| Sn对TiAl基合金烧结致密化与力学性能的影响 |
潘宇, 路新( ), 刘程程, 孙健卓, 佟健博, 徐伟, 曲选辉 |
| 北京科技大学新材料技术研究院 北京 100083 |
|
| Effect of Sn Addition on Densification and Mechanical Properties of Sintered TiAl Base Alloys |
Yu PAN, Xin LU( ), Chengcheng LIU, Jianzhuo SUN, Jianbo TONG, Wei XU, Xuanhui QU |
| Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
潘宇, 路新, 刘程程, 孙健卓, 佟健博, 徐伟, 曲选辉. Sn对TiAl基合金烧结致密化与力学性能的影响[J]. 金属学报, 2018, 54(1): 93-99.
Yu PAN,
Xin LU,
Chengcheng LIU,
Jianzhuo SUN,
Jianbo TONG,
Wei XU,
Xuanhui QU.
Effect of Sn Addition on Densification and Mechanical Properties of Sintered TiAl Base Alloys[J]. Acta Metall Sin, 2018, 54(1): 93-99.
| [1] | Song L, Lin J P, Li J S.Phase transformation mechanisms in a quenched Ti-45Al-8.5Nb-0.2W-0.2B-0.02Y alloy after subsequent annealing at 800 ℃[J]. J. Alloys Compd., 2017, 691: 60 | | [2] | San J J, Simas P, Schmoelzer T, et al.Atomic relaxation processes in an intermetallic Ti-43Al-4Nb-1Mo-0.1B alloy studied by mechanical spectroscopy[J]. Acta Mater., 2014, 65: 338 | | [3] | Park S Y, Seo D Y, Kim S W, et al.High temperature oxidation of Ti-46Al-6Nb-0.5W-0.5Cr-0.3Si-0.1C alloy[J]. Intermetallics, 2016, 74: 8 | | [4] | Lin J P, Zhao L L, Li G Y, et al.Effect of Nb on oxidation behavior of high Nb containing TiAl alloys[J]. Intermetallics, 2011, 19: 131 | | [5] | Bean G E, Kesler M S, Manuel M V.Effect of Nb on phase transformations and microstructure in high Nb titanium aluminides[J]. J. Alloys Compd., 2014, 613: 351 | | [6] | Chen G, Peng Y B, Zheng G, et al.Polysynthetic twinned TiAl single crystals for high-temperature applications[J]. Nat. Mater., 2016, 15: 876 | | [7] | Li H Z, Qi Y L, Liang X P, et al.Microstructure and high temperature mechanical properties of powder metallurgical Ti-45Al-7Nb-0.3W alloy sheets[J]. Mater. Des., 2016, 106: 90 | | [8] | Li J B, Liu Y, Liu B, et al.Microstructure characterization and mechanical behaviors of a hot forged high Nb containing PM-TiAl alloy[J]. Mater. Charact., 2014, 95: 148 | | [9] | Liu Q, Nash P.The effect of Ruthenium addition on the microstructure and mechanical properties of TiAl alloys[J]. Intermetallic, 2011, 19: 1282 | | [10] | Monchoux J P, Luo J S, Voisin T, et al.Deformation modes and size effect in near-γ TiAl alloys[J]. Mater. Sci. Eng., 2017, A679: 123 | | [11] | Liu H W, Bishop D P, Plucknett K P.Densification behaviour and microstructural evolution of Ti-48Al consolidated by spark plasma sintering[J]. J. Mater. Sci., 2017, 52: 613 | | [12] | Yang R.Advances and challenges of TiAl base alloys[J]. Acta Metall. Sin., 2015, 51: 129(杨锐. 钛铝金属间化合物的进展与挑战[J]. 金属学报, 2015, 51: 129) | | [13] | Han Y, Fan J L, Liu T, et al.The effect of trace nickel additive and ball milling treatment on the near-full densification behavior of ultrafine tungsten powder[J]. Int. J. Refract. Met. Hard Mater., 2012, 34: 8 | | [14] | Wang Y H, Lin J P, He Y H, et al.Densification behavior of high Nb containing TiAl alloys through reactive hot pressing[J]. J. Univ. Sci. Technol. Beijing, 2007, 14: 251 | | [15] | Hibino A, Kiuchi M.Pressureless combustion synthesis of dense TiAl intermetallic compounds by Ni/Al powder addition[J]. Mater. Trans., JIM, 1999, 40: 92 | | [16] | Liu Y, Wei W F, Huang B Y, et al.Qualitative and quantitative theory of enhanced sintering in powder metallurgy[J]. Mater. Rev., 2003, 17(3): 1(刘咏, 韦伟峰, 黄伯云等. 