| 加工条件对多相V-Ti-Ni合金的显微组织和氢渗透性能的影响 |
江鹏1( ),袁同心1,于彦东2 |
1 常州大学机械工程学院 常州 213164 2 哈尔滨理工大学材料科学与工程学院 哈尔滨 150040 |
|
| Effect of Processing Conditions on Microstructure and Property of Multiphase V-Ti-Ni Alloys for Hydrogen Purifying |
Peng JIANG1( ),Tongxin YUAN1,Yandong YU2 |
1 School of Mechanical Engineering, Changzhou University, Changzhou 213164, China 2 School of Materials Science and Engineering,Harbin University of Science and Technology, Harbin 150040, China |
引用本文:
江鹏,袁同心,于彦东. 加工条件对多相V-Ti-Ni合金的显微组织和氢渗透性能的影响[J]. 金属学报, 2017, 53(4): 433-439.
Peng JIANG,
Tongxin YUAN,
Yandong YU.
Effect of Processing Conditions on Microstructure and Property of Multiphase V-Ti-Ni Alloys for Hydrogen Purifying[J]. Acta Metall Sin, 2017, 53(4): 433-439.
| [1] | Lubitz W, Tumas W.Hydrogen: An overview[J]. Chem. Rev., 2007, 107: 3900 | | [2] | Adhikari S, Fernando S.Hydrogen membrane separation techniques[J]. Ind. Eng. Chem. Res., 2006, 45: 875 | | [3] | Ward T L, Dao T.Model of hydrogen permeation behavior in palladium membranes[J]. J. Membr. Sci., 1999, 153: 211 | | [4] | Taxak M, Kumar S, Sheelvantra S, et al.Effect of iron on the solubility of hydrogen in tantalum[J]. J. Mater. Sci., 2014, 49: 8471 | | [5] | Xiong L Y, Liu S, Wang L B, et al.Microstructures and hydrogen permeation characteristics of Nb-Ti-Ni alloys[J]. Acta Metall. Sin., 2008, 44: 781 | | [5] | (熊良银, 刘实, 王隆保等. Nb-Ti-Ni合金的显微组织与氢渗透性能[J]. 金属学报, 2008, 44: 781) | | [6] | Oh J Y, Ko W S, Suh J Y, et al.Enhanced high temperature hydrogen permeation characteristics of V-Ni alloy membranes containing a trace amount of yttrium[J]. Scr. Mater., 2016, 116: 122 | | [7] | Buxbaum R E, Kinney A B.Hydrogen transport through tubular membranes of palladium-coated tantalum and niobium[J]. Ind. Eng. Chem. Res., 1996, 35: 530 | | [8] | Alimov V N, Busnyuk A O, Notkin M E, et al.Hydrogen transport through V-Pd alloy membranes: Hydrogen solution, permeation and diffusion[J]. J. Membr. Sci., 2015, 481: 54 | | [9] | Suzuki A, Yukawa H, Ijiri S, et al.Alloying effects on hydrogen solubility and hydrogen permeability for V-based alloy membranes[J]. Mater. Trans., 2015, 56: 1688 | | [10] | Suzuki A, Yukawa H, Nambu T, et al.Analysis of pressure-composition-isotherms for design of non-Pd-based alloy membranes with high hydrogen permeability and strong resistance to hydrogen embrittlement[J]. J. Membr. Sci., 2016, 503: 110 | | [11] | Nishimura C, Komaki M, Hwang S, et al. V-Ni alloy membranes for hydrogen purification [J]. J. Alloys Compd., 2002, 330-332: 902 | | [12] | Yang J Y, Nishimura C, Komaki M. Effect of H2S on hydrogen permeation of Pd60Cu40/V-15Ni composite membrane [J]. J. Alloys Compd., 2007, 446-447: 575 | | [13] | Zhang Y, Ozaki T, Komaki M, et al.Hydrogen permeation of Pd-Ag alloy coated V-15Ni composite membrane: Effects of overlayer composition[J]. J. Membr. Sci., 2003, 224: 81 | | [14] | Nishimura C, Ozaki T, Komaki M, et al. Hydrogen permeation and transmission electron microscope observations of V-Al alloys [J]. J. Alloys Compd., 2003, 356-357: 295 | | [15] | Paglieri S N, Wermer J R, Buxbaum R E, et al.Development of membranes for hydrogen separation: Pd coated V-10Pd[J]. Energy Mater., 2008, 3(3): 169 | | [16] | Zhang Y, Ozaki T, Komaki M, et al.Hydrogen permeation characteristics of vanadium-aluminium alloys[J]. Scr. Mater., 2002, 47: 601 | | [17] | Roark S E, MacKay R, Mundschau M V. Dense, layered membranes for hydrogen separation [P].US Pat., 7001446, 2006 | | [18] | Kim K H, Shim J H, Lee B J.Effect of