| SiCp/Al复合材料热轧过程的有限元模拟* |
周丽1,2,王唱舟1,张星星2,肖伯律2,马宗义2( ) |
| 2 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| FINITE ELEMENT SIMULATION OF HOT ROLLING PROCESS FOR SiCp/Al COMPOSITES |
Li ZHOU1,2,Changzhou WANG1,Xingxing ZHANG2,Bolü XIAO2,Zongyi MA2( ) |
1 School of Mechanical Engineering, Shenyang Ligong University, Shenyang 110159 2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang110016 |
引用本文:
周丽,王唱舟,张星星,肖伯律,马宗义. SiCp/Al复合材料热轧过程的有限元模拟*[J]. 金属学报, 2015, 51(7): 889-896.
Li ZHOU,
Changzhou WANG,
Xingxing ZHANG,
Bolü XIAO,
Zongyi MA.
FINITE ELEMENT SIMULATION OF HOT ROLLING PROCESS FOR SiCp/Al COMPOSITES[J]. Acta Metall Sin, 2015, 51(7): 889-896.
| [1] | Selvam J D R, Smart D S R, Dinaharan I. Mater Des, 2013; 49: 28 | | [2] | Mortensen A, Llorca J. Annu Rev Mater Res, 2010; 40: 243 | | [3] | Wang S S, Mao C H, Yang J, Liang Q S, Sun B. Chin J Rare Met, 2012; 36: 167 (汪山山, 毛昌辉, 杨 剑, 梁秋实, 孙 波. 稀有金属, 2012; 36: 167) | | [4] | Hassani A, Bagherpour E, Qods F. J Alloys Compd, 2014; 591: 132 | | [5] | Balasubramanian I, Maheswaran R. Mater Des, 2015; 65: 511 | | [6] | Liu J W, Zheng Z X, Wang J M, Wu Y C, Tang W M, Lu J. J Alloys Compd, 2008; 465: 239 | | [7] | El-Sabbagh A, Solimam M, Taha M, Palkowski H. J Mater Process Technol, 2012; 212: 497 | | [8] | Goswami R K, Sikand R, Dhar A, Grover O P, Jindal U C, Gupta A K. Mater Sci Technol, 1999; 15: 443 | | [9] | El-Sabbagh A,?Soliman M,?Taha?M,?Palkowski H. J Mater Process Technol, 2013; 213: 1669 | | [10] | Euh K, Kang S B. Mater Sci Eng, 2005; A395: 47 | | [11] | Liu X H. Acta Metall Sin, 2010; 46: 1025 (刘相华. 金属学报, 2010; 46: 1025) | | [12] | Shahani A R, Setayeshi S, Nodamaie S A, Asadi M A, Rezaie S. J Mater Process Technol, 2009; 209: 1920 | | [13] | Duan X J, Sheppard T. J Mater Process Technol, 2004; 150: 100 | | [14] | Yu H L, Jiao Z J, Liu X H, Zhao X M. J Mater Metall, 2005; 4(1): 70 (喻海良, 矫志杰, 刘相华, 赵宪明. 材料与冶金学报, 2005; 4(1): 70) | | [15] | Arif A F M, Khan O, Sheikh A K. J Mater Process Technol, 2004; 147: 255 | | [16] | Kan Y, Liu Z G, Zhang S H, Zhang L W, Cheng M, Song H W. Chin J Rare Met, 2015; 39(4): 289 (阚 盈, 刘振刚, 张士宏, 张立文, 程 明, 宋鸿武. 稀有金属, 2015; 39(4): 289) | | [17] | Shao J C, Xiao B L, Wang Q Z, Ma Z Y, Liu Y, Yang K. Mater Sci Eng, 2010; A527: 7865 | | [18] | Xu H, Zhang X, Li H W, Li S, Wang C S, Wang Y L, Zhang B D. J Wuhan Univ Technol—Mater Sci Ed, 2012; 27: 443 | | [19] | Serajzadeh S, Karimi T A, Nejati M, Izadi J, Fattahi M. J Mater Process Technol, 2002; 128: 88 | | [20] | Yaakoubi M, Kchaou M, Dammak F. Comp Mater Sci, 2013; 68: 297 | | [21] | Chen J, Chandrashekhara K, Mahimkar C, Lekakh S N, Richards V L. J Mater Process Technol, 2011; 211: 245 | | [22] | Zhu Y, Kishawy H A. Int J Mach Tools Manuf, 2005; 45: 389 | | [23] | Tan Y Q, Yang D M, Sheng Y. J Eur Ceram Soc, 2009; 29: 1029 | | [24] | Ducobu F, Rivière-Lorphèvre E, Filippi E. Simul Modell Pract Theory, 2015; 53: 1 | | [25] | Cocchetti G, Pagani M, Perego U. Comp Struct, 2013; 127: 39 |
|
|