| 预氧化处理对G115钢高温蒸气氧化行为的影响 |
白银1,2, 刘正东1( ), 谢建新2, 包汉生1, 陈正宗1 |
| 1 钢铁研究总院 北京 1000812 北京科技大学材料科学与工程学院 北京 100083 |
|
| Effect of Pre-Oxidation Treatment on the Behavior of High Temperature Oxidation in Steam of G115 Steel |
Yin BAI1,2, Zhengdong LIU1( ), Jianxin XIE2, Hansheng BAO1, Zhengzong CHEN1 |
1 Central Iron and Steel Research Institute, Beijing 100081, China 2 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
白银, 刘正东, 谢建新, 包汉生, 陈正宗. 预氧化处理对G115钢高温蒸气氧化行为的影响[J]. 金属学报, 2018, 54(6): 895-904.
Yin BAI,
Zhengdong LIU,
Jianxin XIE,
Hansheng BAO,
Zhengzong CHEN.
Effect of Pre-Oxidation Treatment on the Behavior of High Temperature Oxidation in Steam of G115 Steel[J]. Acta Metall Sin, 2018, 54(6): 895-904.
| [1] | Blum R, Vanstone R W.Materials development for boilers and steam turbines operating at 700 ℃ [A]. Proceedings of the 6th International Charles Parsons Materials Conference[C]. Dublin, Ireland: Trinity College Dublin, 2003: 498 | | [2] | Tschaffon H.The European way to 700 ℃ coal fired power plant [A]. Proceedings of the 8th Liege Conference on Materials for Advanced Power Engineering 2006[C]. Liege, Belgium: Energy Technology Forschungszentrum Julich, 2006: 61 | | [3] | Metzger H K, Maile K, Klenk A, et al.Investigations on nickel based alloys and welds for A-USC applications [A]. Proceedings of the 7th International Conference on Advances in Materials Technology for Fossil Power Plants[C]. Waikoloa, Hawaii, USA: ASM International, 2013: 6 | | [4] | Di Gianfrancesco A, Tizzanini A, Jedamzik M, et al.ENCIO project: An European approach to 700 ℃ power plant [A]. Proceedings of the 7th International Conference on Advances in Materials Technology for Fossil Power Plants[C]. Waikoloa, Hawaii, USA: ASM International, 2013: 19 | | [5] | Viswanathan R, Henry J F, Tanzosh J, et al.U.S. program on materials technology for USC power plants [A]. Proceeding of the 4th International Conference on Advances in Materials Technology for Fossil Power Plants[C]. Hilton Head Island, South Carolina, USA: ASM International, 2005: 3 | | [6] | Shingledecker J, Purgert R, Rawls P.Current status of the U.S. DOE/OCDO A-USC materials technology research and development program [A]. Proceedings of the 7th International Conference on Advances in Materials Technology for Fossil Power Plants[C]. Waikoloa, Hawaii, USA: ASM International, 2013: 41 | | [7] | Fukuda M, Saito E, Semba H, et al.Advanced USC technology development in Japan [A]. Proceedings of the 7th International Conference on Advances in Materials Technology for Fossil Power Plants[C]. Waikoloa, Hawaii, USA: ASM International, 2013: 24 | | [8] | Sun R, Cui Z Z, Tao Y.Progress of China 700 ℃ USC development program [A]. Proceedings of the 7th International Conference on Advances in Materials Technology for Fossil Power Plants[C]. Waikoloa, Hawaii, USA: ASM International, 2013: 1 | | [9] | Mathur A, Bhutani O P, Jayakumar T, et al.India's national A-USC mission-plan and progress [A]. Proceedings of the 7th International Conference on Advances in Materials Technology for Fossil Power Plants[C]. Waikoloa, Hawaii, USA: ASM International, 2013: 53 | | [10] | Yan P, Liu Z D, Bao H S, et al.Effect of tempering temperature on the toughness of 9Cr-3W-3Co martensitic heat resistant steel[J]. Mater. Des., 2014, 54: 874 | | [11] | Yan P, Liu Z D, Bao H S, et al.Effect of microstructural evolution on high-temperature strength of 9Cr-3W-3Co martensitic heat resistant steel under different aging conditions[J]. Mater. Sci. Eng., 2013, A588: 22 | | [12] | Yan