| 超超临界电站用镍基合金热加工过程的再结晶机理 |
韦康, 张麦仓( ), 谢锡善 |
| 北京科技大学材料科学与工程学院 北京 100083 |
|
| Recrystallization Mechanisms in Hot Working Processes of a Nickel-Based Alloy for Ultra-Supercritical Power Plant Application |
Kang WEI, Maicang ZHANG( ), Xishan XIE |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
韦康, 张麦仓, 谢锡善. 超超临界电站用镍基合金热加工过程的再结晶机理[J]. 金属学报, 2017, 53(12): 1611-1619.
Kang WEI,
Maicang ZHANG,
Xishan XIE.
Recrystallization Mechanisms in Hot Working Processes of a Nickel-Based Alloy for Ultra-Supercritical Power Plant Application[J]. Acta Metall Sin, 2017, 53(12): 1611-1619.
| [1] | Guo J T.Materials Science and Engineering for Superalloys [M]. Vol.1, Beijing: Science Press, 2008: 1(郭建亭. 高温合金材料学 [M]. 上册, 北京: 科学出版社, 2008: 1) | | [2] | Doherty R D, Hughes D A, Humphreys F J, et al.Current issues in recrystallization: A review[J]. Mater. Sci. Eng., 1997, A238: 219 | | [3] | Humphreys F J, Hatherly M.Recrystallization and Related Annealing Phenomena[M]. 2nd Ed., Amsterdam: Elsevier, 2004: 169 | | [4] | Zahiri S H, Hodgson P D.The static, dynamic and metadynamic recrystallisation of a medium carbon steel[J]. Mater. Sci. Technol., 2004, 20: 458 | | [5] | Sakai T, Belyakov A, Kaibyshev R, et al.Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions[J]. Prog. Mater. Sci., 2014, 60: 130 | | [6] | Singh R P, Hyzak J M, Howson T E, et al.Recrystallization behavior of cold rolled alloy 718 [A]. Superalloys 718, 625 and Various Derivatives[C]. Warrendale, PA: TMS, 1991: 205 | | [7] | Wang L, Wang S A, Liu Y, et al. Dynamic recrystallization behavior of GH4586 superalloy during hot compression [J]. Mater. Sci. Forum, 2010, 638-642: 2357 | | [8] | Liu Y X, Lin Y, Li H B, et al.Study of dynamic recrystallization in a Ni-based superalloy by experiments and cellular automaton model[J]. Mater. Sci. Eng., 2015, A626: 432 | | [9] | Lin Y C, Liu Y X, Chen M S, et al.Study of static recrystallization behavior in hot deformed Ni-based superalloy using cellular automaton model[J]. Mater. Des., 2016, 99: 107 | | [10] | Hirth J P, Pond R C.Steps, dislocations and disconnections as interface defects relating to structure and phase transformations[J]. Acta. Mater., 1996, 44: 4749 | | [11] | Smith W F, Hashemi J.Foundations of Materials Science and Engineering[M]. 5th Ed., New York: McGraw-Hill Education, 2011: 138 | | [12] | Shirdel M, Mirzadeh H, Parsa M H.Abnormal grain growth in AISI 304L stainless steel[J]. Mater. Charact., 2014, 97: 11 | | [13] | Danflou H L, Macia M, Sanders T H, et al.Mechanisms of formation of serrated grain boundaries in nickel base superalloys [A]. Superalloys 1996[C]. Warrendale, PA: TMS, 1996: 119 | | [14] | Kim K J, Ginsztler J, Nam S W.The role of carbon on the occurrence of grain boundary serration in an AISI 316 stainless steel during aging heat treatment[J]. Mater. Lett., 2005, 59: 1439 | | [15] | Kim K J, Hong H U, Nam S W.A study on the mechanism of serrated grain boundary formation in an austenitic stainless steel[J]. Mater. Chem. Phys., 2011, 126: 480 | | [16] | Hong H U, Kim I S, Choi B G, et al.On the mechanism of serrated grain boundary formation in Ni-based superalloys with low γ′ volume fraction [A]. Superalloys 2012[C]. Warrendale, PA: TMS, 2012: 53 | | [17] | Hong H U, Jeong H W, Kim I S, et al.Significant decrease in interfacial energy of grain boundary through serrated grain boundary transition[J]. Philo. Mag., 2012, 92: 2809 | | [18] | Jiang L, Hu R, Kou H C, et al.The effect of M23C6 carbides on the formation of grain boundary serrations in a wrought Ni-based superalloy[J]. Mater. Sci. Eng., 2012, A536: 37 | | [19] | Lim Y S, Kim D J, Hwang S S, et al.M23C6 precipitation behavior and grain boundary serration in Ni-based alloy 690[J]. Mater. Charact., 2014, 96: 28 | | [20] | Wu Y S, Zhang M C, Xie X S.The design and research of a new low cobalt-molybdenum niobium-containing Ni-base superalloy for 700 ℃ advanced ultra-supercritical power plants[J]. Proc. Eng., 2015, 130: 617 | | [21] | Xie X S, Wu Y S, Chi C Y, et al.Superalloys for advanced ultra-super-critical fossil power plant application [A]. Superalloys[M]. Rijeka: InTech, 2015: 51 | | [22] | Li D F, Guo Q M, Guo S L, et al.The microstructure evolution and nucleation mechanisms of dynamic recrystallization in hot-deformed Inconel 625 superalloy[J]. Mater. Des., 2011, 32: 696 | | [23] | Cao Y, Di H S, Zhang J Q, et al.An electron backscattered diffraction study on the dynamic recrystallization behavior of a nickel-chromium alloy (800H) during hot deformation[J]. Mater. Sci. Eng., 2013, A585: 71 | | [24] | Gleiter H.The mechanism of grain boundary migration[J]. Acta Metall., 1969, 17: 565 | | [25] | Gleiter H.Theory of grain boundary migration rate[J]. Acta Metall., 1969, 17: 853 | | [26] | Rae C M F, Smith D A. On the mechanisms of grain boundary migration[J]. Philos. Mag., 1980, 41A: 477 | | [27] | Rajabzadeh A, Legros M, Combe N, et al.Evidence of grain boundary dislocation step motion associated to shear-coupled grain boundary migration[J]. Philos. Mag., 2013, 93: 1299 | | [28] | Bowers M L, Ophus C, Gautam A, et al.Step coalescence by collective motion at an incommensurate grain boundary[J]. Phys. Rev. Lett., 2016, 116: 106102 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|