| AZ31镁合金在平面应变压缩过程中的孪生行为研究* |
汪炳叔1( ),邓丽萍1,CHAPUIS Adrien2,郭宁3,李强1 |
1 福州大学材料科学与工程学院, 福州 350108 2 重庆大学材料科学与工程学院, 重庆 400044 3 西南大学材料与能源学部材料工程系, 重庆 400715 |
|
| STUDY OF TWINNING BEHAVIOR OF AZ31 Mg ALLOY DURING PLANE STRAIN COMPRESSION |
Bingshu WANG1( ),Liping DENG1,Adrien CHAPUIS2,Ning GUO3,Qiang LI1 |
1 College of Materials Science and Engineering, Fuzhou University, Fuzhou 350108 2 College of Materials Science and Engineering, Chongqing University, Chongqing 400044 3 Department of Materials Engineering, Faculty of Materials Science and Energy, Southwest University, Chongqing 400715 |
引用本文:
汪炳叔,邓丽萍,CHAPUIS Adrien,郭宁,李强. AZ31镁合金在平面应变压缩过程中的孪生行为研究*[J]. 金属学报, 2015, 51(12): 1441-1448.
Bingshu WANG,
Liping DENG,
Adrien CHAPUIS,
Ning GUO,
Qiang LI.
STUDY OF TWINNING BEHAVIOR OF AZ31 Mg ALLOY DURING PLANE STRAIN COMPRESSION[J]. Acta Metall Sin, 2015, 51(12): 1441-1448.
| [1] | Liu Q. Acta Metall Sin, 2010; 56: 1458 | | [1] | (刘 庆. 金属学报, 2010; 46: 1458) | | [2] | Koike J. Metall Mater Trans, 2005; 36A: 1689 | | [3] | Wan G, Wu B L, Zhang Y D, Sha G Y, Esling C. Mater Sci Eng, 2010; A527: 2915 | | [4] | Jiang L, Jonas J J, Mishra R K, Luo A A, Sachdev A K, Godet S. Acta Mater, 2007; 55: 3899 | | [5] | Wang Y N, Huang J C. Acta Mater, 2007; 55: 897 | | [6] | Yang X Y, Zhang L. Acta Metall Sin, 2009; 45: 1303 | | [6] | (杨续跃, 张 雷. 金属学报, 2009; 45: 1303) | | [7] | Nave M D, Barnett M R. Scr Mater, 2004; 51: 881 | | [8] | Jonas J J, Mu S, Al-Samman T, Gottstein G, Jiang L, Martin T. Acta Mater, 2011; 59: 2046 | | [9] | Luo J R, Godfrey A, Liu W, Liu Q. Acta Mater, 2012; 60: 1986 | | [10] | Ma Q, El Kadiri H, Oppedal A L, Baird J C, Horstemeyer M F, Cherkaoui M. Scr Mater, 2011; 64: 813 | | [11] | Hong S-G, Park S H, Lee C S. Scr Mater, 2011; 64: 145 | | [12] | Martin é, Capolungo L, Jiang L, Jonas J J. Acta Mater, 2010; 58: 3970 | | [13] | Hong S G, Park S H, Lee C S. Acta Mater, 2010; 58: 5873 | | [14] | Godet S, Jiang L, Luo A A, Jonas J J. Scr Mater, 2006; 55: 1055 | | [15] | Wang B S, Xin R L, Huang G J, Liu Q. Scr Mater, 2012; 66: 239 | | [16] | Pei Y. Master Thesis, Tsinghua University, Beijing, 2009 | | [16] | (裴 颖. 清华大学硕士学位论文, 北京, 2009) | | [17] | Mu S, Jonas J J, Gottstein G. Acta Mater, 2012; 60: 2043 | | [18] | Barnett M R, Keshavarz Z, Beer A G, Ma X. Acta Mater, 2008; 56: 5 | | [19] | Jiang J, Godfrey A, Liu W, Liu Q. Scr Mater, 2008; 58: 122 | | [20] | Al-Samman T, Ahmad B, Gottstein G. Mater Sci Forum, 2007; 550: 229 | | [21] | Chapuis A, Driver J H. Acta Mater, 2011; 59: 1986 | | [22] | Zhang L, Liu C G, Wang H Y, Nan X L, Wu Z Q, Jiang Q C. Mater Sci Eng, 2013; A578: 362 | | [23] | Maurice C, Piot D, Klocker H, Driver J H. Metall Mater Trans, 2005; 36A: 1039 | | [24] | Chapuis A, Wang B S, Liu Q. Mater Sci Eng, 2014; A597: 349 | | [25] | Jiang J, Godfrey A, Liu Q. Mater Sci Technol, 2005; 21: 1417 | | [26] | Wang B, Deng L, Guo N, Xu Z, Li Q. Mater Charact, 2014; 98: 180 |
|
|