| Na2CrO4-NaHCO3-H2O体系的相平衡和溶液物化性质 |
| 崔金兰 张懿 |
| 中国科学院化工冶金研究所; 北京 100080 |
|
引用本文:
崔金兰; 张懿 . Na2CrO4-NaHCO3-H2O体系的相平衡和溶液物化性质[J]. 金属学报, 1999, 35(10): 1062-1064 .
[1]Cheng S W,Ding Y,Yang C R.Chromate Production Pro- ess Beijing:Chemical Industry Press,1987:4 (成思危,丁翼,杨春荣,铬盐生产工艺.北京:化学工业出版 社,1987:4) [2] Zhang Y, Li Z H Wang Z K, Chen J Y Prog Chem, 1998 10:172 (张懿,李佐虎,王志宽,陈家镛,化学进展,1998;10:172) [3] Institute of Qinghai Salt-Lake, The Chinese Academy of Sci-ences. Analgstical Methods of Brines and Salts, Beijing: Science Press, 1988: 215 (中国科学院青海盐湖研究所分析室,卤水和盐的分析方法,北京: 科学出版社,1988:215) [4]Dai S G. Instrument Analyses, Beijing:Higher Education Press, 1987:43 (戴树桂 仪器分析、北京:高等教育出版社,1987:43) [5] 1959; 36: 16 [6] Fang C H.J Salt Lake Sci, 1990; 2: 15 (房春晖, 盐湖研究,1990;2; 2:15) |
|