Evolution of recrystallization texture in nonoriented electrical steels [J]. Acta Mater., 2003, 51: 3037 | | [18] | Hutchinson W B. Development of textures in recrystallization [J]. Met. Sci., 1974, 8: 185 | | [19] | Park J T, Szpunar J A. Texture development during grain growth in nonoriented electrical steels [J]. ISIJ Int., 2005, 45: 743 | | [20] | Jenkins K, Lindenmo M. Precipitates in electrical steels [J]. J. Magn. Magn. Mater., 2008, 320: 2423 | | [21] | Li M, Xiao Y D, Wang W, et al. Effect of annealing parameter on microstructure and magnetic properties of cold rolled non-oriented electrical steel [J]. Trans. Nonferrous Met. Soc. China, 2007, 17: 74 | | [22] | Zhao Y H, Zhu G H, Wang L T, et al. Effect of annealing temperature on properties of thin specification non-oriented electric steel [J]. Metall. Funct. Mater., 2012, 19(2): 22 | | [22] | 赵亚慧, 朱国辉, 王立涛等. 退火温度对CSP生产薄规格无取向电工钢性能的影响 [J]. 金属功能材料, 2012, 19(2): 22 | | [23] | Yang F, Xiong C G, Xiang L, et al. Effect of annealing time on microstructure of non-oriented electrical steel 50W600 [J]. Hot Work. Technol., 2015, 44: 208 | | [23] | 杨 帆, 熊晨光, 项 利等. 退火时间对无取向电工钢50W600组织的影响 [J]. 热加工工艺, 2015, 44: 208 | | [24] | Zhang N, Yang P, Mao W N. {001}<120>-{113}<361> recrystallization textures induced by initial {001} grains and related microstructure evolution in heavily rolled electrical steel [J]. Mater. Charact., 2016, 119: 225 | | [25] | Sidor J J, Verbeken K, Gomes E, et al. Through process texture evolution and magnetic properties of high Si non-oriented electrical steels [J]. Mater. Charact., 2012, 71: 49 | | [26] | Zu G Q, Zhang X M, Zhao J W, et al. Analysis of {411}<148> recrystallisation texture in twin-roll strip casting of 4.5 wt% Si non-oriented electrical steel [J]. Mater. Lett., 2016, 180: 63 | | [27] | He B B, Hu B, Yen H W, et al. High dislocation density-induced large ductility in deformed and partitioned steels [J]. Science, 2017, 357: 1029 | | [28] | Ungár T, Gubicza J, Ribárik G, et al. Crystallite size distribution and dislocation structure determined by diffraction profile analysis: principles and practical application to cubic and hexagonal crystals [J]. J. Appl. Crystallogr., 2001, 34: 298 | | [29] | Shintani T, Murata Y. Evaluation of the dislocation density and dislocation character in cold rolled type 304 steel determined by profile analysis of X-ray diffraction [J]. Acta Mater., 2011, 59: 4314 | | [30] | Ungár T, Tichy G. The effect of dislocation contrast on X-ray line profiles in untextured polycrystals [J]. Phys. Status Sol., 1999, 171A: 425 | | [31] | Yin F, Hanamura T, Umezawa O, et al. Phosphorus-induced dislocation structure variation in the warm-rolled ultrafine-grained low-carbon steels [J]. Mater. Sci. Eng., 2003, A354: 31 | | [32] | Ungár T, Borbély A. The effect of dislocation contrast on X-ray line broadening: A new approach to line profile analysis [J]. Appl. Phys. Lett., 1996, 69: 3173 | | [33] | Kunieda T, Nakai M, Murata Y, et al. Estimation of the system free energy of martensite phase in an Fe-Cr-C ternary alloy [J]. ISIJ Int., 2005, 45: 1909 | | [34] | Gladman T. The Physical Metallurgy of Microalloyed Steels [M]. London: Maney Pub, 1997: 40 | | [35] | Pickering F B. Physical Metallurgy and the Design of Steels [M]. London: Applied Science Publishers, 1978: 63 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |