奥氏体不锈钢表面改性层耐蚀性实验研究:Ⅱ.3aCl溶液中E-pH图 |
雷明凯 朱雪梅 |
大连理工大学材料工程系;大连 116024 |
|
引用本文:
雷明凯; 朱雪梅 . 奥氏体不锈钢表面改性层耐蚀性实验研究:Ⅱ.3aCl溶液中E-pH图[J]. 金属学报, 1999, 35(10): 1085-1089 .
[1] Let M K, Zhang Z L.J Vac Set Technol, 1995; 13A: 2986 [2] Let M K, Huang Y, Li Y H, Zhang Z L. Tribology,1997; 17: 206 (雷明凯,黄岩,李有宏,张仲麟.摩擦学学报,1997;17:206) [3] Let M K, Zhu X M, Yuan L J, Zhang Z L. Acta Metall sin, 1999; 35(10):1081 (雷明凯,朱雪梅,袁力江,张仲麟,金属学报,1999;35(10): 1081) [4] Chabica M E Williamson D L, Wei R Wilbur P J. Surf Coat Technol, 1992; 51: 24 [5] Menthe E, Rie K-T, Schulze J W, Simson S Surf Coat Tech- nol, 1995; 74/75: 412 [6] Yasumaru N, Tsuchida K, San E, Ibe T.Mater Trans JIM,1993; 34:696 [7] Verink Jr E D, Pourbaix M. Corrosion, 1971; 27: 495 [8] Yang W, Ni R-C, Hua H-Z. Corros Sci, 1984; 24: 691 [9] Bell T, sun y.In Zhu R Z ed,Procedings of International Conference on Surface Science and Engineering, Beijing;In- ternational Academic Publishers, 1995: 9 [10] Chyou S D; Shih H C, Corrosion, 1991;47: 31 [11] Zhang Z L, Bell T. Surf Eng, 1985; 1: 131 [12] Ramchandani A, Dennis J K. Heat Treat Met; 1988; 2: 34 [13] Lei M K, Zhu X M, Zhang Z L. J Mater Sci Lett, 1999; 18:211 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|