P, Liu Z D, Bao H S, et al.Effect of normalizing temperature on the strength of 9Cr-3W-3Co martensitic heat resistant steel[J]. Mater. Sci. Eng., 2014, A597: 148 | | [13] | Tan L, Yang Y, Allen T R.Oxidation behavior of iron-based alloy HCM12A exposed in supercritical water[J]. Corros. Sci., 2006, 48: 3123 | | [14] | Zhang N Q, Zhu Z L, Xu H, et al.Oxidation of ferritic and ferritic-martensitic steels in flowing and static supercritical water[J]. Corros. Sci., 2016, 103: 124 | | [15] | Bischoff J, Motta A T, Eichfeld C, et al.Corrosion of ferritic-martensitic steels in steam and supercritical water[J]. J. Nucl. Mater., 2013, 441: 604 | | [16] | Yin K J, Qiu S Y, Tang R, et al.Corrosion behavior of ferritic/martensitic steel P92 in supercritical water[J]. J. Supercrit. Fluid., 2009, 50: 235 | | [17] | Viswanathan R, Sarver J, Tanzosh J M.Boiler materials for ultra-supercritical coal power plants—Steamside oxidation[J] J. Mater. Eng. Perform., 2006, 15: 255 | | [18] | Oksa M, Tuurna S, Mets?joki J, et al.Oxidation performance coating for future supercritical power plants[J]. J. Nucl. Eng. Radiat. Sci., 2016, 2: 011018 | | [19] | Agüero A, González V, Mayr P, et al.Anomalous steam oxidation behavior of a creep resistant martensitic 9 wt. % Cr steel[J]. Mater. Chem. Phys., 2013, 141: 432 | | [20] | Agüero A, González V, Gutiérrez M, et al.Oxidation under pure steam: Cr based protective oxides and coatings[J]. Surf. Coat. Technol., 2013, 237: 30 | | [21] | ?urek J, De Bruycker E, Huysmans S, et al.Steam oxidation of 9% to 12%Cr steels: Critical evaluation and implications for practical application[J]. Corrosion, 2014, 70: 112 | | [22] | Yu X L, Jiang Z Y, Zhao J W, et al.Effect of a grain-refined microalloyed steel substrate on the formation mechanism of a tight oxide scale[J]. Corros. Sci., 2014, 85: 115 | | [23] | Gao R, Xia L L, Zhang T, et al.Oxidation resistance in LBE and air and tensile properties of ODS ferritic steels containing Al/Zr elements[J]. J. Nucl. Mater., 2014, 455: 407 | | [24] | Jacob Y,Haanappel V A C,Stroosnijder M F, et al.The effect of gas composition on the isothermal oxidation behaviour of PM chromium[J]. Corros. Sci., 2002, 44: 2027 | | [25] | Jonsson T, Pujilaksono B, Heidari H, et al.Oxidation of Fe-10Cr in O2 and in O2 + H2O environment at 600 ℃: A microstructural investigation[J]. Corros. Sci., 2013, 75: 326 | | [26] | Meier G H, Jung K, Mu N, et al.Effect of alloy composition and exposure conditions on the selective oxidation behavior of ferritic Fe-Cr and Fe-Cr-X alloys[J]. Oxid. Met., 2010, 74: 319 | | [27] | Abe F, Kutsumi H, Haruyama H, et al.Improvement of oxidation resistance of 9 mass% chromium steel for advanced-ultra supercritical power plant boilers by pre-oxidation treatment[J]. Corros. Sci., 2017, 114: 1 | | [28] | Zhou R C, Tang L Y, Wang H Z, et al. High temperature steam oxidation test device [P]. Chin Pat, CN101118211, 2008(周荣灿, 唐丽英, 王弘喆等. 高温蒸汽氧化试验装置 [P]. 中国专利, CN101118211, 2008) | | [29] | ?urek J, Michalik M, Schmitz F, et al.The effect of water-vapor content and gas flow rate on the oxidation mechanism of a 10%Cr-ferritic steel in Ar-H2O mixtures[J]. Oxid. Met., 2005, 63: 401 | | [30] | Schütze M, Renusch D, Schorr M.Chemical-mechanical failure of oxide scales on 9% Cr steels in air with H2O[J]. Mater. High Temp., 2005, 22: 113 | | [31] | Holcomb G H.Steam oxidation and chromia evaporation in ultra-supercritical steam boilers and turbines[J]. J. Electrochem. Soc., 2009, 156: C292 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|