淬火后预拉伸对自然时效状态Al-Li合金组织和性能的影响* |
张显峰,李国爱( ),陆政,于娟,郝敏 |
北京航空材料研究院北京市先进铝合金材料及应用工程技术研究中心, 北京 100095 |
|
EFFECT OF PREAGED STRETCH AFTER QUENCHED ON THE PROPERTIES AND MICROSTRUCTURE OF A NATURALLY AGED Al-Li ALLOY |
Xianfeng ZHANG,Guoai LI( ),Zheng LU,Juan YU,Min HAO |
Beijing Engineering Research Center of Advanced Aluminum Alloys and Applications, Beijing Institute of Aeronautical Material, Beijing 100095, China |
引用本文:
张显峰,李国爱,陆政,于娟,郝敏. 淬火后预拉伸对自然时效状态Al-Li合金组织和性能的影响*[J]. 金属学报, 2016, 52(12): 1497-1502.
Xianfeng ZHANG,
Guoai LI,
Zheng LU,
Juan YU,
Min HAO.
EFFECT OF PREAGED STRETCH AFTER QUENCHED ON THE PROPERTIES AND MICROSTRUCTURE OF A NATURALLY AGED Al-Li ALLOY[J]. Acta Metall Sin, 2016, 52(12): 1497-1502.
[1] | Meric C.Mater Res Bull, 2000; 35: 1479 | [2] | Rioja R J, Liu J.Metall Mater Trans, 2012; 43A: 3325 | [3] | Tsivoulas D, Prangnell P B.Metall Mater Trans, 2014; 45A: 1338 | [4] | Lequeu P, Smith K P, Daniélou A.J Mater Eng Perform, 2010; 19: 841 | [5] | Acosta E, Garcia O, Dakessian A, Aung Ra K, Torroledo J, Tsang A. Mater Sci Forum#/magtechI#, 2002; 396-402: 1157 | [6] | Lequeu P, Lassince P, Warner T.Adv Mater Processes, 2007; 165(7): 41 | [7] | Lequeu P.Adv Mater Processes, 2008; 166(2): 47 | [8] | Kertz J E, Gouma P I, Buchheit R G.Metall Mater Trans, 2001; 32A: 2561 | [9] | Li H Y, Tang Y, Zeng Z D, Zheng Z Q, Zheng F.Mater Sci Eng, 2008; A498: 314 | [10] | Wang S C, Starink M J.Int Mater Rev, 2005; 50: 193 | [11] | Decreus B, Deschamps A, De Geuser F, Donnadieu P, Sigli C, Weyland M.Acta Mater, 2013; 61: 2207 | [12] | Ovri H, J?gle E A, Stark A, Lilleodden E T.Mater Sci Eng, 2015; A637: 162 | [13] | Thomas D, Frédéric D G, Williams L, Christophe S, Alexis D.Mater Sci Eng, 2014; A605: 119 | [14] | Huang B P, Zheng Z Q.Scr Mater, 1998; 38: 357 | [15] | Cassada W A, Shiflet G J, Jr Starke E A.Metall Mater Trans, 1991; 22A: 299 | [16] | Gable B M, Zhu A W, Csontos A A, Jr Starke E A.J Light Met, 2001; 1: 1 | [17] | Buchheit R G, Moran J P, Stoner G E.Corrosion, 1994; 50: 120 | [18] | Proton V, Alexis J, Andrieu E, Delfosse J, Deschamps A, Geuser F D, Lafont M C, Blanc C.Corros Sci, 2014; 80: 494 | [19] | Decreus B B, Deschamps A, Geuser F D, Sigli C.Adv Eng Mater, 2013; 15: 1082 | [20] | Li H Y, Tang Y, Z Z D, Zheng F.Trans Nonferrous Met Soc China, 2008; 18: 778 | [21] | Noble B, Thompson G E.Met Sci J, 1972; 6: 167 | [22] | Sinyavskii V S, Semenov A M.Prot Met, 2002; 38: 132 | [23] | Feng D. Metal Physics.Vol.1, Beijing: Science Press, 1998: 305 | [23] | (冯端. 金属物理学. 第1卷, 北京: 科学出版社, 1998: 305) | [24] | Kumar K S, Brown S A, Pickens J R.Acta Mater, 1996; 44: 1899 | [25] | Yoshimura R, Konno T J, Abe E, Hiraga K.Acta Mater, 2003; 51: 4251 | [26] | Kumar K S, Brown S A, Pickens J R.Scr Metall Mater, 1990; 24: 1245 | [27] | Gayle F W, Heubaum F H, Pickens J R.Scr Metall Mater, 1990; 24: 79 | [28] | Zhang L, Chen Q Z, Wang Y Y, Yan W D.J Aeronaut Mater, 2007; 27(4): 31 | [28] | (张蕾, 陈群志, 王逾涯, 严卫东. 航空材料学报, 2007; 27(4): 31) | [29] | Liu B X, Li G A.Heat Treat Met, 2004; 29(5): 32 | [29] | (刘北兴, 李国爱. 金属热处理, 2004; 29(5): 32) |
|
|