|
|
|
| 固溶处理对热压CoCrW合金组织及力学性能的影响* |
游晓红1,王刚刚1,王军2,许涛2,张洪宇3,韦华3( ) |
1 太原科技大学材料科学与工程学院, 太原 0300002 2 驻某厂军代表室, 西安 7100773 3 中国科学院金属研究所, 沈阳 110016 |
|
| EFFECT OF SOLID SOLUTION TREATMENT ONMICROSTRUCTURE AND MECHANICALPROPERTIES OF HOT-PRESS CoCrW ALLOYS |
Xiaohong YOU1,Ganggang WANG1,Jun WANG2,Tao XU2,Hongyu ZHANG3,Hua WEI3( ) |
1 School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030000, China 2 Military Representative Office in Factory, Xi'an 710077, China 3 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
游晓红,王刚刚,王军,许涛,张洪宇,韦华. 固溶处理对热压CoCrW合金组织及力学性能的影响*[J]. 金属学报, 2016, 52(2): 161-167.
Xiaohong YOU,
Ganggang WANG,
Jun WANG,
Tao XU,
Hongyu ZHANG,
Hua WEI.
EFFECT OF SOLID SOLUTION TREATMENT ONMICROSTRUCTURE AND MECHANICALPROPERTIES OF HOT-PRESS CoCrW ALLOYS[J]. Acta Metall Sin, 2016, 52(2): 161-167.
| [1] | Kuzucu V, Ceylan M, Celik H, Aksoy I.J Mater Process Technol, 1997; 69: 257 | | [2] | Lemarie E, Calvar M L.Wear, 2001; 249: 338 | | [3] | Otterloo J D, Hosson J D.Acta Mater, 1997; 45: 1225 | | [4] | Ashworth M A, Bryar J C, Jacobs M H, Davies S.Powder Metall, 1999; 42: 243 | | [5] | Ahmed R, Ashraf A, Elameen M, Faisal N F, El-Sherik A M, Elakwah Y O, Goosen M F A.Wear, 2014; 312: 70 | | [6] | Northwood D O.Mater Des, 1985; 6: 58 | | [7] | Frenk A, Kurz W.Wear, 1994; 174: 81 | | [8] | Crook P.Adv Mater Process, 1994; 145: 27 | | [9] | Sims C T, Stoloff N S, Hagel W C. Superalloys II. New York: Wiley, 1987: 140 | | [10] | Fu Z M, Song K J.Chinese Sci Bull, 1987; 5: 390 | | [10] | (傅祖明, 宋科匠. 科学通报, 1987; 5: 390) | | [11] | Yu H, Ahmed R, Lovelock H D.In: Davies S ed., Proc World Congress Eng 2007, Vol II, London: Newswood Limited, 2007: 435 | | [12] | Malayoglu U, Neville A.Wear, 2003; 255: 181 | | [13] | Malayoglu U, Neville A.Wear, 2005; 259: 219 | | [14] | Huang P Y. Powder Metallurgy Principle.2nd Ed., Beijing: Metallurgical Industry Press, 2006: 331 | | [14] | (黄培云. 粉末冶金原理. 第2版, 北京: 冶金工业出版社, 2006: 331) | | [15] | Ahmed R, Lovelock H D, Davies S, Faisal N H.Tribol Int, 2013; 57: 8 | | [16] | Jiang W H, Guan H R, Hu Z Q.Mater Sci Eng, 1999; A271: 101 | | [17] | Larson J M.In: Hausner H H, Smith W E eds., Proc 1973 Int Pow der Metall Conf, Berlin: Springer, 1974: 537 | | [18] | Wallace W, Dunthorne H B, Sprague R A.Can Metall Quart, 1974; 13: 517 | | [19] | Kear K H.In: Hausner H H ed., Proc 1970 Int Powder Metally Conf, Berlin: Springer, 1971: 85 | | [20] | Guo W M, Wu J T, Zhang F G, Zhao M H.J Iron Steel Res Int, 2006; 13(5): 65 | | [21] | Rao G A, Kumar M, Srinivas M, Sarma D S.Mater Sci Eng, 2003; A355: 114 | | [22] | Mao J, Yang W H, Wang W X, Zou J W, Zhou R F.Acta Metall Sin, 1993; 29: 187 | | [22] | (毛健, 杨万宏, 汪武祥, 邹金文, 周瑞发. 金属学报, 1993; 29: 187) | | [23] | Prakash T L, Tewari S N.In: Ramakrishnan P ed., Powder Metall Related High Temperature Materials. Zurich: Trans Tech Publications, 1985: 402 | | [24] | Wu C F, Ma M X, Liu W J, Zhong M L, Zhang W M, Zhang H J.Acta Metall Sin, 2009; 45: 1013 | | [24] | (吴朝锋, 马明星, 刘文今, 钟敏霖, 张伟明, 张红军. 金属学报, 2009; 45: 1013) | | [25] | John R, David F.In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Champion: TMS, 2004: 381 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|