| 温度对Zr-45Ti-5Al-3V合金准静态力学性能的影响 |
刘丁铭1,2, 张波3, 王杰1, 王爱民1( ), 王沿东2, 张海峰1, 胡壮麒1 |
1 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 2 东北大学材料与冶金学院, 沈阳 110819 3 沈阳航空航天大学材料科学与工程学院, 沈阳 110136 |
|
| INFLUENCE OF TEMPERATURE ON QUASI-STATIC MECHANICAL PROPERTIES OF Zr-45Ti-5Al-3V ALLOY |
LIU Dingming1,2, ZHANG Bo3, WANG Jie1, WANG Aimin1( ), WANG Yandong2, ZHANG Haifeng1, HU Zhuangqi1 |
1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 2 School of Materials and Metallurgy, Northeastern University, Shenyang 110819 3 Department of Materials Science and Engineering, Shenyang Aerospace University, Shenyang 110136 |
引用本文:
刘丁铭, 张波, 王杰, 王爱民, 王沿东, 张海峰, 胡壮麒. 温度对Zr-45Ti-5Al-3V合金准静态力学性能的影响[J]. 金属学报, 2014, 50(12): 1498-1504.
Dingming LIU,
Bo ZHANG,
Jie WANG,
Aimin WANG,
Yandong WANG,
Haifeng ZHANG,
Zhuangqi HU.
INFLUENCE OF TEMPERATURE ON QUASI-STATIC MECHANICAL PROPERTIES OF Zr-45Ti-5Al-3V ALLOY[J]. Acta Metall Sin, 2014, 50(12): 1498-1504.
| [1] |
Wang S H, Yang D Z, He S Y, Lv G. Mater Sci Technol, 2004; 12(6): 579
|
| [1] |
(王淑花, 杨德庄, 何世禹, 吕 钢. 材料科学与工艺, 2004; 12(6): 579)
|
| [2] |
Li X, Wang L, Yu X M. Mater Sci Eng, 2003; A33: 2987
|
| [3] |
Qian J,Zhu Y L,Feng Y Y,Li F B. The Basic of Space Technology. Beijing: Science Press, 1986: 520
|
| [3] |
(钱 骥,朱毅麟,冯英远,李凡本.空间技术基础. 北京: 科学出版社, 1986: 520)
|
| [4] |
Zhao W J, Zhou B X, Miao Z, Peng Q, Jiang Y R, Jiang H M, Pang H. At Energy Sci Technol, 2005; 39(Sl): 2
|
| [4] |
(赵文金, 周邦新, 苗 志, 彭 倩, 蒋有荣, 蒋宏曼, 庞 华. 原子能科学技术, 2005; 39(增刊): 2
|
| [5] |
Saintoyant L, Legras L, Brchet Y. Scr Mater, 2011; 64: 418
|
| [6] |
Farhat Z N. Mater Sci Eng, 2008; A474: 96
|
| [7] |
Kondo R, Suyalatu, Tsutsumi Y, Doi H, Nomura N, Hanawa T. Mater Sci Eng, 2011; C31: 900
|
| [8] |
Sun C, Tan J, Ying S H, Li C. Rare Met Mater Eng, 2008; 37(4): 584
|
| [8] |
(孙 超, 谭 军, 应诗浩, 李 聪. 稀有金属材料与工程, 2008; 37(4): 584)
|
| [9] |
Liang S X, Ma M Z, Jing R, Zhou Y K, Jing Q, Liu R P. Mater Sci Eng, 2012; A539: 42
|
| [10] |
Liang S X, Ma M Z, Jing R, Zhang X Y, Liu R P. Mater Sci Eng, 2012; A532: 1
|
| [11] |
Liang S X, Yin L X, Che H W, Jing R, Zhou Y K, Ma M Z, Liu R P. Mater Des, 2013; 52: 246
|
| [12] |
Li Y, Zhang L, Zhu Z W, Li H, Wang A M, Zhang H F. Acta Metall Sin, 2014; 50: 19
|
| [12] |
(李 烨, 张 龙, 朱正旺, 李 宏, 王爱民, 张海峰. 金属学报, 2014; 50: 19)
|
| [13] |
Liang S X, Ma M Z, Jing R, Tan C L, Liu R P. Mater Sci Eng, 2012; A541: 67
|
| [14] |
Wang J, Zhang H W, Wang A M, Li H, Fu H M, Zhu Z W, Zhang H F. Acta Metall Sin, 2012; 48: 636
|
| [14] |
(王 杰, 张宏伟, 王爱民, 李 宏, 付华萌, 朱正旺, 张海峰. 金属学报, 2012; 48: 636)
|
| [15] |
Liang S X, Yin L X, Jing R, Zhang X Y, Ma M Z, Liu R P. J Mater Res, 2013; 28: 2715
|
| [16] |
Tan Y B, Liu W C, Yuan H, Liu R P, Zhang X Y. Metall Mater Trans, 2013; 44A: 5284
|
| [17] |
Liang S X, Yin L X, Che H W, Tan C L, Jing R, Zhou Y K, Ma M Z, Liu R P. Mater Des, 2014; 55: 64
|
| [18] |
Tan Y B, Yang L H, Tian C, Liu W C, Liu R P, Zhang X Y. Mater Sci Eng, 2014; A597: 171
|
| [19] |
Tan Y B, Yang L H, Tian C, Liu R P, Zhang X Y, Liu W C. Mater Sci Eng, 2013; A577: 218
|
| [20] |
Zhan Y Z, Zhang G D. Aerospace Mater Technol, 2003; (1): 1
|
| [20] |
(湛永钟, 张国定. 宇航材料工艺, 2003; (1): 1)
|
| [21] |
Cui Z Q,Tan Y C. Metallography and Heat Treatment. Beijing: Mechanical Industry Press, 2007: 186
|
| [21] |
(崔忠圻,覃耀春. 金属学与热处理. 北京: 机械工业出版社, 2007: 186)
|
| [22] |
Xu L, Guo R P, Bai C G, Lei J F, Yang R. J Mater Sci Technol, 2014, doi:10.1016/j.jmst.2014.04.011
|
| [23] |
Venkatesh B D, Chen D L, Bhole S D. Mater Sci Eng, 2009; A506: 117
|
| [24] |
Singh G, Sen I, Gopinath K, Ramamurty U. Mater Sci Eng, 2012; A540: 142
|
| [25] |
Feng D.Physics of Metals. Beijing: China Machine Press, 1999: 354
|
| [25] |
(冯 端. 金属物理学. 北京: 中国机械出版社, 1999: 354)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|