| 7050铝合金淬火敏感性研究和微观组织分析* |
吴书舟1,易幼平1,黄始全1( ),李俊1,李晨2 |
1 中南大学机电工程学院高性能复杂制造国家重点实验室, 长沙 410083 2 中航工业第一飞机设计研究院, 西安 710089 |
|
| RESERCH ON QUENCH SENSITIVITY AND MICROSTRUCTURE ANALYSIS OF 7050 ALUMINUM ALLOY |
Shuzhou WU1,Youping YI1,Shiquan HUANG1( ),Jun LI1,Chen LI2 |
1 State Key Laboratory of High Performance Complex Manufacturing, School of Mechanical and Electrical Engineering, Central South University, Changsha 410083, China 2 The First Aircraft Institute of AVIC, Xi'an 710089, China |
引用本文:
吴书舟,易幼平,黄始全,李俊,李晨. 7050铝合金淬火敏感性研究和微观组织分析*[J]. 金属学报, 2016, 52(12): 1503-1509.
Shuzhou WU,
Youping YI,
Shiquan HUANG,
Jun LI,
Chen LI.
RESERCH ON QUENCH SENSITIVITY AND MICROSTRUCTURE ANALYSIS OF 7050 ALUMINUM ALLOY[J]. Acta Metall Sin, 2016, 52(12): 1503-1509.
| [1] | Wang Z T, Tian R Z.Aluminum Alloy and Processing Handbook. Changsha: Central South University of Technology Press, 1989: 34 | | [1] | (王祝堂, 田荣璋. 铝合金及其加工手册. 长沙: 中南工业大学出版社, 1989: 34) | | [2] | Zhang X M, Deng Y L, Zhang Y.Acta Metall Sin, 2015; 51: 268 | | [2] | (张新明, 邓运来, 张勇. 金属学报, 2015; 51: 268) | | [3] | Li C G, Wu S J, Dai S L.Trans Nonferrous Met Soc China, 2002; 12: 15 | | [3] | (李成功, 巫世杰, 戴圣龙. 中国有色金属学报, 2002; 12: 15) | | [4] | Sampson D S, translated by Hong R X. Album of Deformation Aluminum Alloy in Modern Times. Beijing: Metallurgy Industry Press, 1987: 97 | | [4] | (Sampson D S 著, 洪仁先译. 国外近代变形铝合金专集. 北京: 冶金工业出版社, 1987: 97) | | [5] | Liu Y Z, Li Z L, Gu C X.Acta Metall Sin, 2013; 49: 1598 | | [5] | (刘允中, 李志龙, 顾才鑫. 金属学报, 2013; 49: 1598) | | [6] | Dumont D, Deschamps A, Brechet Y.Acta Mater, 2004; 52: 2529 | | [7] | Deschamps A, Brechet Y.Scr Mater, 1998; 39: 1517 | | [8] | Thomson D S, Subramanya B S, Levy S A.Metall Trans, 1971; 2: 1149 | | [9] | Conserva M, Russo E D, Caloni O.Metall Trans, 1971; 2: 1227 | | [10] | Gong H, Wu Y X, Liao K.J Mater Eng, 2010; (1): 42 | | [10] | (龚海, 吴运新, 廖凯. 材料工程, 2010; (1): 42) | | [11] | Davydov V G, Ber L B, Ananiev V N.In: Fridlyander I N ed., Proc 5th Int Conf on Aluminum Alloys, Amsterdam: Kluwer Academic Publishers-Plenum Publishers, 1996: 859 | | [12] | Alekseev A A, Ber L B.Light Alloys Technol, 1993; 5: 18 | | [13] | Archambault P, Godard D.Scr Mater, 2000; 42: 675 | | [14] | Li S L, Huang Z Q, Chen W P, Liu Z M, Qi W J.Trans Mater Heat Treat, 2013; 34(4): 57 | | [14] | (李慎兰, 黄志其, 陈维平, 刘志铭, 戚文军. 材料热处理学报, 2013; 34(4): 57) | | [15] | Wang G, Yin Z M, Zhao K, Duan J Q, Liu B, Shang B C.Mater Sci Technol, 2011; 19(4): 84 | | [15] | (王岗, 尹志民, 赵凯, 段佳琦, 刘博, 商宝川. 材料科学与工艺, 2011; 19(4): 84) | | [16] | Robinson J S, Cudd R L, Tanner D A.J Mater Process Technol, 2001; 119: 261 | | [17] | Chen L, Yu Y N.Phase Transformations in Metals and Alloys. Beijing: Higher Education Press, 2011: 233 | | [17] | (陈冷, 余永宁. 金属和合金中的相变. 北京: 高等教育出版社, 2011: 233) | | [18] | Staley J T.Mater Sci Technol, 1987; 3: 923 | | [19] | Christian J W.The Theory of Transformations in Metals and Alloys. Oxford: Pergamon Press, 1975: 58 | | [20] | Liu S D, Zhang X M, You J H, Huang Z B, Zhang C, Zhang X Y.Trans Nonferrous Met Soc China, 2006; 12: 2034 | | [20] | (刘胜胆, 张新明, 游江海, 黄振宝, 张翀, 张小艳. 中国有色金属学报, 2006; 12: 2034) | | [21] | Li P Y, Xiong B Q, Zhang Y A, Li Z H, Zhu B H, Wang F, Liu H W.Trans Nonferrous Met Soc China, 2011; 21: 513 | | [21] | (李培跃, 熊柏青, 张永安, 李志辉, 朱宝宏, 王锋, 刘红伟. 中国有色金属学报, 2011; 21: 513) | | [22] | Liu W J.PhD Dissertation, Central South University, Changsha, 2011 | | [22] | (刘文军. 中南大学博士学位论文, 长沙, 2011) | | [23] | Chen H.Master Thesis, Central South University, Changsha, 201 | | [23] | (陈慧. 中南大学硕士学位论文, 长沙, 2012) | | [24] | Dai X Y.PhD Dissertation, Central South University, Changsha, 2008 | | [24] | (戴晓元. 中南大学博士学位论文, 长沙, 2008) | | [25] | Godard D, Archambault P, Aeby-Gautier E. Acta Mater, 2002; 50: 2319 | | [26] | Tang J G, Chen H, Zhang X M, Liu S D, Liu W J, Ouyang H, Li H P.Trans Nonferrous Met Soc China, 2012; 22: 1255 | | [27] | Tian F Q, Cui J Z.Trans Nonferrous Met Soc China, 2006; 16: 958 | | [27] | (田福泉, 崔建忠. 中国有色金属学报, 2006; 16: 958) |
|
|