alloying elements (Al, Co, Fe, Ni) on the solubility of hydrogen in vanadium: A thermodynamic calculation[J]. Int. J. Hydrogen Energy, 2012, 37: 7836 | | [19] | Adams T M, Mickalonis J.Hydrogen permeability of multiphase V-Ti-Ni metallic membranes[J]. Mater. Lett., 2007, 61: 817 | | [20] | Hashi K, Ishikawa K, Matsuda T, et al. Hydrogen permeation characteristics of (V, Ta)-Ti-Ni alloys [J]. J. Alloys Compd., 2005, 404-406: 273 | | [21] | Jeon S I, Magnone E, Park J H, et al.The effect of temperature and pressure on the hydrogen permeation through Pd-coated Ti26Ni21V53 alloy membrane under different atmospheres[J]. Mater. Lett., 2011, 65: 2495 | | [22] | Hashi K, Ishikawa K, Matsuda T, et al.Hydrogen permeation characteristics of multi-phase Ni-Ti-Nb alloys[J]. J. Alloys Compd., 2004, 368: 215 | | [23] | Magnone E, Jeon S I, Park J H, et al.Relationship between microstructure and hydrogen permeation properties in the multiphase Ni21Ti23Nb56 alloy membranes[J]. J. Membr. Sci., 2011, 384: 136 | | [24] | Ishikawa K, Tokui S, Aoki K.Microstructure and hydrogen permeation of cold rolled and annealed Nb40Ti30Ni30 alloy[J]. Intermetallics, 2009, 17: 109 | | [25] | Luo W, Ishikawa K, Aoki K.Hydrogen permeable Ta-Ti-Ni duplex phase alloys with high resistance to hydrogen embrittlement[J]. J. Alloys Compd., 2008, 460: 353 | | [26] | Hashi K, Ishikawa K, Matsuda T, et al.Microstructure and hydrogen permeability in Nb-Ti-Co multiphase alloys[J]. J. Alloys Compd., 2006, 425: 284 | | [27] | Li X Z, Liu D M, Liang X, et al.Hydrogen transport behavior of as-cast, cold rolled and annealed Nb40Ti30Co30 alloy membranes[J]. J. Membr. Sci., 2016, 514: 294 | | [28] | Ishikawa K, Takano T, Matsuda T, et al.High hydrogen permeability in the Nb-Zr-Ni eutectic alloy containing the primary body-centered-cubic (Nb, Zr) phase[J]. Appl. Phys. Lett., 2005, 87: 081906 | | [29] | Jiang P, Yu Y D.Effect of heat treatment process on microstructure and hardness of V55Ti30Ni15 alloy for hydrogen permeation[J]. Acta Metall. Sin., 2013, 49: 1105 | | [29] | (江鹏, 于彦东. 热处理工艺对透氢V55Ti30Ni15合金的显微组织和硬度的影响[J]. 金属学报, 2013, 49: 1105) | | [30] | Dolan M D.Non-Pd BCC alloy membranes for industrial hydrogen separation[J]. J. Membr. Sci., 2010, 362: 12 | | [31] | Fleury E, Suh J Y, Kim D I, et al.Hydrogen permeation characteristics of rolled V85Al10Co5 alloys[J]. Curr. Appl. Phys., 2012, 12: 1131 | | [32] | Williamson G K, Smallman R E.III. Dislocation densities in some annealed and cold-worked metals from measurements on the X-ray debye-scherrer spectrum[J]. Philos. Mag., 1956, 1: 34 | | [33] | Revay L.X-ray line broadening in electrodeposited gold coatings[J]. Electrodepo. Surf. Treat., 1975, 3: 139 | | [34] | Dolan M D, McLennan K G, Way J D. Diffusion of atomic hydrogen through V-Ni alloy membranes under nondilute conditions[J]. J. Phys. Chem., 2012, 116C: 1512 | | [35] | Nishimura C, Komaki M, Amano M.Hydrogen permeation characteristics of vanadium-nickel alloys[J]. Mater. Trans., 1991, 32: 501 | | [36] | Connor H.Palladium alloy diffusion cells[J]. Platin. Met. Rev., 1962, 6: 130 | | [37] | Kurkela M, Latanision R M.The effect of plastic deformation on the transport of hydrogen in nickel[J]. Scr. Metall., 1979, 13: 927 | | [38] | Hirth J P.Effects of hydrogen on the properties of iron and steel[J]. Metall. Mater. Trans., 1980, 11A: 861 | | [39] | Kumnick A J, Johnson H H.Deep trapping states for hydrogen in deformed iron[J]. Acta Metall., 1980, 28: 33 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|