粉末冶金强化烧结的定性与定量分析理论综述[J]. 材料导报, 2003, 17(3): 1) | | [17] | Qiu W T, Pang Y, Xiao Z, et al.Preparation of W-Cu alloy with high density and ultrafine grains by mechanical alloying and high pressure sintering[J]. Int. J. Refract. Met. Hard Mater., 2016, 61: 91 | | [18] | Pan K M, Zhang L Q, Wei S Z, et al.Study on the preparation process of T2 alloy in the Mo-Si-B system[J]. Acta Metall. Sin., 2015, 51: 1377(潘昆明, 张来启, 魏世忠等. Mo-Si-B三元系中T2相合金的制备工艺研究[J]. 金属学报, 2015, 51: 1377) | | [19] | Zhu Q S, Fan B A.Low temperature sintering of 8YSZ electrolyte film for intermediate temperature solid oxide fuel cells[J]. Solid State Ionics, 2005, 176: 889 | | [20] | Zhou H M, Li M L, Guo Y J, et al.Effect of MnO2 on sintering ability and properties of 8YSZ[J]. J. Cent. South Univ.(Sci. Technol.), 2012, 43: 1254(周宏明, 李淼磊, 郭雁军等. MnO2对8YSZ低温活化烧结及其性能的影响[J]. 中南大学学报(自然科学版), 2012, 43: 1254) | | [21] | Xia Y, Luo S D, Wu X, et al.The sintering densification, microstructure and mechanical properties of gamma Ti-48Al-2Cr-2Nb alloy with a small addition of copper[J]. Mater. Sci. Eng., 2013, A559: 293 | | [22] | Xia Y, Schaffer G B, Qian M.The effect of a small addition of nickel on the sintering, sintered microstructure, and mechanical properties of Ti-45Al-5Nb-0.2C-0.2B alloy[J]. J. Alloys Compd., 2013, 578: 195 | | [23] | Xia Y, Yu P, Schaffer G B, et al.Cobalt-doped Ti-48Al-2Cr-2Nb alloy fabricated by cold compaction and pressureless sintering[J]. Mater. Sci. Eng., 2013, A574: 176 | | [24] | Soyama J, Oehring M, Limberg W, et al.The effect of zirconium addition on sintering behaviour, microstructure and creep resistance of the powder metallurgy processed alloy Ti-45Al-5Nb-0.2B-0.2C[J]. Mater. Des., 2015, 84: 87 | | [25] | He Y H, Qu X H, Huang B Y, et al.The effect of Sn addition on the TiAl based alloy[J]. J. Central South Univ.(Sci. Technol.), 1993, 24: 788(贺跃辉, 曲选辉, 黄伯云等. 锡的添加对TiAl基合金的影响[J]. 中南大学学报(自然科学版), 1993, 24: 788) | | [26] | Shida Y, Anada H.The influence of ternary element addition on the oxidation behaviour of TiAl intermetallic compound in high temperature air[J]. Corros. Sci., 1993, 35: 945 | | [27] | Wang D N, Inui H, Lin D L, et al.Effects of Sn additions on the microstructures and tensile properties of two-phase TiAl alloys[J]. Intermetallics, 1996, 4: 191 | | [28] | Zhao J C.Effect of alloying on the microstructure and mechanical properties of Ti-48Al-2Cr-2Nb alloys [D]. Changsha: Xiangtan University, 2015(赵俊才. 合金化对Ti-48Al-2Cr-2Nb合金显微组织和力学性能的影响 [D]. 长沙: 湘潭大学, 2015) | | [29] | Lu X, He X B, Zhang B, et al.Microstructure and mechanical properties of a spark plasma sintered Ti-45Al-8.5Nb-0.2W-0.2B-0.1Y alloy[J]. Intermetallics, 2009, 17: 840 |
|
|